Abstract:
An electrical storage system is provided that has a thickness of less than 2 mm, where the system includes at least one sheet-type discrete element, the sheet-type discrete element exhibiting high resistance to an attack of alkali metals or alkali metal ions, in particular lithium, wherein the sheet-type discrete element has a low content of TiO2, the TiO2 content preferably being less than 2 wt %, preferably less than 0.5 wt %, and preferably free of TiO2.
Abstract:
An additive for electrochemical energy storages is disclosed, wherein the additive contains at least one silicon- and alkaline earth metal-containing compound V1 which in contact with a fluorine-containing compound V2 in the energy storage forms at least one compound V3 selected from the group consisting of silicon- and fluorine-containing, lithium-free compounds V3a, alkaline earth metal- and fluorine-containing, lithium-free compounds V3b, silicon-, alkaline earth metal- and fluorine-containing, lithium-free compounds V3c and combinations thereof. Also disclosed is an electrochemical energy storage containing the additive.
Abstract:
A glass ceramic containing lithium-ions and having a garnet-like main crystal phase having an amorphous proportion of at least 5% is disclosed. The garnet-like main crystal phase preferably has the chemical formula Li7+x−yMxIIM3−xIIIM2−yIVMyVO12, wherein MII is a bivalent cation, MIII is a trivalent cation, MIV is a tetravalent cation, MV is a pentavalent cation. The glass ceramic is prepared by a melting technology preferably within a Skull crucible and has an ion conductivity of at least 5·10−5 S/cm, preferably of at least 1·10−4 S/cm.
Abstract:
An additive for electrochemical energy storages is disclosed, wherein the additive contains at least one silicon- and alkaline earth metal-containing compound V1 which in contact with a fluorine-containing compound V2 in the energy storage forms at least one compound V3 selected from the group consisting of silicon- and fluorine-containing, lithium-free compounds V3a, alkaline earth metal- and fluorine-containing, lithium-free compounds V3b, silicon-, alkaline earth metal- and fluorine-containing, lithium-free compounds V3c and combinations thereof. Also disclosed is an electrochemical energy storage containing the additive.
Abstract:
The present invention relates to glasses having a composition made up of base glasses. The glasses have a good chemical toughenability in combination with an advantageous coefficient of thermal expansion. Owing to their composition and the production process, the homogeneity of the properties of the glasses at their surface is high compared to the bulk glass. Furthermore, the fragility of the glasses is low, so that they can be processed to produce very thin glass articles.
Abstract:
The present invention relates to glasses having a composition made up of base glasses. The glasses have a good chemical toughenability in combination with an advantageous coefficient of thermal expansion. Owing to their composition and the production process, the homogeneity of the properties of the glasses at their surface is high compared to the bulk glass. Furthermore, the fragility of the glasses is low, so that they can be processed to produce very thin glass articles.
Abstract:
The present disclosure relates to a bonding glass which has improved water resistance and has a coefficient of thermal expansion α(25-300) of from 14·10−6K−1 to 17·10−6K−1, comprising, in mol % on an oxide basis, 5-7 of B2O3, 10-14 of Al2O3, 36-43 of P2O5, 15-22 of Na2O, 12.5-20 of K2O, 2-6 of Bi2O3 and >0-6 of R oxide, where R oxide is an oxide selected from the group consisting of MnO2 and SiO2 and SnO2 and Ta2O5 and Nb2O5 and Fe2O3 and GeO2 and CaO. The bonding glass is free of PbO except for, at most, impurities. The bonding glass may have a glass transition temperature Tg of from 390° C. to 430° C. The present disclosure also relates to uses of this bonding glass.
Abstract:
A lithium-ion-conducting composite material is provided that includes at least one polymer and lithium-ion-conducting particles. The interfacial resistance for the lithium-ion conductivity between the polymer and the particles is reduced as a result of a surface modification of the particles and therefore the lithium-ion conductivity is greater than for a comparable composite material wherein the interfacial resistance between the polymer and the particles is not reduced.
Abstract:
An electrical storage system is provided that has a thickness of less than 2 mm, which includes at least one sheet-type discrete element. The sheet-type discrete element exhibits high resistance against an attack of transition metals or transition metal ions, in particular titanium, wherein the sheet-type discrete element contains titanium. The invention also relates to a sheet-type discrete element for use in an electrical storage system, which exhibits high resistance to the attack of transition metals or of transition metal ions, in particular titanium.
Abstract:
The present disclosure relates to a bonding glass which has improved water resistance and has a coefficient of thermal expansion α(25-300) of from 14·10−6K−1 to 17·10−6K−1, comprising, in mol % on an oxide basis, 5-7 of B2O3, 10-14 of Al2O3, 36-43 of P2O5, 15-22 of Na2O, 12.5-20 of K2O, 2-6 of Bi2O3 and >0-6 of R oxide, where R oxide is an oxide selected from the group consisting of MnO2 and SiO2 and SnO2 and Ta2O5 and Nb2O5 and Fe2O3 and GeO2 and CaO. The bonding glass is free of PbO except for, at most, impurities. The bonding glass may have a glass transition temperature Tg of from 390° C. to 430° C. The present disclosure also relates to uses of this bonding glass.