Abstract:
Methods for applying a liner-free, or liner-less label, to a substrate, particularly glass or plastic (e.g., PET) substrates are described herein. The method includes applying an adhesive composition, such as a polymeric coating, to a label face sheet, activating the adhesive composition with an activating fluid, and contacting the label to the substrate. The activating fluid is preferably a mixture of water and one or more organic solvents, such as low molecular weight alcohols. In some embodiments, the labels exhibit a percent fiber tear greater than about 50, 55, 60, 65, 70, 75, 80, 85, 90, or 95% after one, two, three, four, or five minutes. In particular embodiments, the labels exhibits a percent fiber tear greater than 60, 65, 70, 75, 80, 85, 90, or 95% after two minutes.
Abstract:
Methods for applying a liner-free, or liner-less label, to a substrate, particularly glass or plastic (e.g., PET) substrates are described herein. The method includes applying an adhesive composition, such as a polymeric coating, to a label face sheet, activating the adhesive composition with an activating fluid, and contacting the label to the substrate. The activating fluid is preferably a mixture of water and one or more organic solvents, such as low molecular weight alcohols. In some embodiments, the labels exhibit a percent fiber tear greater than about 50, 55, 60, 65, 70, 75, 80, 85, 90, or 95% after one, two, three, four, or five minutes. In particular embodiments, the labels exhibits a percent fiber tear greater than 60, 65, 70, 75, 80, 85, 90, or 95% after two minutes.
Abstract:
Methods for applying a liner-free, or liner-less label, to a substrate, particularly glass or plastic (e.g., polyethylene terephthalate) substrates, are described herein. The method includes applying an adhesive composition, such as a polymeric coating, to a label face sheet, activating the adhesive composition with an activating fluid, and contacting the label to the substrate. The activating fluid is preferably a mixture of water and one or more organic solvents, such as low molecular weight alcohols.
Abstract:
A fluid activatable adhesive for a liner-free label and methods of using are described. Preferably, the adhesive composition includes a polymer, such as an emulsion polymer formed from monomers selected from the group consisting of butyl acrylate, 2-ethylhexyl acrylate, methyl acrylate, 2-acrylamido-2-methylpropane sulfonic acid (AMPS), a salt of AMPS, such as its sodium salt, styrene, and combinations thereof. The adhesive composition adheres to the liner-free label to the surface of a substrate that is at room temperature, at room temperature and wet, cold, or cold and wet. In preferred embodiments, the substrate is glass or plastic, such as polyethylene terephthalate.
Abstract:
Methods for applying a liner-free, or liner-less label, to a substrate, particularly glass or plastic (e.g., PET) substrates are described herein. The method includes applying an adhesive composition, such as a polymeric coating, to a label face sheet, activating the adhesive composition with an activating fluid, and contacting the label to the substrate. The activating fluid is preferably a mixture of water and one or more organic solvents, such as low molecular weight alcohols. In some embodiments, the labels exhibit a percent fiber tear greater than about 50, 55, 60, 65, 70, 75, 80, 85, 90, or 95% after one, two, three, four, or five minutes. In particular embodiments, the labels exhibits a percent fiber tear greater than 60, 65, 70, 75, 80, 85, 90, or 95% after two minutes.
Abstract:
A fluid activatable adhesive for a liner-free label and methods of using are described. Preferably, the adhesive composition includes a polymer, such as an emulsion polymer formed from monomers selected from the group consisting of butyl acrylate, 2-ethylhexyl acrylate, methyl acrylate, 2-acrylamido-2-methylpropane sulfonic acid (AMPS), a salt of AMPS, such as its sodium salt, styrene, and combinations thereof. The adhesive composition adheres to the liner-free label to the surface of a substrate that is at room temperature, at room temperature and wet, cold, or cold and wet. In preferred embodiments, the substrate is glass or plastic, such as polyethylene terephthalate.
Abstract:
Methods for applying a liner-free, or liner-less label, to a substrate, particularly glass or plastic (e.g., polyethylene terephthalate) substrates, are described herein. The method includes applying an adhesive composition, such as a polymeric coating, to a label face sheet, activating the adhesive composition with an activating fluid, and contacting the label to the substrate. The activating fluid is preferably a mixture of water and one or more organic solvents, such as low molecular weight alcohols.
Abstract:
Methods for applying a liner-free, or liner-less label, to a substrate, particularly glass or plastic (e.g., PET) substrates are described herein. The method includes applying an adhesive composition, such as a polymeric coating, to a label face sheet, activating the adhesive composition with an activating fluid, and contacting the label to the substrate. The activating fluid is preferably a mixture of water and one or more organic solvents, such as low molecular weight alcohols. In some embodiments, the labels exhibit a percent fiber tear greater than about 50, 55, 60, 65, 70, 75, 80, 85, 90, or 95% after one, two, three, four, or five minutes. In particular embodiments, the labels exhibits a percent fiber tear greater than 60, 65, 70, 75, 80, 85, 90, or 95% after two minutes.
Abstract:
Methods for applying a liner-free, or liner-less label, to a substrate, particularly glass or plastic (e.g., polyethylene terephthalate) substrates, are described herein. The method includes applying an adhesive composition, such as a polymeric coating, to a label face sheet, activating the adhesive composition with an activating fluid, and contacting the label to the substrate. The activating fluid is preferably a mixture of water and one or more organic solvents, such as low molecular weight alcohols.
Abstract:
Methods for applying a liner-free, or liner-less label, to a substrate, particularly glass or plastic (e.g., PET) substrates are described herein. The method includes applying an adhesive composition, such as a polymeric coating, to a label face sheet, activating the adhesive composition with an activating fluid, and contacting the label to the substrate. The activating fluid is preferably a mixture of water and one or more organic solvents, such as low molecular weight alcohols. In some embodiments, the labels exhibit a percent fiber tear greater than about 50, 55, 60, 65, 70, 75, 80, 85, 90, or 95% after one, two, three, four, or five minutes. In particular embodiments, the labels exhibits a percent fiber tear greater than 60, 65, 70, 75, 80, 85, 90, or 95% after two minutes.