Method for manufacturing indium tin oxide nanowires
    5.
    发明授权
    Method for manufacturing indium tin oxide nanowires 有权
    铟锡氧化物纳米线的制造方法

    公开(公告)号:US08652648B2

    公开(公告)日:2014-02-18

    申请号:US13916774

    申请日:2013-06-13

    Abstract: A method for manufacturing indium tin oxide nanowires by preparing a solution that includes an indium-containing species, a tin-containing species and a polymeric material, wherein the solution has a molar ratio of tin to indium in a range from about 5 to about 15 percent, electrospinning fibers using the solution, and heating the fibers to a calcination temperature and maintaining the fibers at the calcination temperature for a predetermined calcination time.

    Abstract translation: 一种通过制备包含含铟物质,含锡物质和聚合材料的溶液来制造铟锡氧化物纳米线的方法,其中所述溶液的锡与铟的摩尔比在约5至约15的范围内 百分比,使用该溶液的静电纺丝纤维,并将纤维加热至煅烧温度,并将纤维保持在煅烧温度下一段预定的煅烧时间。

    METHOD FOR MANUFACTURING INDIUM TIN OXIDE NANOWIRES
    9.
    发明申请
    METHOD FOR MANUFACTURING INDIUM TIN OXIDE NANOWIRES 有权
    用于制造氧化锌纳米颗粒的方法

    公开(公告)号:US20130272953A1

    公开(公告)日:2013-10-17

    申请号:US13916774

    申请日:2013-06-13

    Abstract: A method for manufacturing indium tin oxide nanowires by preparing a solution that includes an indium-containing species, a tin-containing species and a polymeric material, wherein the solution has a molar ratio of tin to indium in a range from about 5 to about 15 percent, electrospinning fibers using the solution, and heating the fibers to a calcination temperature and maintaining the fibers at the calcination temperature for a predetermined calcination time.

    Abstract translation: 一种通过制备包含含铟物质,含锡物质和聚合材料的溶液来制造铟锡氧化物纳米线的方法,其中所述溶液的锡与铟的摩尔比在约5至约15的范围内 百分比,使用该溶液的静电纺丝纤维,并将纤维加热至煅烧温度,并将纤维保持在煅烧温度下一段预定的煅烧时间。