摘要:
A two-phase electrophoretic medium comprises a continuous phase and a discontinuous phase. The discontinuous phase comprises a plurality of droplets, each of which comprises a suspending fluid and at least one particle disposed within the suspending fluid and capable of moving through the fluid upon application of an electric field to the electrophoretic medium. The continuous phase surrounds and encapsulates the discontinuous phase. To reduce the humidity sensitivity of the medium, a non-ionizable or crystalline polymer may be used as the continuous phase.
摘要:
A two-phase electrophoretic medium comprises a continuous phase and a discontinuous phase. The discontinuous phase comprises a plurality of droplets, each of which comprises a suspending fluid and at least one particle disposed within the suspending fluid and capable of moving through the fluid upon application of an electric field to the electrophoretic medium. The continuous phase surrounds and encapsulates the discontinuous phase. To reduce the humidity sensitivity of the medium, a non-ionizable or crystalline polymer may be used as the continuous phase.
摘要:
An encapsulation material, intended for use in encapsulated electrophoretic displays, comprises the coacervation product of a polyanionic polymer having a vinyl main chain and a plurality of anionic groups bonded to the main chain, with a cationic or zwitterionic water-soluble polymer capable of forming an immiscible second phase on contact with the polyanionic polymer.
摘要:
A first electro-optic display comprises first and second substrates, and an adhesive layer and a layer of electro-optic material disposed between the first and second substrates, the adhesive layer comprising a mixture of a polymeric adhesive material and a hydroxyl containing polymer having a number average molecular weight not greater than about 5000. A second electro-optic display is similar to the first but has an adhesive layer comprising a thermally-activated cross-linking agent to reduce void growth when the display is subjected to temperature changes. A third electro-optic display, intended for writing with a stylus or similar instrument, is produced by forming a layer of an electro-optic material on an electrode; depositing a substantially solvent-free polymerizable liquid material over the electro-optic material; and polymerizing the polymerizable liquid material.
摘要:
An electrophoretic medium comprises an electrophoretic layer, a layer of lamination adhesive and a polymeric layer disposed between the electrophoretic layer and the lamination adhesive layer, the polymeric layer being impermeable to the fluid. A second form of electrophoretic medium has a layer of a complex of an alkali metal and a polymer in contact with the electrophoretic layer. A third form of electrophoretic medium comprises a plurality of discrete droplets of internal phase in a binder, and further comprises a salt.
摘要:
An electrophoretic medium comprises an electrophoretic layer, a layer of lamination adhesive and a polymeric layer disposed between the electrophoretic layer and the lamination adhesive layer, the polymeric layer being impermeable to the fluid. A second form of electrophoretic medium has a layer of a complex of an alkali metal and a polymer in contact with the electrophoretic layer. A third form of electrophoretic medium comprises a plurality of discrete droplets of internal phase in a binder, and further comprises a salt.
摘要:
A first electro-optic display comprises first and second substrates, and an adhesive layer and a layer of electro-optic material disposed between the first and second substrates, the adhesive layer comprising a mixture of a polymeric adhesive material and a hydroxyl containing polymer having a number average molecular weight not greater than about 5000. A second electro-optic display is similar to the first but has an adhesive layer comprising a thermally-activated cross-linking agent to reduce void growth when the display is subjected to temperature changes. A third electro-optic display, intended for writing with a stylus or similar instrument, is produced by forming a layer of an electro-optic material on an electrode; depositing a substantially solvent-free polymerizable liquid material over the electro-optic material; and polymerizing the polymerizable liquid material.
摘要:
An electrophoretic medium comprises an electrophoretic layer, a layer of lamination adhesive and a polymeric layer disposed between the electrophoretic layer and the lamination adhesive layer, the polymeric layer being impermeable to the fluid. A second form of electrophoretic medium has a layer of a complex of an alkali metal and a polymer in contact with the electrophoretic layer. A third form of electrophoretic medium comprises a plurality of discrete droplets of internal phase in a binder, and further comprises a salt.
摘要:
A two-phase electrophoretic medium comprises a continuous phase and a discontinuous phase. The discontinuous phase comprises a plurality of droplets, each of which comprises a suspending fluid and at least one particle disposed within the suspending fluid and capable of moving through the fluid upon application of an electric field to the electrophoretic medium. The continuous phase surrounds and encapsulates the discontinuous phase. The discontinuous phase comprises at least about 40 percent by volume of the electrophoretic medium.
摘要:
In electrophoretic media, it is advantageous to use pigment particles having about 1 to 15 per cent by weight of a polymer chemically bonded to, or cross-linked around, the pigment particles. The polymer desirably has a branched chain structure with side chains extending from a main chain. Charged or chargeable groups can be incorporated into the polymer or can be bonded to the particles separately from the polymer. The polymer-coated particles can be prepared by first attaching a polymerizable or polymerization-initiating group to the particle and then reacting the particle with one or more polymerizable monomers or oligomers.