摘要:
A high-strength steel pipe having a strength of API X65 grade or higher consisting essentially of, by mass %, 0.02 to 0.08% of C, 0.01 to 0.5% of Si, 0.5 to 1.8% of Mn, 0.01% or less of P, 0.002% or less of S, 0.01 to 0.7% of Al, 0.005 to 0.04% of Ti, 0.05 to 0.50% Mo, at least one element selected from 0.005 to 0.05% of Nb and 0.005 to 0.10% of V, and the balance being Fe, in which the volume percentage of the ferritic phase is 90% or higher, and complex carbides containing Ti, Mo, and at least one element selected from the group consisting of Nb and V are precipitated in the ferritic phase. The high-strength steel pipe has excellent HIC resistance and good toughness of a heat-affected zone, and can be manufactured stably at a low cost.
摘要:
A high strength steel plate containing 0.02 to 0.08% C, by mass, and has substantially a two phase microstructure of ferrite and bainite. The ferrite contains precipitates having a particle size of 30 nm or smaller grain size. The steel plate has a yield strength of 448 MPa or higher. A method for manufacturing the high strength steel plate which comprises hot rolling, accelerated cooling and reheating. The accelerated cooling is conducted down to a temperature of 300 to 600° C. at a cooling rate of 5° C./s or higher. The reheating is conducted up to a temperature of 550 to 700° C. at a heating rate of 0.5° C./s or higher.
摘要:
A high-strength steel pipe having a strength of API X65 grade or higher consisting essentially of, by mass %, 0.02 to 0.08% of C, 0.01 to 0.5% of Si, 0.5 to 1.8% of Mn, 0.01% or less of P, 0.002% or less of S, 0.01 to 0.7% of Al, 0.005 to 0.04% of Ti, 0.05 to 0.50% Mo, at least one element selected from 0.005 to 0.05% of Nb and 0.005 to 0.10% of V, and the balance being Fe, in which the volume percentage of the ferritic phase is 90% or higher, and complex carbides containing Ti, Mo, and at least one element selected from the group consisting of Nb and V are precipitated in the ferritic phase. The high-strength steel pipe has excellent HIC resistance and good toughness of a heat-affected zone, and can be manufactured stably at a low cost.
摘要:
A high strength steel plate containing 0.02 to 0.08% C, by mass, and has substantially a two phase microstructure of ferrite and bainite. The ferrite contains precipitates having a particle size of 30 nm or smaller grain size. The steel plate has a yield strength of 448 MPa or higher. A method for manufacturing the high strength steel plate which comprises hot rolling, accelerated cooling and reheating. The accelerated cooling is conducted down to a temperature of 300 to 600° C. at a cooling rate of 5° C./s or higher. The reheating is conducted up to a temperature of 550 to 700° C. at a heating rate of 0.5° C./s or higher.
摘要:
A high strength steel plate containing 0.02 to 0.08% C, by mass, and has substantially a two phase microstructure of ferrite and bainite. The ferrite contains precipitates having a particle size of 30 nm or smaller grain size. The steel plate has a yield strength of 448 MPa or higher. A method for manufacturing the high strength steel plate which comprises hot rolling, accelerated cooling and reheating. The accelerated cooling is conducted down to a temperature of 300 to 600° C. at a cooling rate of 5° C./s or higher. The reheating is conducted up to a temperature of 550 to 700° C. at a heating rate of 0.5° C./s or higher.
摘要:
A high-strength steel pipe having a strength of API X65 grade or higher consisting essentially of, by mass %, 0.02 to 0.08% of C, 0.01 to 0.5% of Si, 0.5 to 1.8% of Mn, 0.01% or less of P, 0.002% or less of S, 0.01 to 0.7% of Al, 0.005 to 0.04% of Ti, 0.05 to 0.50% Mo, at least one element selected from 0.005 to 0.05% of Nb and 0.005 to 0.10% of V, and the balance being Fe, in which the volume percentage of the ferritic phase is 90% or higher, and complex carbides containing Ti, Mo, and at least one element selected from the group consisting of Nb and V are precipitated in the ferritic phase. The high-strength steel pipe has excellent HIC resistance and good toughness of a heat-affected zone, and can be manufactured stably at a low cost.
摘要:
The high strength steel plate according to the present invention contains 0.02 to 0.08% C, by mass, and has substantially a two phase microstructure of ferrite and bainite. The ferrite contains precipitates having particle size of 30 nm or smaller grain size. The steel plate has yield strength of 448 MPa or higher. The method for manufacturing the high strength steel plate comprises the steps of hot rolling, accelerated cooling, and reheating. The accelerated cooling is conducted down to the temperature of 300 to 600° C. at a cooling rate of 5° C./s or higher. The reheating is conducted up to temperature of 550 to 700° C. at a heating rate of 0.5° C./s or higher.
摘要:
A low yield ratio, high toughness steel plate which can be manufactured at high manufacturing efficiency and low cost, without increasing material cost by adding large amount of alloy elements and the like, and without degrading toughness of a welding heat affected zone, a low yield ratio, high strength and high toughness steel pipe using the steel plate, and a method for manufacturing those are provided. Specifically, the steel plate and the steel pipe contain C of 0.03% to 0.1%, Si of 0.01 to 0.5%, Mn of 1.2 to 2.5% and Al of 0.08% or less, wherein a metal structure is a substantially three-phase structure of ferrite, bainite and island martensite, and an area fraction of the island martensite is 3 to 20%, in addition, a complex carbide is precipitated in the ferrite phase.
摘要:
A low yield ratio, high toughness steel plate which can be manufactured at high manufacturing efficiency and low cost, without increasing material cost by adding large amount of alloy elements and the like, and without degrading toughness of a welding heat affected zone, a low yield ratio, high strength and high toughness steel pipe using the steel plate, and a method for manufacturing those are provided. Specifically, the steel plate and the steel pipe contain C of 0.03% to 0.1%, Si of 0.01 to 0.5%, Mn of 1.2 to 2.5% and Al of 0.08% or less, wherein a metal structure is a substantially three-phase structure of ferrite, bainite and island martensite, and an area fraction of the island martensite is 3 to 20%, in addition, a complex carbide is precipitated in the ferrite phase.
摘要:
A method and apparatus manufactures a closed structure part without flange having a curvature and welded edges along a longitudinal direction of the part and further having a varying cross-sectional shape, from two metal plates. Each of two metal plates provided with a curvature along the longitudinal direction of the plate and provided with both ends in a width direction of the plate, are press-formed such that a folding line is formed at positions corresponding to a non-welded bent edge in a cross section of the part, and stacked on each other vertically such that their bulging sides face outward. Their left ends and right ends in the width direction are mutually welded along the longitudinal direction to form welded edges.