The object of the present invention is to provide a compact for producing a sintered alloy which allows a sintered alloy obtained by sintering the compact to have improved mechanical strength and wear resistance, a wear-resistant iron-based sintered alloy, and a method for producing the same. The wear-resistant iron-based sintered alloy is produced by: forming a compact for producing a sintered alloy from a powder mixture containing a hard powder, a graphite powder, and an iron-based powder by powder compacting; and sintering the compact for producing a sintered alloy while diffusing C in the graphite powder of the compact for producing a sintered alloy in hard particles that constitute the hard powder. The hard particles contain 10% to 50% by mass of Mo, 3% to 20% by mass of Cr, and 2% to 15% by mass of Mn, with the balance made up of incidental impurities and Fe, and the hard powder and the graphite powder contained in the powder mixture account for 5% to 60% by mass and 0.5% to 2.0% by mass of the total amount of the hard powder, the graphite powder, and the iron-based powder, respectively.
摘要:
Mixed powder that contains first hard particles, second hard particles, graphite particles, and iron particles is used to manufacture a sintered alloy. The first hard particle is a Fe—Mo—Cr—Mn based alloy particle, the second hard particle is a Fe—Mo—Si based alloy particle. The mixed powder contains 5 to 50 mass % of the first hard particles, 1 to 8 mass % of the second hard particles, and 0.5 to 1.0 mass % of the graphite particles when total mass of the first hard particles, the second hard particles, the graphite particles, and the iron particles is set as 100 mass %.
摘要:
A sintered alloy is produced from mixed powder containing first hard particles, second hard particles, graphite particles, and iron particles. The first hard particles are Fe—Mo—Ni—Co—Mn—Si—C-based alloy particles, the second hard particles are Fe—Mo—Si-based alloy particles, the mixed powder contains 5 to 50 mass % of the first hard particles, 1 to 8 mass % of the second hard particles, and 0.5 to 1.5 mass % of the graphite particles, when total mass of the first hard particles, the second hard particles, the graphite particles, and the iron particles is set as 100 mass %.
摘要:
A self-piercing rivet includes a head, an outer cylindrical part extending from the head and formed in a cylindrical shape, and an inner cylindrical part extending from the head, provided spaced apart inside the outer cylindrical part, and formed in a cylindrical shape. In the manufacturing method for a fastening structure, a self-piercing rivet is driven into an overlapping part of a first fastened member and a second fastened member to fasten the first fastened member and the second fastened member.
摘要:
A thickened part is formed in the first member. The thickened part has a protruded part that is convex on one side in the thickness direction of the first member, so that the thick portion is set thicker than the general portion as the other portion. At least a part of the second member overlaps a part of the first member that includes the thickened part from another side of the first member in the plate thickness direction, and the self-piercing rivet is driven into a fastening overlapped part that is a part that the second member overlaps the thickened part from a second member side, so as to fasten the first member and the second member.
摘要:
A vehicle skeleton structure, including: a die-cast skeleton body formed integrally and including a floor part configuring a vehicle cabin floor portion and a side member disposed at both sides, in a vehicle width direction, of the floor part and extending in a vehicle front-rear direction; and a severance origin point, the severance origin point being formed at the skeleton body, and the severance origin point configuring a starting point when at least a part of the side member is severed.
摘要:
According the present invention, an alloy powder for overlay welding that prevents generation of gas defects in a weld overlay alloy in order to improve the toughness and wear resistance of the weld overlay alloy is provided. The alloy powder is an alloy powder for overlay welding on a steel surface containing nitrogen, which is characterized in that it contains 30% to 45% by mass of Mo, 10% to 30% by mass of Ni, 0.2% to 0.6% by mass of C, and 0.30% to 2.0% by mass of Al, with the balance made up of incidental impurities and Co.
摘要:
A vehicle skeleton structure, including: a die-cast skeleton body formed integrally and including a floor part configuring a vehicle cabin floor portion and a side member extending from the floor part towards a vehicle front or a vehicle rear; a transverse concave bead, the transverse concave bead being formed at a leading end side of the side member in the skeleton body, and the transverse concave bead extending in at least one of a vehicle width direction or a vehicle vertical direction; and a longitudinal concave bead, the longitudinal concave bead being formed at a base end side of the side member in the skeleton body, and the longitudinal concave bead extending in a vehicle front-rear direction.
摘要:
Hard particles are incorporated as a starting material in a sintered alloy. The hard particles contain 20 to 60 mass % Mo and 3 to 15 mass % Mn, the balance being Fe and unavoidable impurities.
摘要:
A forged component having a chemical composition including, by mass %, C: 0.30 to 0.45%, Si: 0.05 to 0.35%, Mn: 0.50 to 0.90%, P: 0.030 to 0.070%, S: 0.040 to 0.070%, Cr: 0.01 to 0.50%, Al: 0.001 to 0.050%, V: 0.25 to 0.35%, Ca: 0 to 0.0100%, N: 0.0150% or less, and the balance being Fe and unavoidable impurities, and satisfying formula 1. Metal structure is a ferrite pearlite structure, and a ferrite area ratio is 30% or more. Vickers hardness is in the range of 320 to 380 HV. 0.2% yield strength is 800 MPa or more. A Charpy V-notch impact value is in the range of 7 to 15 J/cm2.