摘要:
A cathode active material having a large capacity and improved charge/discharge cycle characteristics is disclosed. A battery has a cathode (2) having a cathode active material, an anode (3) and a non-aqueous electrolyte, and uses a cathode active material composed of a mixture of a first lithium-transition metal composite oxide containing Ni and Co and comprising a layer structure and a second lithium-transition metal composite oxide containing Ni and Mn and comprising a layer structure.
摘要:
A cathode active material and non-aqueous electrolyte secondary battery. The non-aqueous electrolyte secondary battery includes a positive electrode and a negative electrode which are electrochemically doped and dedoped with lithium; and an electrolyte disposed between the positive electrode and the negative electrode. The positive electrode contains a cathode active material including a mixture of: a first cathode active material represented by a general formula: LitCoMsO2 where M represents a metal, 0≦s≦0.03, and 0.05≦t≦1.15; and a second cathode active material represented by a general formula: LixNi(1-y-z)CoyMnzAaO2 where A represents a metal, 0.05≦x≦1.15, 0.15≦y+z≦0.70, 0.05≦z≦0.40, and 0≦a≦0.10.
摘要翻译:正极活性物质和非水电解质二次电池。 非水电解质二次电池包括电化学掺杂并脱锂的正极和负极; 以及设置在正极和负极之间的电解质。 正极含有阴极活性物质,该阴极活性物质包含以下通式的混合物:由以下通式表示的第一阴极活性物质:Li sub> >其中M表示金属,0 <= s <= 0.03,而0.05 <= t <= 1.15; 和由以下通式表示的第二阴极活性材料:Li x Ni(1-yz)Mn x Mn z 其中A表示金属,0.05 <= x <= 1.15,0.15 <= y + z <= 0.70,0.05 <= z < 0.40,0 <= a <= 0.10。
摘要:
A cathode active material having a large capacity and improved charge/discharge cycle characteristics is disclosed. A battery has a cathode (2) having a cathode active material, an anode (3) and a non-aqueous electrolyte, and uses a cathode active material composed of a mixture of a first lithium-transition metal composite oxide containing Ni and Co and comprising a layer structure and a second lithium-transition metal composite oxide containing Ni and Mn and comprising a layer structure.
摘要:
A cathode active material and non-aqueous electrolyte secondary battery. The non-aqueous electrolyte secondary battery includes a positive electrode and a negative electrode which are electrochemically doped and dedoped with lithium; and an electrolyte disposed between the positive electrode and the negative electrode. The positive electrode contains a cathode active material including a mixture of: a first cathode active material represented by a general formula: LitCoMsO2 where M represents a metal, 0≦s≦0.03, and 0.05≦t≦1.15; and a second cathode active material represented by a general formula: LixNi(1-y-z)CoyMnzAaO2 where A represents a metal, 0.05≦x≦1.15, 0.15≦y+z≦0.70, 0.05≦z≦0.40, and 0≦a≦0.10.
摘要翻译:阴极活性物质和非水电解质二次电池。 非水电解质二次电池包括电化学掺杂并脱锂的正极和负极; 以及设置在正极和负极之间的电解质。 正极含有阴极活性物质,该阴极活性物质包含以下通式的混合物:由以下通式表示的第一阴极活性物质:Li sub> >其中M表示金属,0 <= s <= 0.03,而0.05 <= t <= 1.15; 和由以下通式表示的第二阴极活性材料:Li x Ni(1-yz)Mn x Mn z 其中A表示金属,0.05 <= x <= 1.15,0.15 <= y + z <= 0.70,0.05 <= z < 0.40,0 <= a <= 0.10。
摘要:
A positive active material including a compound expressed by a general formula LimMxM′yM″zO2 (here, M designates at least one kind of element selected from Co, Ni and Mn, M′ designates at least one kind of element selected from Al, Cr, V, Fe, Cu, Zn, Sn, Ti, Mg, Sr, B, Ga, In, Si and Ge, and M″ designates at least one kind of element selected from Mg, Ca, B and Ga. Further, x is designated by an expression of 0.9≦x
摘要:
A cathode active material includes: (a) first oxide including (1) lithium (Li), nickel (Ni) and manganese, (2) a first element MI selected from Group 2 to Group 14 elements, and (3) oxygen; (b) a second oxide including (1) lithium, (2) a second element MII including nickel and cobalt, (3) manganese, (4) a third element including at least one of the elements of Group 2 to Group 14 elements, except for nickel, cobalt and manganese, and (5) oxygen.
