摘要:
The present invention relates to a method for dosing and dispensing a laundry detergent, preferably a liquid laundry detergent, into a washing machine comprising the steps of: i) measuring a dose of laundry detergent into a dosing and dispensing device (10) comprising a hollow cavity defined by a base (11) and side-walls (12), wherein the base (11) and/or side walls (12) are at least partly covered by a sleeve (20), and wherein the sleeve (20) comprises a film of material comprising printed indicia (21) thereupon, wherein the printed indicia (21) are resistant to removal from the film when the dosing and dispensing device (10) is exposed to wash conditions inside a washing machine; ii) placing both the laundry and the dosing and dispensing device containing laundry detergent into a washing machine, and running the washing machine on a selected cleaning cycle; and iii) subsequently reusing the dosing and dispensing device (10) for steps i) and ii).
摘要:
A process for blow-molding a container, the container comprising a handle, whereby the process comprises the steps of: (i) introducing a preform (2) into a mold cavity and stretching the preform (2) with a stretch rod; (ii) increasing the pressure within the preform (2) so that the preform (2) expands within the mold cavity in a first blowing step, the pressure in the first blowing step is from 1 to 10 bar; (iii) inwardly moving jaws (3, 4) within the mold cavity so that the expanding preform (2) is partially gripped between the jaws in the handle region; (iv) subsequently increasing the pressure within the preform (2) wherein the maximum pressure in the second blowing step is greater than 10 bar, so that the preform (2) expands to the limits of the mold cavity in a second blowing step to form a container; and wherein the inward movement of the jaws (3, 4) is completed within the first blowing step.
摘要:
The present invention relates to a process for making a container having an integral handle, comprising the steps of: a) providing a preform (6) in a mold cavity (1); b) stretch-blow molding the preform (6) to form an intermediate container (8) which comprises at least one, preferably two, convex bubble(s) (9); c) deforming the or each convex bubble (9) by means of an inwardly moving plug (5) to form one or more concave gripping region(s), while maintaining the pressure within the intermediate container (8) above 1 bar and while the temperature of the material in the gripping region of the intermediate container is maintained at a temperature between the glass transition temperature, Tg, and the melt temperature, Tm; d) releasing excess pressure within the container, preferably prior to withdrawing the plug (5) from within the container; and e) ejecting the finished container from the mold cavity (1, 3).
摘要:
The present invention relates to a process for making a container having an integral handle, comprising the steps of: a) providing a preform (1) in a mould cavity (2); b) stretch-blow moulding the preform (1) to form an intermediate container (3); c) applying one or more inwardly moving plugs (5) to form one or more concave gripping region(s), whilst maintaining the pressure within the intermediate container (3) above 1 bar and whilst the temperature of the material in the gripping region of the intermediate container is at a temperature below the glass transition temperature, Tg; d) releasing excess pressure within the container, preferably prior to withdrawing the plug (5) from within the container; and e) ejecting the finished container(6) from the mould cavity (2,4).
摘要:
The present invention relates to a process for making a container having an integral handle, comprising the steps of: a) providing a preform (1) in a mould cavity (2); b) stretch-blow moulding the preform (1) to form an intermediate container (3); c) applying one or more inwardly moving plugs (5) to form one or more concave gripping region(s), whilst maintaining the pressure within the intermediate container (3) above 1 bar and whilst the temperature of the material in the gripping region of the intermediate container is at a temperature below the glass transition temperature, Tg; d) releasing excess pressure within the container, preferably prior to withdrawing the plug (5) from within the container; and e) ejecting the finished container(6) from the mould cavity (2,4).
摘要:
The present invention relates to a process for blow molding a polyethylene container comprising the steps of: a) providing a solid preform made from a polyethylene material having a melt flow index from 0.01 to 10.0 g/10 minutes, wherein the preform comprises a neck region, side walls and a base region, and wherein the side walls between the neck region and the base region have substantially straight and parallel outer walls; b) reheating the preform so that the maximum temperature difference between the hottest and coldest regions of the side walls and the base region of the reheated preform is less than 4° C.; c) transferring the reheated preform to a blow mould; d) stretching the preform at a pressure below 10 bars; and e) increasing the pressure within the reheated preform so as to cause the walls of the stretched preform to expand to the shape and dimensions inside the blow mould. A polyethylene container made according to the present invention preferably has a minimum wall thickness of the container of less than 200 micrometers, and a weight to volume ratio of the empty container of less than 50 grams per litre.
摘要:
The present invention relates to a process for blow molding a polyethylene container comprising the steps of: a) providing a solid preform made from a polyethylene material having a melt flow index from 0.01 to 10.0 g/10 minutes, wherein the preform comprises a neck region, side walls and a base region, and wherein the side walls between the neck region and the base region have substantially straight and parallel outer walls; b) reheating the preform so that the maximum temperature difference between the hottest and coldest regions of the side walls and the base region of the reheated preform is less than 4° C.; c) transferring the reheated preform to a blow mold; d) stretching the preform at a pressure below 10 bars; and e) increasing the pressure within the reheated preform so as to cause the walls of the stretched preform to expand to the shape and dimensions inside the blow mold. A polyethylene container made according to the present invention preferably has a minimum wall thickness of the container of less than 200 micrometers, and a weight to volume ratio of the empty container of less than 50 grams per liter.
摘要:
The present invention relates to a solid preform made from polyethylene material, wherein the preform comprises a neck region, side walls and a base region, and has an interior having inner walls and an exterior having outer walls; characterised in that at least 65% of the polyethylene material by weight of the total polyethylene material has a Z-average molecular weight (Mz) of between 300,000 g/mol and 6,000,000 g/mol, and a Mz/Mn value of greater than 28, where Mn is the number average molecular weight, and Mz/Mn is the Mz value divided by the Mn value.