    摘要: A core material of an aluminum brazing sheet restricts Mg to less than 0.3 wt % and Fe to not more than 0.2 wt %, and contains more than 0.2 wt % and not more than 1.0 wt % of Cu, 0.3 to 1.3 wt % of Si, 0.3 to 1.5 wt % of Mn and the balance of Al and inevitable impurities. A brazing filler material is formed on one surface of the core material by Al—Si based aluminum alloy. Also, a cladding material is formed on the other surface of the core material, and contains less than 0.2 wt % of Si, 2.0 to 3.5 wt % of Mg, not less than 0.5 wt % and less than 2.0 wt % of Zn and the balance of Al and inevitable impurities. Further, the value (cladding material hardness)/(the core material hardness) that is a ratio of the hardness of the cladding material to the hardness of the core material is not more than 1.5.

    摘要翻译: 铝钎焊片的芯材将Mg抑制在0.3重量%以下,Fe:0.2重量%以下,含有0.2重量%以上且1.0重量%以下的Cu,0.3〜1.3重量%的Si ,Mn为0.3〜1.5重量%,余量由Al和不可避免的杂质构成。 通过Al-Si基铝合金在芯材的一个表面上形成钎料。 此外,在芯材的另一个表面上形成包覆材料,其含有少于0.2重量%的Si,2.0-3.5重量%的Mg,不小于0.5重量%且小于2.0重量%的Zn, 平衡Al和不可避免的杂质。 此外,包层材料的硬度与芯材的硬度的比值(包层材料硬度)/(芯材硬度)为1.5以下。

    Method of repairing aluminum heat exchanger
    2.
    发明授权
    Method of repairing aluminum heat exchanger 有权
    修理铝热交换器的方法

    公开(公告)号:US06620274B1

    公开(公告)日:2003-09-16

    申请号:US09639974

    申请日:2000-08-16

    IPC分类号: B32B3500

    摘要: A partly damaged aluminum heat exchanger such as an aluminum radiator is repaired by closing a hole in the damaged portion with an acrylic resin adhesive material. A certain area around the damaged portion is pressed down to form a cup-shaped depressed portion. The adhesive material is supplied to the depressed portion so that it is retained therein. Then, the adhesive material is hardened by curing it under the room temperature. The hardened adhesive material completely closes the hole with a sufficient thickness and strength because it is retained in the depressed portion. The adhesive material is cured in a relatively short time because the acrylic resin is used as the adhesive material.

    摘要翻译: 通过用丙烯酸树脂粘合剂材料封闭损坏部分的孔来修复铝散热器等部分损坏的铝热交换器。 受损部分周围的一定区域被压下以形成杯形凹陷部分。 将粘合剂材料供应到凹部,使其保持在其中。 然后,粘合剂材料通过在室温下固化来硬化。 硬化的粘合剂材料由于保持在凹陷部分中而以足够的厚度和强度完全封闭孔。 粘合剂材料在相对短的时间内固化,因为使用丙烯酸树脂作为粘合剂材料。

    ALUMINUM ALLOY BRAZING SHEET FOR HEAT EXCHANGER
    4.
    发明申请
    ALUMINUM ALLOY BRAZING SHEET FOR HEAT EXCHANGER 有权
    用于热交换器的铝合金制动片

    公开(公告)号:US20100112370A1

    公开(公告)日:2010-05-06

    申请号:US12519023

    申请日:2007-12-18

    IPC分类号: B23K35/02

    摘要: Disclosed is an aluminum alloy brazing sheet for heat exchangers, which has high strength after brazing, high corrosion resistance and excellent brazability. Specifically disclosed is an aluminum alloy brazing sheet (1a) for heat exchangers comprising a core member (2), a sacrificial member (3) formed on one side of the core member (2), and a brazing filler metal (4) formed on the other side of the core member (2) and composed of an Al—Si alloy. The sacrificial member (3) contains 0.03-0.30% by mass of Fe, 0.01-0.40% by mass of Mn, 0.4-1.4% by mass of Si, 2.0-5.5% by mass of Zn, not more than 0.05% by mass of Mg and the balance of Al and unavoidable impurities. In addition, the sacrificial member (3) has a crystal grain size of 100-400 & mgr;m after 5-minute heat treatment at 600 & ring;C during the brazing.

