Process for producing polyamide
    2.
    发明授权
    Process for producing polyamide 失效
    生产聚酰胺的方法

    公开(公告)号:US4810753A

    公开(公告)日:1989-03-07

    申请号:US921387

    申请日:1986-10-22

    摘要: Disclosed herein is a process for producing a polyamide comprising polymerizing at least one monomer of polyamide in the presence of(1) a hydrocarbon polymer having at least one group selected from the group consisting of a carboxyl group, a derivative group of carboxylic acid, an amino group, and a hydroxyl group, or(2) a polymer produced by reacting the hydrocarbon polymer with a polyamide, or polymerizing at least one monomer of polyamide in the presence of the hydrocarbon polymer.

    摘要翻译: 本文公开了一种制备聚酰胺的方法,其包括在(1)具有至少一个选自下组的烃聚合物存在下聚合至少一种聚酰胺单体:羧基,羧酸衍生物组, 氨基和羟基,或(2)通过烃聚合物与聚酰胺反应制备的聚合物,或在烃聚合物存在下聚合至少一种聚酰胺单体。

    Polyamide resin
    4.
    发明授权
    Polyamide resin 失效
    聚酰胺树脂

    公开(公告)号:US4921932A

    公开(公告)日:1990-05-01

    申请号:US228515

    申请日:1988-08-05

    IPC分类号: C08G69/34

    CPC分类号: C08G69/34

    摘要: A copolyamide resin containing a dimerized fatty acid as a copolymer component, which has (1) at least 25 equivalent %, based on the total number of terminal groups, of hydrocarbon groups having from 6 to 22 carbon atoms at its terminals, (2) a content of a dimerized fatty acid of from 0.1 to 40% by weight based on the total amount of the resin, and (3) a melt viscosity as measured at 240.degree. C. of from 2,000 to 15,000 poise.

    摘要翻译: 含有二聚脂肪酸作为共聚物成分的共聚酰胺树脂,其末端具有(1)至少25当量%的末端基团,具有6-22个碳原子的烃基的总数;(2) 基于树脂总量,二聚脂肪酸的含量为0.1〜40重量%,(3)在240℃下测定的熔融粘度为2000〜15000泊。

    Jointing structure of vehicle traveling path joints having expansion function and method of mounting elastic member therein
    7.
    发明授权
    Jointing structure of vehicle traveling path joints having expansion function and method of mounting elastic member therein 有权
    具有膨胀功能的车辆行驶路径接头的接合结构和其中安装弹性构件的方法

    公开(公告)号:US08602678B2

    公开(公告)日:2013-12-10

    申请号:US13413931

    申请日:2012-03-07

    IPC分类号: E01C11/02

    CPC分类号: E01D19/06

    摘要: A jointing structure comprising multiple steps provided face to face at the coaxially built traveling path ends with an expansion gap between, multiple elastic members respectively mounted inside the multiple steps, and a joint block mounted on the multiple elastic members across the expansion gap. Multiple supporting blocks and one or more than one intermediate joint block are mounted inside the multiple steps with the joint block between. The multiple supporting blocks, the joint block and the one or more than one intermediate joint block are of concrete. The elastic members are joined together across the expansion gap. The elastic member on one side is fixed to the inside of the step on one side and then subjected to deformation toward the bridge girder axis, and thereafter, the elastic member on the other side is fixed to the inside of the step on the other side.

    摘要翻译: 包括在同轴构造的行进路径上面对面设置的多个台阶的接合结构,分别安装在多个台阶内的多个弹性构件之间的膨胀间隙,以及安装在多个弹性构件上的膨胀间隙的接头块。 多个支撑块和一个或多于一个中间接合块安装在多个台阶内,其间具有接合块。 多个支撑块,接头块和一个或多个中间接头块是具体的。 弹性构件通过膨胀间隙连接在一起。 一侧的弹性部件固定在一侧的台阶的内侧,然后朝向桥梁轴线变形,此后,另一侧的弹性部件固定在台阶的另一侧的内侧 。

    Production method of aromatic polycarbonate
    9.
    发明授权
    Production method of aromatic polycarbonate 有权
    芳香族聚碳酸酯的生产方法

    公开(公告)号:US07754845B2

    公开(公告)日:2010-07-13

    申请号:US12064343

    申请日:2007-05-22

    IPC分类号: C08G64/00 C08G63/02

    CPC分类号: C08G64/307

    摘要: The object of the present invention is to provide a production method of a high molecular weight aromatic polycarbonate containing a reduced amount of a high melting point product, and having less thermal history received and excellent hue by a melt process. The present invention relates to a production method of an aromatic polycarbonate, characterized in that in producing an aromatic polycarbonate using an aromatic dihydroxy compound and a carbonic diester as raw materials and using plural reactors, a molten reactant temperature T1 (° C.) in at least one reactor A and a molten reactant temperature T2 (° C.) in a reactor B subsequent to the reactor A are satisfied with the relationship of T2

    摘要翻译: 本发明的目的是提供一种高分子量芳族聚碳酸酯的制造方法,该方法含有低熔点产物,并且具有较少的热历史记录和通过熔融加工具有优异的色调。 本发明涉及一种芳族聚碳酸酯的制造方法,其特征在于,在使用芳香族二羟基化合物和碳酸二酯作为原料制造使用多个反应器的芳香族聚碳酸酯时,将熔融反应物温度T1(℃) 反应器A之后的反应器B中的至少一个反应器A和熔融反应物温度T2(℃)满足T2

    Aromatic polycarbonate, process for producing the same, polycarbonate composition, and hollow container obtained from the same
    10.
    发明授权
    Aromatic polycarbonate, process for producing the same, polycarbonate composition, and hollow container obtained from the same 有权
    芳族聚碳酸酯,其制备方法,聚碳酸酯组合物和由其制得的中空容器

    公开(公告)号:US07084233B2

    公开(公告)日:2006-08-01

    申请号:US10813042

    申请日:2004-03-31

    IPC分类号: C08G64/00

    摘要: A subject for the invention is to provide a branched aromatic polycarbonate which is excellent in hue and in melt characteristics such as melt strength.The invention provides a branched aromatic polycarbonate having a viscosity-average molecular weight of 16,000 or higher obtained by the transesterification method, characterized in that the ratio of the weight-average molecular weight (Mw) to number-average molecular weight (Mn) as measured by gel permeation chromatography and calculated for standard polystyrene (Mw/Mn) is in the range of from 2.8 to 4.5 and that the proportion of the number of moles of all structural units yielded by a rearrangement reaction in the course of melt polymerization reaction to 1 mol of structural units having the framework of an aromatic dihydroxy compound used as a starting material is higher than 0.3 mol % and not higher than 0.95 mol.

    摘要翻译: 本发明的主题是提供一种色调和熔融特性如熔体强度优异的支链芳族聚碳酸酯。 本发明提供通过酯交换法得到的粘均分子量为16000以上的支链芳香族聚碳酸酯,其特征在于,测定的重均分子量(Mw)与数均分子量(Mn)的比例 通过凝胶渗透色谱法和标准聚苯乙烯(Mw / Mn)的计算值在2.8至4.5的范围内,并且在熔融聚合反应过程中通过重排反应产生的所有结构单元的摩尔数的比例为1 具有用作原料的芳族二羟基化合物的骨架的结构单元的摩尔数高于0.3摩尔%且不高于0.95摩尔。