Fiber optic cable having a component with an absorptive polymer coating and a method of making the cable

    公开(公告)号:US06304699B2

    公开(公告)日:2001-10-16

    申请号:US09791375

    申请日:2001-02-23

    IPC分类号: G02B644

    摘要: A fiber optic cable (10) having at least one optical fiber (22) and a component disposed within the cable (10) between a core (20) and a jacket section (30) of the cable, and a method of making the cable. The component includes a substrate (34) with a water blocking formulation (50) thereon, the water blocking formulation (50) comprising a radiation curable resin (52) and a water absorptive substance (54) at least partially embedded or compounded in the radiation curable resin (52). The radiation curable resin (52) includes an initiator for rapid processing speeds. The water blocking formulation (50) may include a non-compatible material for reducing friction and/or enhancing physical properties. Water blocking formulation (50) is advantageously adaptable to application on various exemplary cable components (40,75,87,94,96,98,104).

    Fiber optic cable having a low-shrink cable jacket and methods of manufacturing the same
    3.
    发明授权
    Fiber optic cable having a low-shrink cable jacket and methods of manufacturing the same 有权
    具有低收缩电缆护套的光缆及其制造方法

    公开(公告)号:US06925235B2

    公开(公告)日:2005-08-02

    申请号:US10958143

    申请日:2004-10-04

    IPC分类号: G02B6/44

    摘要: A fiber optic cable and methods for manufacturing the same the fiber optic cable including a fiber optic cable core, the fiber optic cable core includes at least one optical fiber and a separation layer. The separation layer generally surrounds the at least one optical fiber, and a cable jacket generally surrounds the separation layer. The cable jacket has an average shrinkage of about 2.0% or less during a cable jacket shrinkage test conducted at a temperature of 110° C. for 2 hours with the cable core removed. The low-shrink characteristic of the cable jacket preserves optical performance during, for example, temperature variations.

    摘要翻译: 一种光纤电缆及其制造方法,所述光纤电缆包括光纤电缆芯,所述光纤电缆芯包括至少一个光纤和分离层。 分离层通常围绕至少一个光纤,并且电缆护套通常围绕分离层。 在110℃下进行的电缆套管收缩试验中,电缆护套的电缆芯已除去2小时,其平均收缩率约为2.0%以下。 电缆护套的低收缩特性在例如温度变化期间保持光学性能。

    Filling materials for communications cable
    4.
    发明授权
    Filling materials for communications cable 失效
    通讯电缆填充材料

    公开(公告)号:US4426230A

    公开(公告)日:1984-01-17

    申请号:US423818

    申请日:1982-09-27

    CPC分类号: H01B7/285 G02B6/4401

    摘要: Disclosed are telephone cable filling materials and telephone cables comprised of a plurality of insulated electrical conductors twisted together to form a core in which there are a multiplicity of interstices between the insulated electrical conductors filled with the cable filler materials. The filling materials are composed of a petrolatum base material and inorganic microspheres and can be divided into two groups: (1) a first group to fill cables used at temperatures below the melting point of the petrolatum and (2) a second group to fill cables that may be used above that temperature. The first group is composed of mixtures of 40 to 90 weight percent petrolatum and 1 to 60 weight percent inorganic hollow (air filled) microspheres. When mixtures from this group are used as a filler in a telephone cable, the filler has a drip point nearly equal to the average melting point of the petrolatum, normally 57.2.degree. C. The second group is composed of two embodiments. The first embodiment comprises 62 to 95 weight percent petrolatum, 1 to 35 weight percent inorganic hollow microspheres, and 1 to 8 weight percent low molecular weight polyethylene dissolved in the petrolatum. The second embodiment comprises 60 to 98 weight percent petrolatum, 1 to 39 weight percent inorganic hollow microspheres and 1 to 15 weight percent of glycerol hydroxy stearate dissolved in the petrolatum. When mixtures from the second group are used as a filler in a telephone cable, drip points ranging from the average melting point of petrolatum to temperatures in excess of 75.degree. C. are observed.

