公开(公告)号:US09534089B2
公开(公告)日:2017-01-03
申请号:US14329884
申请日:2014-07-11
Applicant: The Boeing Company
Inventor: Chaoyin Zhou , Andrew P. Nowak , Richard E. Sharp , Wen Li , James E. French
IPC: C08L83/14 , C08G77/58 , C08G77/04 , C08G77/52 , C08G77/56 , C08K3/22 , C08G77/00 , C08G77/42 , C08L83/10
CPC classification number: C08G77/04 , C08G77/42 , C08G77/44 , C08G77/442 , C08G77/48 , C08G77/52 , C08G77/56 , C08G77/58 , C08G77/80 , C08K3/22 , C08K5/54 , C08K5/5415 , C08K5/57 , C08K2003/2241 , C08K2003/2265 , C08K2003/2272 , C08L83/10 , C08L83/14
Abstract: Methods and formulations for modified silicone resins of Formula (II) are presented. Formula (II) comprises at least one of each of the following subunits: The R1, R2, R3, R6, R7, R8, R9, R10, R11, R12 and R13 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl. The X is selected from a group consisting of arylene, transition metal, inorganic oxide, and silsesquioxane. The values oft ranges from 1 to 10, y ranges from 1 to 200 and z ranges from 1 to 1,000. The elastomeric materials prepared from modified silicone resins display robust mechanical properties following prolonged exposure to high temperatures (e.g., 316° C. or higher).
Abstract translation: 提出了式(II)的改性有机硅树脂和包含这种式(II)的改性有机硅树脂的弹性体制剂。 式(II)包含以下亚基中的至少一个:R 1,R 2,R 3,R 6,R 7,R 8,R 9,R 10,R 11,R 12和R 13为 各自独立地选自H,烷基,烯基,炔基和芳基。 X选自亚芳基,过渡金属,无机氧化物和倍半硅氧烷。 t的值范围为1至10,y的范围为1至200,z的范围为1至1,000。 由改性硅树脂制备的弹性体材料在长时间暴露于高温(例如316℃或更高)下显示出坚固的机械性能。
-
公开(公告)号:US20160009867A1
公开(公告)日:2016-01-14
申请号:US14329885
申请日:2014-07-11
Applicant: The Boeing Company
Inventor: Chaoyin Zhou , Andrew P. Nowak , Richard E. Sharp , Wen Li , James E. French
CPC classification number: C08L85/02 , C08G77/395 , C08G77/42 , C08G77/58 , C08G77/80 , C08G79/04 , C08K3/22 , C08K3/36 , C08K2003/2265 , C08L83/10
Abstract: Methods and formulations for modified silicone resins of Formula (I) are presented: The R1, R2, and R3 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl; n ranges from 1 to 10; m ranges from 1 to 200; and p ranges from 2 to 1,000. The elastomeric materials prepared from modified silicone resins display robust mechanical properties following prolonged exposure to high temperatures (e.g., 316° C. or higher).
Abstract translation: 呈现式(I)的改性有机硅树脂的方法和配方:R1,R2和R3各自独立地选自H,烷基,烯基,炔基和芳基; n范围从1到10; m范围从1到200; p范围从2到1,000。 由改性硅树脂制备的弹性体材料在长时间暴露于高温(例如316℃或更高)后显示出坚固的机械性能。
-
公开(公告)号:US09309359B2
公开(公告)日:2016-04-12
申请号:US14329885
申请日:2014-07-11
Applicant: The Boeing Company
Inventor: Chaoyin Zhou , Andrew P. Nowak , Richard E. Sharp , Wen Li , James E. French
CPC classification number: C08L85/02 , C08G77/395 , C08G77/42 , C08G77/58 , C08G77/80 , C08G79/04 , C08K3/22 , C08K3/36 , C08K2003/2265 , C08L83/10
Abstract: Methods and formulations for modified silicone resins of Formula (I) are presented: The R1, R2, and R3 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl; n ranges from 1 to 10; m ranges from 1 to 200; and p ranges from 2 to 1,000. The elastomeric materials prepared from modified silicone resins display robust mechanical properties following prolonged exposure to high temperatures (e.g., 316° C. or higher).
