Polyurethane resin-based material for slush molding
    1.
    发明授权
    Polyurethane resin-based material for slush molding 有权
    用于搪塑的聚氨酯树脂基材料

    公开(公告)号:US07405257B2

    公开(公告)日:2008-07-29

    申请号:US10510905

    申请日:2003-04-08

    IPC分类号: C08L75/08

    摘要: The present invention provides a material for slush molding which is improved in melt properties during slush molding and is excellent in heat resistance, the material being made up of a thermoplastic polyurethane resin (A) the difference between the softening starting temperature (STi) and the softening ending temperature by TMA being from 0 to 30° C., and STi being 135 to 200° C. The resin (A) has a hard segment with an Mn of 200 to 2000 comprising a diisocyanate having a symmetrical structure, a low molecular-weight diamine having a symmetrical structure, and/or a low molecular-weight diol, the content of which being from 5 to 50 wt %, and a soft segment making up of a high molecular-weight diol with an Mn of 500 to 5000, with the aromatic content being 35 wt % or less and the aromatic ring content x and the urea group content y satisfying −0.1x+2.5≦y≦−0.1x+6.

    摘要翻译: 本发明提供一种用于搪塑的材料,其在搪塑期间的熔融性能得到改善并且耐热性优异,该材料由热塑性聚氨酯树脂(A)组成,软化起始温度(STi)与 软化结束温度为TMA为0〜30℃,STi为135〜200℃。树脂(A)具有Mn为200〜2000的硬链段,其包含对称结构的二异氰酸酯,低分子量 具有对称结构的重量二胺和/或低分子量二醇,其含量为5至50重量%,和由Mn分数为500至5000的高分子量二醇组成的软链段 ,芳香族含量为35重量%以下,芳香环含量x和尿素基含量y满足<β在线公式描述=“内联式”末端=“铅”→> -0.1x + 2.5 <= y <= - 0.1x + 6。<?in-line-formula description =“In-line Formulas”end =“tail “?>

    Polyurethane resin based slush molding material
    2.
    发明申请
    Polyurethane resin based slush molding material 有权
    聚氨酯树脂基搪塑料

    公开(公告)号:US20060045996A1

    公开(公告)日:2006-03-02

    申请号:US10510905

    申请日:2003-04-08

    IPC分类号: B60R13/00 C08G18/00

    摘要: The present invention provides a material for slush molding which is improved in melt properties during slush molding and is excellent in heat resistance, the material being made up of a thermoplastic polyurethane resin (A) the difference between the softening starting temperature (STi) and the softening ending temperature by TMA being from 0 to 30° C., and STi being 135 to 200° C. The resin (A) has a hard segment with an Mn of 200 to 2000 comprising a diisocyanate having a symmetrical structure, a low molecular-weight diamine having a symmetrical structure, and/or a low molecular-weight diol, the content of which being from 5 to 50 wt %, and a soft segment making up of a high molecular-weight diol with an Mn of 500 to 5000, with the aromatic content being 35 wt % or less and the aromatic ring content x and the urea group content y satisfying −0.1x+2.5≦y≦−0.1x+6.

    摘要翻译: 本发明提供一种用于搪塑的材料,其在搪塑期间的熔融性能得到改善并且耐热性优异,该材料由热塑性聚氨酯树脂(A)组成,软化起始温度(STi)与 软化结束温度为TMA为0〜30℃,STi为135〜200℃。树脂(A)具有Mn为200〜2000的硬链段,其包含对称结构的二异氰酸酯,低分子量 具有对称结构的重量二胺和/或低分子量二醇,其含量为5至50重量%,和由Mn分数为500至5000的高分子量二醇组成的软链段 ,芳香族含量为35重量%以下,芳香环含量x和尿素基含量y满足<β在线公式描述=“内联式”末端=“铅”→> -0.1x + 2.5 <= y <= - 0.1x + 6。 <?in-line-formula description =“In-line Formulas”end =“tail”?>