Method of maufacturing a tubular extrusion molding product comprising a
high molecular weight polyarylene sulfide
    1.
    发明授权
    Method of maufacturing a tubular extrusion molding product comprising a high molecular weight polyarylene sulfide 失效
    制造包含高分子量聚芳硫醚的管状挤压成型产品的方法

    公开(公告)号:US5777069A

    公开(公告)日:1998-07-07

    申请号:US658645

    申请日:1996-06-05

    IPC分类号: C08G75/02 C08G75/16

    摘要: A tubular extrusion molding product comprising a high molecular weight polyarylene sulfide having a melt viscosity of from 3,100 poise to 60,000 poise produced by reacting an alkali metal sulfide and a dihaloaromtic compound in the presence of an organic amide solvent, cooling a gaseous phase part in the reaction zone during the reaction thereby condensating at least a part of the gaseous phase and refluxing the resultant condensate to a liquid phase in the reaction zone. A tubular extrusion molding product having further improved impact resistance can be provided by copolymerizing from 0.2 mol % to 1 mol % of a polyhaloaromatic compound to the alkali metal sulfide. A tubular extrusion molding product of improved impact resistance is provided by further applying a heat treatment of the polyarylene sulfide intermediate product thereby increasing the melt viscosity.

    摘要翻译: 一种管状挤出成型产品,其包含通过在有机酰胺溶剂的存在下使碱金属硫化物和二卤代醇化合物反应而产生的熔体粘度为3,100泊至6万泊的高分子量聚芳硫醚,将有机酰胺溶剂中的气相部分冷却 在反应过程中由此使至少一部分气相冷凝并将所得冷凝物回流到反应区中的液相。 通过从0.2mol%至1mol%的多卤芳族化合物与碱金属硫化物共聚,可以提供具有进一步改善耐冲击性的管状挤出成型产品。 通过进一步施加聚芳硫醚中间体产品的热处理,提高耐冲击性的管状挤出成型产品,从而提高熔融粘度。

    Polyarylene sulfide and a composition thereof
    2.
    发明授权
    Polyarylene sulfide and a composition thereof 失效
    聚芳硫醚及其组合物

    公开(公告)号:US5945490A

    公开(公告)日:1999-08-31

    申请号:US952286

    申请日:1997-11-10

    IPC分类号: C08G75/02 C08K5/54 C08L81/02

    CPC分类号: C08G75/0254 C08K5/54

    摘要: Polyarylene sulfide (PAS) is disclosed, of which extract with methylene chloride is in an amount of not more than 0.7% by weight, a melt viscosity V.sub.6 is 20 to 15,000 poises and a content of --SX groups is at least 15 micro moles/g, wherein X represents an alkali metal or a hydrogen atom. The PAS is prepared as follows: an alkali metal sulfide is reacted with a dihaloaromatic compound in an organic amide solvent, while a part of a gaseous phase in a reactor is condensed by cooling a gaseous phase part of the reactor to return the condensed liquid to a liquid phase; and the polyarylene sulfide thus prepared is washed with an organic solvent and then with water. The present invention also provides a composition comprising 100 parts by weight of (A) the aforesaid PAS and 0.01 to 5.0 parts by weight of (B) at least a silane compound selected from the group consisting of methacryloxysilane compounds, ureidosilane compounds and epoxy silane compounds.

    摘要翻译: PCT No.PCT / JP97 / 01138 Sec。 371日期:1997年11月10日 102(e)日1997年11月10日PCT 1997年4月2日PCT公开了聚二硫醚(PAS),其中二氯甲烷的提取物的量不大于0.7重量%,熔体粘度V6为20〜 15000泊,-SX基团的含量为至少15微摩尔/ g,其中X表示碱金属或氢原子。 PAS如下制备:碱金属硫化物与二卤代芳族化合物在有机酰胺溶剂中反应,同时反应器中的一部分气相通过冷却反应器的气相部分而使冷凝的液体返回到 液相; 将由此制备的聚芳硫醚用有机溶剂洗涤,然后用水洗涤。 本发明还提供一种组合物,其包含100重量份(A)上述PAS和0.01至5.0重量份(B)至少一种选自甲基丙烯酰氧基硅烷化合物,脲基硅烷化合物和环氧硅烷化合物的硅烷化合物 。