    摘要翻译: 公开了电话电缆填充材料和电话电缆,其由多个绝缘电导体组成,扭绞在一起以形成芯,其中填充有电缆填充材料的绝缘电导体之间存在多个间隙。 填充材料由凡士林基材和无机微球组成,可分为两组:(1)第一组填充在低于凡士林熔点的温度下使用的电缆,(2)第二组填充电缆 可以在该温度以上使用。 第一组由40至90重量百分比的凡士林和1至60重量%的无机中空(空气填充)微球体的混合物组成。 当来自该组的混合物用作电话电缆中的填料时,填料的滴点几乎等于凡士林的平均熔点,通常为57.2℃。第二组由两个实施方案组成。 第一个实施方案包含62至95重量百分比的凡士林,1至35重量%的无机中空微球和1至8重量%的低分子量聚乙烯溶于凡士林。 第二个实施方案包含60至98重量百分比的凡士林,1至39重量%的无机中空微球和1至15重量%的溶于凡士林的羟基硬脂酸甘油酯。 当来自第二组的混合物用作电话电缆中的填料时,观察到从凡士林的平均熔点到超过75℃的温度的滴点。

    Fiber optic cable having a low-shrink cable jacket and methods of manufacturing the same
    5.
    发明授权
    Fiber optic cable having a low-shrink cable jacket and methods of manufacturing the same 有权
    具有低收缩电缆护套的光缆及其制造方法

    公开(公告)号:US06801695B2

    公开(公告)日:2004-10-05

    申请号:US10038073

    申请日:2002-01-04

    IPC分类号: G02B644

    摘要: A fiber optic cable and methods for manufacturing the same the fiber optic cable including a fiber optic cable core, the fiber optic cable core includes at least one optical fiber and a separation layer. The separation layer generally surrounds the at least one optical fiber, and a cable jacket generally surrounds the separation layer. The cable jacket has an average shrinkage of about 2.0% or less during a cable jacket shrinkage test conducted at a temperature of 110° C. for 2 hours with the cable core removed. The low-shrink characteristic of the cable jacket preserves optical performance during, for example, temperature variations.

    摘要翻译: 一种光纤电缆及其制造方法,所述光纤电缆包括光纤电缆芯,所述光纤电缆芯包括至少一个光纤和分离层。 分离层通常围绕至少一个光纤,并且电缆护套通常围绕分离层。 在110℃下进行的电缆套管收缩试验中,电缆护套的电缆芯已除去2小时,其平均收缩率约为2.0%以下。 电缆护套的低收缩特性在例如温度变化期间保持光学性能。

    Fiber optic cable having a component with an absorptive polymer coating and a method of making the cable
    6.
    发明授权
    Fiber optic cable having a component with an absorptive polymer coating and a method of making the cable 失效
    具有吸收聚合物涂层的部件的光纤电缆和制造电缆的方法

    公开(公告)号:US06195486B1

    公开(公告)日:2001-02-27

    申请号:US09089201

    申请日:1998-06-02

    IPC分类号: G02B644

    摘要: A fiber optic cable (10) having at least one optical fiber (22) and a component disposed within the cable (10) between a core (20) and a jacket section (30) of the cable, and a method of making the cable. The component includes a substrate (34) with a water blocking formulation (50) thereon, the water blocking formulation (50) comprising a radiation curable resin (52) and a water absorptive substance (54) at least partially embedded or compounded in the radiation curable resin (52). The radiation curable resin (52) includes an initiator for rapid processing speeds. The water blocking formulation (50) may include a non-compatible material for reducing friction and/or enhancing physical properties. Water blocking formulation (50) is advantageously adaptable to application on various exemplary cable components (40,75,87,94,96,98,104).

