Abstract:
An asymmetric membrane having a substantially non-porous surface layer is made by a method including: dissolving a poly(phenylene ether) copolymer in a solvent mixture including a first solvent and a second solvent to provide a membrane-forming composition; and phase-inverting the membrane forming composition in a first non-solvent to form the membrane comprising a substantially non-porous surface layer. The first solvent is a water-miscible polar aprotic solvent, and the second solvent is a polar solvent having two to eight carbon atoms.
Abstract:
A porous membrane made from a poly(phenylene ether) copolymer has at least one of: a molecular weight cut off of less than 40 kilodaltons or a surface pore size of 0.001 to 0.1 micrometers. The porous membrane is made by dissolving the poly(phenylene ether) copolymer in a water-miscible polar aprotic solvent to form a porous membrane-forming composition; and phase-inverting the porous asymmetric membrane forming-composition in a first non-solvent composition to form the porous mem-brane. The porous membrane can be in the form of a sheet or a hollow fiber, and can be fabricated into separation modules.
Abstract:
An amphiphilic block copolymer comprises a poly(phenylene ether) block or a poly(phenylene ether) copolymer block and a hydrophilic block or graft. A method of making the amphiphilic block copolymer comprises polymerization of a hydrophilic ethylenically unsaturated monomer in the presence of poly(phenylene ether) or a poly(phenylene ether) copolymer to make the amphiphilic block copolymer. A porous asymmetric membrane comprises a poly(phenylene ether) or poly(phenylene ether) copolymer, and the amphiphilic block copolymer comprising a poly(phenylene ether) block or a poly(phenylene ether) copolymer block, and a hydrophilic block or graft. The porous asymmetric membrane is made by phase-inversion of a dope solution of the poly(phenylene ether) or poly(phenylene ether) copolymer and the amphiphilic block copolymer in a coagulation bath.
Abstract:
A separation module that includes a porous membrane, where the porous membrane includes a poly(phenylene ether) copolymer containing 10 to 40 mole percent repeat units derived from 2-methyl-6-phenylphenol and 60 to 90 mole percent repeat units derived from 2,6-dimethylphenol; and a block copolymer containing backbone or pendant blocks of poly(C2-4 alkylene oxide). The separation module can be used in devices for wastewater treatment, water purification, desalination, separating water-insoluble oil from oil-containing wastewater, membrane distillation, sugar purification, protein concentration, enzyme recovery, dialysis, liver dialysis, or blood oxygenation.
Abstract:
An amphiphilic block copolymer comprises a poly(phenylene ether) block or a poly(phenylene ether) copolymer block and a hydrophilic block or graft. A method of making the amphiphilic block copolymer comprises polymerization of a hydrophilic ethylenically unsaturated monomer in the presence of poly(phenylene ether) or a poly(phenylene ether) copolymer to make the amphiphilic block copolymer. A porous asymmetric membrane comprises a poly(phenylene ether) or poly(phenylene ether) copolymer, and the amphiphilic block copolymer comprising a poly(phenylene ether) block or a poly(phenylene ether) copolymer block, and a hydrophilic block or graft. The porous asymmetric membrane is made by phase-inversion of a dope solution of the poly(phenylene ether) or poly(phenylene ether) copolymer and the amphiphilic block copolymer in a coagulation bath.
Abstract:
An method of making a porous asymmetric membrane involves dissolving a poly(phenylene ether), poly(phenylene ether) copolymer, polyethersulfone, polysulfone, polyphenylsulfone, polyimide, polyetherimide, polyvinylidene fluoride, or a combination thereof in a water-miscible polar aprotic solvent to provide a membrane-forming composition; and phase-inverting the membrane-forming composition in a first non-solvent composition composed of water, a water-miscible polar aprotic solvent, or a mixture thereof, and a polymer additive dissolved in the first non-solvent composition. The method can be a method of making a hollow fiber by coextrusion through a spinneret having an annulus and a bore, including coextruding the membrane-forming composition through the annulus, and the first non-solvent composition through the bore, into a second non-solvent composition composed of water, a water-miscible polar aprotic solvent, or a mixture thereof to form the hollow fiber.
Abstract:
A porous asymmetric membrane comprises a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer; and a polymer additive. A separation module can be fabricated from the porous asymmetric membrane. A method of forming the porous asymmetric membrane comprises: dissolving a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer and, a polymer additive in a water-miscible polar aprotic solvent to form a porous asymmetric membrane-forming composition; and phase-inverting the porous asymmetric membrane forming-composition in a first non-solvent composition to form the porous asymmetric membrane. The polymer additive comprises hydrophilic functional groups, copolymerized hydrophilic monomers, or blocks of hydrophilic monomer repeat units. For example, the polymer additive can comprise a hydrophilic polymer or amphiphilic polymer. The porous asymmetric membrane can be a flat membrane or hollow fiber.
Abstract:
A porous asymmetric membrane comprises a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer; and a polymer additive. A separation module can be fabricated from the porous asymmetric membrane. A method of forming the porous asymmetric membrane comprises: dissolving a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer and, a polymer additive in a water-miscible polar aprotic solvent to form a porous asymmetric membrane-forming composition; and phase-inverting the porous asymmetric membrane forming-composition in a first non-solvent composition to form the porous asymmetric membrane. The polymer additive comprises hydrophilic functional groups, copolymerized hydrophilic monomers, or blocks of hydrophilic monomer repeat units. For example, the polymer additive can comprise a hydrophilic polymer or amphiphilic polymer. The porous asymmetric membrane can be a flat membrane or hollow fiber.
Abstract:
A porous membrane is made from a poly(phenylene ether) copolymer containing 10 to 40 mole percent repeat units derived from 2-methyl-6-phenylphenol and 60 to 90 mole percent repeat units derived from 2,6-dimethylphenol; and a block copolymer containing backbone or pendant blocks of poly(C2-4 alkylene oxide). The porous membrane is made by dissolving the poly(phenylene ether) copolymer in a water-miscible polar aprotic solvent to form a membrane-forming composition; and phase-inverting the membrane forming-composition in a first non-solvent composition to form the porous membrane. A method of making a hollow fiber by coextrusion through a spinneret having an annulus and a bore, includes coextruding the membrane-forming composition through the annulus, and a first non-solvent composition through the bore, into a second non-solvent composition to form the hollow fiber.
Abstract:
A porous asymmetric membrane comprises a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer; and a polymer additive. A separation module can be fabricated from the porous asymmetric membrane. A method of forming the porous asymmetric membrane comprises: dissolving a hydrophobic polymer comprising a poly(phenylene ether) or poly(phenylene ether) copolymer and, a polymer additive in a water-miscible polar aprotic solvent to form a porous asymmetric membrane-forming composition; and phase-inverting the porous asymmetric membrane forming-composition in a first non-solvent composition to form the porous asymmetric membrane. The polymer additive comprises hydrophilic functional groups, copolymerized hydrophilic monomers, or blocks of hydrophilic monomer repeat units. For example, the polymer additive can comprise a hydrophilic polymer or amphiphilic polymer. The porous asymmetric membrane can be a flat membrane or hollow fiber.