NANOCRYSTAL-SIZED CERIUM-ZIRCONIUM OXIDE MATERIAL AND METHOD OF MAKING THE SAME

    公开(公告)号:US20210300778A1

    公开(公告)日:2021-09-30

    申请号:US17345121

    申请日:2021-06-11

    Abstract: A nanocrystal-sized cerium-zirconium mixed oxide material includes at least 30% by mass zirconium oxide; between 5% to 55% by mass cerium oxide; and a total of 25% or less by mass of at least one oxide of a rare earth metal selected from the group of lanthanum, neodymium, praseodymium, or yttrium. The nanocrystal-sized cerium-zirconium mixed oxide exhibits hierarchically ordered aggregates having a d50 particle size less than 1.5 μm and a total pore volume after calcination at a temperature of 600° C. or more that is at least 0.7 cm3/g with a fraction of pores between 2 nm to 10 nm being less than 15%. The nanocrystal-sized cerium-zirconium mixed oxide material is prepared using a co-precipitation method followed by milling the dried and calcined oxide material. The nanocrystal-sized cerium-zirconium mixed oxide material forms a particulate filter that may be used in an exhaust system arising from a gas or diesel engine.

    Nanocrystal-sized cerium-zirconium-aluminum oxide material and method of making the same

    公开(公告)号:US12227428B2

    公开(公告)日:2025-02-18

    申请号:US17422770

    申请日:2019-12-19

    Abstract: A nanocrystal-sized cerium-zirconium-aluminum mixed oxide material includes at least 20% by mass zirconium oxide; between 5% to 55% by mass cerium oxide; between 5% to 60% by mass aluminum oxide; and a total of 25% or less by mass of at least one oxide of a rare earth metal selected from the group of lanthanum, neodymium, praseodymium, or yttrium. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide exhibits hierarchically ordered aggregates having a dso particle size less than 1.5 μm, and retains at least 80% of surface area and pore volume after ageing at temperature higher than 1000° C. for at least 6 hours. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material is prepared using a co-precipitation method followed by milling the dried and calcined oxide material. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material forms a particulate filter that may be used in an exhaust system arising from a gas or diesel engine.

    NANOCRYSTAL-SIZED CERIUM-ZIRCONIUM-ALUMINUM OXIDE MATERIAL AND METHOD OF MAKING THE SAME

    公开(公告)号:US20220064017A1

    公开(公告)日:2022-03-03

    申请号:US17422770

    申请日:2019-12-19

    Abstract: A nanocrystal-sized cerium-zirconium-aluminum mixed oxide material includes at least 20% by mass zirconium oxide; between 5% to 55% by mass cerium oxide; between 5% to 60% by mass aluminum oxide; and a total of 25% or less by mass of at least one oxide of a rare earth metal selected from the group of lanthanum, neodymium, praseodymium, or yttrium. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide exhibits hierarchically ordered aggregates having a dso particle size less than 1.5 μm, and retains at least 80% of surface area and pore volume after ageing at temperature higher than 1000° C. for at least 6 hours. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material is prepared using a co-precipitation method followed by milling the dried and calcined oxide material. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material forms a particulate filter that may be used in an exhaust system arising from a gas or diesel engine