    摘要翻译: 一种具有至少一个光纤(22)的光纤电缆(10)和设置在所述电缆(10)内的所述电缆(10)内的部件之间的电缆的芯子(20)和护套部分(30)之间的一种方法, 。 该组件包括其上具有防水制剂(50)的基底(34),所述防水制剂(50)包含辐射固化树脂(52)和至少部分地嵌入或复合在辐射中的吸水物质(54) 固化树脂(52)。 辐射固化树脂(52)包括用于快速处理速度的引发剂。 防水配方(50)可包括用于减少摩擦和/或增强物理性能的不相容材料。 阻水制剂(50)有利地适用于各种示例性电缆组件(40,75,87,94,96,98,104)。

    Filled transmission cable
    7.
    发明授权
    Filled transmission cable 失效
    填充传输电缆

    公开(公告)号:US4497538A

    公开(公告)日:1985-02-05

    申请号:US521954

    申请日:1983-08-10

    申请人: Naren I. Patel

    发明人: Naren I. Patel

    摘要: An improved transmission cable containing a filling material having superior handling and melt point characteristics useful for waterproofing telecommunication cables composed of a styrene-ethylene butylene-styrene block copolymer dissolved in petrolatum with polyethylene added for consistency and to increase the melting point of the mixture.

    摘要翻译: 一种改进的传输电缆,其包含具有优异的处理和熔点特性的填充材料,该填充材料可用于由溶于石榴油中的苯乙烯 - 乙烯 - 丁烯 - 苯乙烯嵌段共聚物与聚乙烯一起加入以增加混合物的熔点而防水通信电缆。

    Optical ribbon cable component
    9.
    发明授权
    Optical ribbon cable component 失效
    光带电缆组件

    公开(公告)号:US5166998A

    公开(公告)日:1992-11-24

    申请号:US839153

    申请日:1992-02-21

    申请人: Naren I. Patel

    发明人: Naren I. Patel

    IPC分类号: G02B6/44

    摘要: An optical cable component made up of an elongated flexible substrate, having first and second groups of plastic coated optical fibers, the first group being removably affixed to a first surface of the substrate and the surface opposite from the first group on its opposite surface being essentially unoccupied. The second group of plastic coated optical fibers are removably affixed to the second surface of the substrate and the surface opposite from the second group being essentially unoccupied. Between the first and second groups of plastic coated optical fibers, there is delimited an unoccupied portion on both surfaces essentially equal to the diameter of one of the plastic coated optical fibers. Each group of plastic coated optical fibers bear an indicia for identification purposes.

    摘要翻译: 由细长柔性基板构成的光缆部件,其具有第一和第二组塑料涂覆的光纤,第一组可移除地固定到基板的第一表面,并且在其相对表面上与第一组相对的表面基本上是 空闲 第二组塑料涂覆的光纤可移除地固定到基板的第二表面,并且与第二组相对的表面基本上未被占据。 在第一和第二组塑料涂覆的光纤之间,在两个表面上限定了空心部分,基本上等于其中一个塑料涂覆的光纤的直径。 每组塑料涂层光纤都有一个用于识别目的的标记。

    Filling materials for communications cable

    公开(公告)号:US4382821A

    公开(公告)日:1983-05-10

    申请号:US317483

    申请日:1981-11-02

    CPC分类号: G02B6/4401 H01B7/285

    摘要: Disclosed are telephone cable filling materials and telephone cables comprised of a plurality of insulated electrical conductors twisted together to form a core in which there are a multiplicity of interstices between the insulated electrical conductors filled with the cable filler materials. The filling materials are composed of a petrolatum base material and inorganic microspheres and can be divided into two groups: (1) a first group to fill cables used at temperatures below the melting point of the petrolatum and (2) a second group to fill cables that may be used above that temperature. The first group is composed of mixtures of 40 to 90 weight percent petrolatum and 1 to 60 weight percent inorganic hollow (air filled) microspheres. When mixtures from this group are used as a filler in a telephone cable, the filler has a drip point nearly equal to the average melting point of the petrolatum, normally 57.2.degree. C. The second group is composed of two embodiments. The first embodiment comprises 62 to 95 weight percent petrolatum, 1 to 35 weight percent inorganic hollow microspheres, and 1 to 8 weight percent low molecular weight polyethylene dissolved in the petrolatum. The second embodiment comprises 60 to 98 weight percent petrolatum, 1 to 39 weight percent inorganic hollow microspheres and 1 to 15 weight percent of glycerol hydroxy stearate dissolved in the petrolatum. When mixtures from the second group are used as a filler in a telephone cable, drip points ranging from the average melting point of petrolatum to temperatures in excess of 75.degree. C. are observed.