摘要:
A method of joining an amorphous alloy material to a heterogeneous material and a composite formed by the same are provided. The method comprises steps of: placing a pre-formed piece made of one of the amorphous alloy material and the heterogeneous material into a mold; heating the other of the amorphous alloy material and the heterogeneous material to a predetermined temperature, and casting the other of the amorphous alloy material and the heterogeneous material into the mold to form a transition connection part joining the amorphous alloy material to the heterogeneous material and having a fusion welded structure, a microstructure reinforcing connection structure and a composite connection structure; and cooling the amorphous alloy material and the heterogeneous material at a rate higher than a critical cooling rate of the amorphous alloy material to obtain a composite formed by joining the amorphous alloy material to the heterogeneous material by the transition connection part.
摘要:
A die-cast aluminum alloy and a preparation method and application thereof are disclosed. Based on the total weight of the aluminum alloy, the aluminum alloy includes: 8-11 wt % of Si, 2.5-5 wt % of Cu, 0.5-1.5 wt % of Mg, 0.1-0.3 wt % of Ni, 0.6-1.2 wt % of Fe, 0.1-0.3 wt % of Cr, 0.03-0.05 wt % of Sr, 0-0.3 wt % of Er, 80.25-88.1 wt % of Al, and 0.1 wt % or below of impurities.
摘要:
The present disclosure discloses a heat-conductive aluminum alloy and application thereof. The heat-conductive aluminum alloy contains alloying elements, unavoidable impurities and the balance of an aluminum element. Based on the total weight of the heat-conductive aluminum alloy, the alloying elements include: 5.0 to 11.0% by weight of Si, 0.4 to 1.0% by weight of Fe, 0.2 to 1.0% by weight of Mg, less than 0.1% by weight of Zn, less than 0.1% by weight of Mn, less than 0.1% by weight of Sr and less than 0.1% by weight of Cu. The heat-conductive aluminum alloy prepared by the present disclosure has a tensile strength of not less than 250 MPa, a yield strength of not less than 150 MPa, an elongation of not less than 3.5%, and a thermal conductivity of not less than 150 W/(m·K).
摘要:
A die-cast aluminum alloy and a preparation method and use thereof are disclosed. Based on the total mass of the die-cast aluminum alloy, the die-cast aluminum alloy includes: 4-9 wt % of Mg; 1.6-2.8 wt % of Si; 1.1-2 wt % of Zn; wt % of Mn; 0.1-0.3 wt % of Ti; 0.009-0.05 wt % of Be; the balance of Al; and less than 0.2 wt % of inevitable impurities.