Polyamide resin
    1.
    发明授权
    Polyamide resin 失效
    聚酰胺树脂

    公开(公告)号:US4921932A

    公开(公告)日:1990-05-01

    申请号:US228515

    申请日:1988-08-05

    IPC分类号: C08G69/34

    CPC分类号: C08G69/34

    摘要: A copolyamide resin containing a dimerized fatty acid as a copolymer component, which has (1) at least 25 equivalent %, based on the total number of terminal groups, of hydrocarbon groups having from 6 to 22 carbon atoms at its terminals, (2) a content of a dimerized fatty acid of from 0.1 to 40% by weight based on the total amount of the resin, and (3) a melt viscosity as measured at 240.degree. C. of from 2,000 to 15,000 poise.

    摘要翻译: 含有二聚脂肪酸作为共聚物成分的共聚酰胺树脂,其末端具有(1)至少25当量%的末端基团,具有6-22个碳原子的烃基的总数;(2) 基于树脂总量,二聚脂肪酸的含量为0.1〜40重量%,(3)在240℃下测定的熔融粘度为2000〜15000泊。

    Polyamide resin composition
    3.
    发明授权
    Polyamide resin composition 失效
    聚酰胺树脂组合物

    公开(公告)号:US4804720A

    公开(公告)日:1989-02-14

    申请号:US178224

    申请日:1988-04-06

    CPC分类号: C08K5/54 C08K3/36 C08K9/06

    摘要: Disclosed herein is a polyamide resin composition comprising a polyamide resin, from 0.1 to 1% by weight of fine silica based on the polyamide resin and from 1 to 99% by weight of a silane coupling agent based on the fine silica. The packaging material obtained from the polyamide resin composition of the present invention has uniform and satisfactory transparency and is excellent in the blocking resistance.

    摘要翻译: 本文公开了一种聚酰胺树脂组合物,其包含聚酰胺树脂,0.1至1重量%的基于聚酰胺树脂的二氧化硅和1至99重量%的基于二氧化硅微粒的硅烷偶联剂。 由本发明的聚酰胺树脂组合物得到的包装材料具有均匀且令人满意的透明性,耐粘连性优异。

    Water-in-oil emulsion process for producing an aromatic polycarbonate
    4.
    发明授权
    Water-in-oil emulsion process for producing an aromatic polycarbonate 失效
    用于生产芳族聚碳酸酯的油包水乳液工艺

    公开(公告)号:US5047497A

    公开(公告)日:1991-09-10

    申请号:US506093

    申请日:1990-04-09

    IPC分类号: C08G64/20 C08G64/24 C08G64/26

    CPC分类号: C08G64/24 C08G64/26

    摘要: A process for producing an aromatic polycarbonate in a water-in-oil emulsified form, having an improved heat stability during molding at a high temperature, is described. In the process according to the present invention, a tertiary amine is added to the water-to-oil emulsion after the average diameter of liquid droplets of the water phase is reduced to not more than 10.mu.m. The polycarbonate obtained by the process of the present invention is improved in heat stability and can provide a molded article with less coloration.