POLYMER EXPANDED PARTICLE, EXPANDED TONER AND METHOD FOR PRODUCING POLYMER EXPANDED PARTICLE AND EXPANDED TONER
    2.
    发明申请
    POLYMER EXPANDED PARTICLE, EXPANDED TONER AND METHOD FOR PRODUCING POLYMER EXPANDED PARTICLE AND EXPANDED TONER 审中-公开
    聚合物膨胀颗粒,膨胀聚合物和生产聚合物膨胀颗粒和膨胀碳粉的方法

    公开(公告)号:US20130011782A1

    公开(公告)日:2013-01-10

    申请号:US13635385

    申请日:2011-03-17

    摘要: A polymer expanded particle and an expanded toner having small pores, and a production method thereof are provided. A polymer expanded particle comprises micropores having an average pore diameter of less than 50 μm. An expanded toner comprises micropores having an average pore diameter of 1 μm to less than 3 μm, wherein volume average particle diameter is 5 μm to less than 15 μm. A method for producing a polymer expanded particle comprises a first step for mixing specific polymer particles with high pressure gas or supercritical fluid, to prepare a mixture, a second step for impregnating with the high pressure gas or the supercritical fluid to the inside of the polymer particles, and a third step for reducing pressure and temperature of the mixture, to form the polymer expanded particle, wherein the pressure and temperature in the third step is reduced for 5 minutes or less from a state of 20 MPa or greater and 60° C. or greater to a state of less than 1 MPa and less than 30° C., respectively.

    摘要翻译: 提供聚合物发泡粒子和具有小孔的膨胀调色剂及其制备方法。 聚合物发泡颗粒包含平均孔径小于50μm的微孔。 膨胀调色剂包括平均孔径为1μm至小于3μm的微孔,其中体积平均粒径为5μm至小于15μm。 聚合物发泡粒子的制造方法包括:将特定聚合物粒子与高压气体或超临界流体混合的第一工序,制备混合物;第二步骤,用于将高压气体或超临界流体浸渍到聚合物内部 颗粒和第三步骤,用于降低混合物的压力和温度,以形成聚合物膨胀颗粒,其中第三步骤中的压力和温度从20MPa或更高和60℃的状态降低5分钟或更短 或更大到分别小于1MPa且小于30℃的状态。