    摘要翻译: 公开了一种用于热交换器的铝合金钎焊片,其在钎焊后具有高强度,高耐腐蚀性和优异的钎焊性。 具体公开了一种用于热交换器的铝合金钎焊板(1a),其包括芯构件(2),形成在芯构件(2)的一侧上的牺牲构件(3)和形成在芯构件 芯体(2)的另一侧由Al-Si合金构成。 牺牲构件(3)含有0.03-0.30质量%的Fe,0.01〜0.40质量%的Mn,0.4〜1.4质量%的Si,2.0-5.5质量%的Zn,0.05质量% 的Mg和余量的Al和不可避免的杂质。 此外,牺牲构件(3)在钎焊期间在600℃环境下经过5分钟热处理后的晶粒尺寸为100-400μm。

    Automobile cooling system component
    5.
    发明授权
    Automobile cooling system component 有权
    汽车冷却系统部件

    公开(公告)号:US08474518B2

    公开(公告)日:2013-07-02

    申请号:US12531435

    申请日:2008-03-19

    IPC分类号: F28F9/02

    摘要: A tank body 125 comprising header tanks 120 of a radiator is composed with a polyamide composition containing polyamide 6,10, glass fiber, copper and nucleating agent. At this time, the polyamide composition contains, based on the total weight of the polyamide 6,10, the glass fiber, the copper and the nucleating agent, (a) 48.9 to 79.988 percent by weight of the polyamide 6,10, (b) 20 to 50 percent by weight of the glass fiber, (c) 0.002 to 0.1 percent by weight of the copper, and (d) 0.01 to 1.5 percent by weight of the nucleating agent, and the result of measuring half-crystallization time of the polyamide composition is 5 minutes or less. In addition, the polyamide 6,10 used has a relative viscosity, as measured in 98 percent sulfuric acid, of 2.3 to 2.9.

    摘要翻译: 包括散热器的集水箱120的罐体125由含有聚酰胺6,10,玻璃纤维,铜和成核剂的聚酰胺组合物构成。 此时,聚酰胺组合物含有聚酰胺6,10的总重量,玻璃纤维,铜和成核剂,(a)聚酰胺6,10,(b)的48.9〜79.988重量% )20〜50重量%的玻璃纤维,(c)0.002〜0.1重量%的铜,(d)0.01〜1.5重量%的成核剂,测定半结晶时间的结果 聚酰胺组合物为5分钟以下。 此外,使用的聚酰胺6,10具有2.3至2.9的98%硫酸中测得的相对粘度。

    AUTOMOBILE COOLING SYSTEM COMPONENT
    6.
    发明申请
    AUTOMOBILE COOLING SYSTEM COMPONENT 有权
    汽车冷却系统组件

    公开(公告)号:US20100116482A1

    公开(公告)日:2010-05-13

    申请号:US12531435

    申请日:2008-03-19

    IPC分类号: F28F9/02 C08K3/08

    摘要: A tank body 125 comprising header tanks 120 of a radiator is composed with a polyamide composition containing polyamide 6,10, glass fiber, copper and nucleating agent. At this time, the polyamide composition contains, based on the total weight of the polyamide 6,10, the glass fiber, the copper and the nucleating agent,(a) 48.9 to 79.988 percent by weight of the polyamide 6,10, (b) 20 to 50 percent by weight of the glass fiber, (c) 0.002 to 0.1 percent by weight of the copper, and (d) 0.01 to 1.5 percent by weight of the nucleating agent, and the result of measuring half-crystallization time of the polyamide composition is 5 minutes or less. In addition, the polyamide 6,10 used has a relative viscosity, as measured in 98 percent sulfuric acid, of 2.3 to 2.9.

    摘要翻译: 包括散热器的集水箱120的罐体125由含有聚酰胺6,10,玻璃纤维,铜和成核剂的聚酰胺组合物构成。 此时,聚酰胺组合物含有聚酰胺6,10的总重量,玻璃纤维,铜和成核剂,(a)聚酰胺6,10,(b)的48.9〜79.988重量% )20〜50重量%的玻璃纤维,(c)0.002〜0.1重量%的铜,(d)0.01〜1.5重量%的成核剂,测定半结晶时间的结果 聚酰胺组合物为5分钟以下。 此外,使用的聚酰胺6,10具有2.3至2.9的98%硫酸中测得的相对粘度。