摘要:
A secondary battery both having a cathode and an anode with a separator in between. The cathode comprises a stable complex oxide LixNi1-y-zMnyMIzO2 and a highly conductive complex oxide LisMIIl-t-uMntMIIIuO2. Each of MI and MIII includes at least one kind selected from the group consisting of elements in Group 2 through Group 14, and MII includes at least one kind selected from the group consisting of Ni and Co, and the values of x, y, z, s, t and u are within a range of 0.9≦x≦1.1, 0.25≦y≦0.45, 0.01≦z≦0.30, 0.9≦s≦1.1, 0.05≦t≦0.20, and 0.01≦u≦0.10, respectively.
摘要:
Provided are a cathode active material and a secondary battery both having a higher capacity and superior cycle characteristics and capable of obtaining a sufficient discharge capacity during large current discharge. A cathode (21) and an anode (22) with a separator (23) in between are spirally wound. The cathode (21) comprises a highly stable complex oxide LixNi1-y-zMnyMIzO2 and a highly conductive complex oxide Li8MII1-t-uMntMIIIuO2. Each of MI and MIII includes at least one kind selected from the group consisting of elements in Group 2 through Group 14, and MII includes at least one kind selected from the group consisting of Ni and Co, and the values of x, y, z, s, t and u are within a range of 0.9≦x
摘要翻译:提供具有较高容量和优异的循环特性并能够在大电流放电期间获得足够的放电容量的正极活性材料和二次电池。 具有隔膜(23)的阴极(21)和阳极(22)螺旋卷绕。 阴极(21)包括高度稳定的复合氧化物Li x Ni 1-y z Mn x Si z O 2和高导电性复合氧化物Li 3 MII 1-tu Mn 3 M 3 N 2 O 3 / 2&gt; 2&lt; 2&gt;。 MI和MIII中的每一个包括选自组2至组14中的元素中的至少一种,MII包括选自Ni和Co中的至少一种,x,y,z的值 ,s,t和u在0.9 <= x <1.1,0.25 <= y <=0.45,0.01≤z≤0.30,0.9≤s≤1.1,0.05≤t≤0.20的范围内,以及 0.01 <= u <= 0.10。 其中不同元素的取代量较大的高度稳定的复合氧化物和不同元素的取代量较小的高导电性复合氧化物混合,因此在大电流下具有优异的循环特性和足够的放电容量 可以实现放电。
摘要:
A positive electrode active material includes particles composed of a compound oxide; and coating layers composed of a compound oxide formed on at least parts of the surfaces of the particles. The particles have a layered structure and include a first compound oxide mainly composed of lithium and nickel. The coating layers include a second compound oxide mainly composed of lithium and titanium. The ratio by weight of the first compound oxide to the second compound oxide is between 96:4 and 65:35. The positive electrode active material has a mean particle diameter of 5 to 20 μm.
摘要:
A positive active material is composed of particles of a compound oxide of lithium and a transition metal. This compound oxide has a layered structure. A coating layer of an inorganic compound and a carbonaceous material is formed on at least part of each surface of the particles. The inorganic compound is a lithium compound. The weight ratio of the inorganic compound to the carbonaceous material ranges between 99:1 and 60:40. The weight ratio of the particles to the coating layers ranges between 98:2 and 70:30.