    Process for the preparation of polyarylene sulfide
    3.
    发明授权
    Process for the preparation of polyarylene sulfide 失效
    制备聚芳硫醚的方法

    公开(公告)号:US06600009B2

    公开(公告)日:2003-07-29

    申请号:US08957414

    申请日:1997-10-24

    IPC分类号: C08G6502

    CPC分类号: C08G75/0254

    摘要: In the preparation of polyarylene sulfide (PAS) by reacting an alkali metal sulfide with a dihaloaromatic compound in an organic amide solvent to obtain a polyarylene sulfide slurry and subjecting the slurry to acid treatment, an acid or hydrogen salt is added to the slurry in such an amount that a pH of the slurry is more than 7.0 and at most 11.0 to carry out the acid treatment. Alternatively, a zinc compound in an amount of 0.1 to 1.5 mole % per mole of the alkali metal sulfide supplied is added to the polyarylene sulfide slurry to treat the slurry, and, then, an acid or hydrogen salt in an amount of at least 0.2 mole % per mole of the alkali metal sulfide supplied is added. The PAS thus obtained has high crystallization speed, high whiteness, high mechanical strength and high melt viscosity, V6.

    摘要翻译: 在通过碱金属硫化物与二卤代芳族化合物在有机酰胺溶剂中反应制备聚芳硫醚(PAS)以获得聚芳硫醚浆料并对浆料进行酸处理时,将酸或氢盐加入到浆料中 为了进行酸处理,浆料的pH为7.0以上且11.0以下的量。 或者,将供给的碱金属硫化物的摩尔数为0.1〜1.5摩尔%的锌化合物加入到聚芳硫醚浆料中以处理浆料,然后加入至少0.2重量的酸或氢盐 加入每摩尔供应的碱金属硫化物的摩尔%。由此获得的PAS具有高结晶速度,高白度,高机械强度和高熔体粘度V6。

    Process for controlling a particle size of polyarylene sulfide and polyarylene sulfide thus produced
    7.
    发明授权
    Process for controlling a particle size of polyarylene sulfide and polyarylene sulfide thus produced 失效
    用于控制由此制备的聚芳硫醚和聚芳硫醚的粒度的方法

    公开(公告)号:US06369191B1

    公开(公告)日:2002-04-09

    申请号:US08505620

    申请日:1995-07-21

    IPC分类号: C08G7514

    CPC分类号: C08G75/0254

    摘要: A particle size of polyarylene sulfide obtained in polymerization is controlled by a process characterized in that a gaseous phase part of a reactor is cooled or heated after starting decreasing a temperature of a reaction system o an end of precipitation of polyarylene sulfide formed In an embodiment, a water content in the reaction system is 0.8 to 1.7 moles per mole of the alkali metal sulfide; the gaseous phase part of the reactor is cooled in a polymerization stage to thereby condense a part of a gaseous phase in the reactor and the condensed liquid is refluxed to a liquid phase in the reactor; and the gaseous phase part is only cooled after starting decreasing the temperature of the reaction system, whereby high molecular weight polyarylene sulfide suitable for powder coating is formed, which has a weight average molecular weight of at least 30,000 and an average particle size of 50 to 80 &mgr;m, wherein particles of 40 to 150 &mgr;m account for at least 90% by weight of the whole particles in a particle size distribution, and the amount of particles of 180 &mgr;m or more is 0.5% lby weight or less.