Abstract translation: 呈现式(I)的改性有机硅树脂的方法和配方:R1,R2和R3各自独立地选自H,烷基,烯基,炔基和芳基; n范围从1到10; m范围从1到200; p范围从2到1,000。 由改性硅树脂制备的弹性体材料在长时间暴露于高温(例如316℃或更高)后显示出坚固的机械性能。
-
公开(公告)号:US10189953B2
公开(公告)日:2019-01-29
申请号:US15389084
申请日:2016-12-22
Applicant: THE BOEING COMPANY
Inventor: Chaoyin Zhou , Andrew P. Nowak , Richard E. Sharp , Wen Li , James E. French
IPC: C08G77/48 , C08G77/04 , C08G77/52 , C08G77/58 , C08G77/56 , C08K3/22 , C08G77/42 , C08K5/54 , C08K5/57 , C08G77/00 , C08L83/10 , C08L83/14 , C08G77/442 , C08K5/5415 , C08G77/44
Abstract: Methods and formulations for modified silicone resins of Formula (II) are presented. Formula (II) comprises at least one of each of the following subunits: The R1, R2, R3, R6, R7, R8, R9, R10, R11, R12 and R13 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl. The X is selected from a group consisting of arylene, transition metal, inorganic oxide, and silsesquioxane. The values of t ranges from 1 to 10, y ranges from 1 to 200 and z ranges from 1 to 1,000. The elastomeric materials prepared from modified silicone resins display robust mechanical properties following prolonged exposure to high temperatures (e.g., 316° C. or higher).
-
公开(公告)号:US09932475B2
公开(公告)日:2018-04-03
申请号:US15061459
申请日:2016-03-04
Applicant: THE BOEING COMPANY
Inventor: Chaoyin Zhou , Andrew P. Nowak , Richard E. Sharp , Wen Li , James E. French
IPC: C08L75/02 , C08G79/04 , C08G77/395 , C08L85/02 , C08G77/58 , C08K3/22 , C08G77/42 , C08K3/36 , C08G77/00
CPC classification number: C08L85/02 , C08G77/395 , C08G77/42 , C08G77/58 , C08G77/80 , C08G79/04 , C08K3/22 , C08K3/36 , C08K2003/2265 , C08L83/10
Abstract: Methods and formulations for modified silicone resins of Formula (I) are presented: The R1, R2, and R3 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl; n ranges from 1 to 10; m ranges from 1 to 200; and p ranges from 2 to 1,000. The elastomeric materials prepared from modified silicone resins display robust mechanical properties following prolonged exposure to high temperatures (e.g., 316° C. or higher).
-
公开(公告)号:US10563017B2
公开(公告)日:2020-02-18
申请号:US15813701
申请日:2017-11-15
Applicant: THE BOEING COMPANY
Inventor: Chaoyin Zhou , Andrew P. Nowak , Richard E. Sharp , Wen Li , James E. French
IPC: C08G77/48 , C08G77/52 , C08G77/395 , C08G77/58 , C08G79/04 , C08K3/22 , C08L85/02 , C08K3/36 , C08G77/00
Abstract: Methods and formulations for modified silicone resins of Formula (I) are presented: The R1, R2, and R3 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl; n ranges from 1 to 10; m ranges from 1 to 200; and p ranges from 2 to 1,000. The elastomeric materials prepared from modified silicone resins display robust mechanical properties following prolonged exposure to high temperatures (e.g., 316° C. or higher).
-
公开(公告)号:US20160009864A1
公开(公告)日:2016-01-14
申请号:US14329884
申请日:2014-07-11
Applicant: The Boeing Company
Inventor: Chaoyin Zhou , Andrew P. Nowak , Richard E. Sharp , Wen Li , James E. French
CPC classification number: C08G77/04 , C08G77/42 , C08G77/44 , C08G77/442 , C08G77/48 , C08G77/52 , C08G77/56 , C08G77/58 , C08G77/80 , C08K3/22 , C08K5/54 , C08K5/5415 , C08K5/57 , C08K2003/2241 , C08K2003/2265 , C08K2003/2272 , C08L83/10 , C08L83/14
Abstract: Methods and formulations for modified silicone resins of Formula (II) are presented. Formula (II) comprises at least one of each of the following subunits: The R1, R2, R3, R6, R7, R8, R9, R10, R11, R12 and R13 are each independently selected from a group consisting of H, alkyl, alkenyl, alkynyl, and aryl. The X is selected from a group consisting of arylene, transition metal, inorganic oxide, and silsesquioxane. The values oft ranges from 1 to 10, y ranges from 1 to 200 and z ranges from 1 to 1,000. The elastomeric materials prepared from modified silicone resins display robust mechanical properties following prolonged exposure to high temperatures (e.g., 316° C. or higher).
Abstract translation: 提出了式(II)改性有机硅树脂的方法和配方。 式(II)包括以下亚基中的至少一个:R 1,R 2,R 3,R 6,R 7,R 8,R 9,R 10,R 11,R 12和R 13各自独立地选自H,烷基, 烯基,炔基和芳基。 X选自亚芳基,过渡金属,无机氧化物和倍半硅氧烷。 t值为1〜10,y为1〜200,z为1〜1,000。 由改性硅树脂制备的弹性体材料在长时间暴露于高温(例如316℃或更高)后显示出坚固的机械性能。
-
-
-
-
-
-