    摘要翻译: 在聚合反应中获得的聚芳硫醚的粒度通过以下方法控制,其特征在于反应器的气相部分在开始之后被冷却或加热,降低了形成的聚芳硫醚的沉淀结束时的反应体系的温度。在一个实施方案中, 反应体系中的水含量为每摩尔碱金属硫化物0.8〜1.7摩尔; 将反应器的气相部分在聚合阶段中冷却,从而在反应器中冷凝一部分气相,并将冷凝的液体回流至反应器中的液相; 并且气相部分在开始降低反应体系的温度后才被冷却,由此形成适用于粉末涂料的高分子量聚芳硫醚,其重均分子量为至少30,000,平均粒径为50至 80μm,其中40-150μm的颗粒占整个颗粒的至少90重量%的粒度分布,并且180μm或更多的颗粒的量为0.5重量%以下。

    Process for controlling a particle size of polyarylene sulfide and
polyarylene sulfide thus produced
    9.
    发明授权
    Process for controlling a particle size of polyarylene sulfide and polyarylene sulfide thus produced 失效
    用于控制由此制备的聚芳硫醚和聚芳硫醚的粒度的方法

    公开(公告)号:US5475081A

    公开(公告)日:1995-12-12

    申请号:US151474

    申请日:1993-11-12

    IPC分类号: C08G75/02 C08G75/14

    CPC分类号: C08G75/0254

    摘要: A particle size of potyarylene sulfide obtained in polymerization is controlled by a process characterized in that a gaseous phase part of a reactor is cooled or heated after starting decreasing a temperature of a reaction system o an end of precipitation of polyarylene sulfide formed In an embodiment, a water content in the reaction system is 0.8 to 1.7 moles per mole of the alkali metal sulfide; the gaseous phase part of the reactor is cooled in a polymerization stage to thereby condense a part of a gaseous phase in the reactor and the condensed liquid is refluxed to a liquid phase in the reactor; and the gaseous phase part is only cooled after starting decreasing the temperature of the reaction system, whereby high molecular weight polyarylene sulfide suitable for powder coating is formed, which has a weight average molecular weight of at least 30,000 and an average particle size of 50 to 80 .mu.m, wherein particles of 40 to 150 .mu.m account for at least 90% by weight of the whole particles in a particle size distribution, and the amount of particles of 180 .mu.m or more is 0.5% by weight or less.

    摘要翻译: 通过以下方法控制在聚合中获得的聚亚芳基硫醚的粒度:其特征在于反应器的气相部分在开始之后冷却或加热,降低形成的聚芳硫醚沉淀的反应体系的温度。在一个实施方案中, 反应体系中的水含量为每摩尔碱金属硫化物0.8〜1.7摩尔; 将反应器的气相部分在聚合阶段中冷却,从而在反应器中冷凝一部分气相,并将冷凝的液体回流至反应器中的液相; 并且气相部分在开始降低反应体系的温度后才被冷却,由此形成适用于粉末涂料的高分子量聚芳硫醚,其重均分子量为至少30,000,平均粒径为50至 80μm,其中40〜150μm的粒子占粒径分布中的全部粒子的至少90重量%,并且180μm以上的粒子的量为0.5重量%以下。

    Polyarylenesulfide resin composition
    10.
    发明授权
    Polyarylenesulfide resin composition 有权
    聚芳硫醚树脂组合物

    公开(公告)号:US06492448B1

    公开(公告)日:2002-12-10

    申请号:US09613146

    申请日:2000-07-11

    IPC分类号: C08K322

    CPC分类号: C08L81/02 C08K3/22 C08K3/30

    摘要: A resin composition is provided which composition comprises 100 parts by weight of (A) polyarylene sulfide, and 0.01 to 5.0 parts by weight of (B) a product compound of an element selected from the group consisting of group IIA and group IIB of the periodic table, wherein said product compound has such alkalinity that a mixture of said product compound with a 20-fold weight of ultrapure water of grade A4 specified in the Japanese Industrial Standards (JIS) K0557 has a pH of from 10.0 to 12.0. The composition is particularly suited to be used for an optical instrument part such as an object lens driving unit and the like.

    摘要翻译: 提供了一种树脂组合物,其组合物包含100重量份的(A)聚芳硫醚,和0.01-5.0重量份的(B)选自下组的元素的产物化合物:IIA族和IIB族的定期 其中所述产物化合物具有这样的碱度,使得所述产物化合物与日本工业标准(JIS)K0557中规定的A4级超纯水的20倍重量的混合物具有10.0至12.0的pH。 该组合物特别适合用于诸如物镜驱动单元等的光学仪器部件。