摘要:
The present invention provides a catalyst for polyester production capable of producing a polyester with high catalytic activity and a process for producing a polyester using the catalyst. The catalyst for polyester production comprises a solid titanium compound which is obtained by dehydro-drying a hydrolyzate obtained by hydrolysis of a titanium halide and which has a molar ratio (OH/Ti) of a hydroxyl group (OH) to titanium (Ti) exceeding 0.09 and less than 4. The present invention also provides a method to obtain a polyester having a small increase of the acetaldehyde content during the molding. This method comprises bringing a polyester, which is obtained by the use of a titanium compound catalyst and in which the reaction has been completed, into contact with a phosphoric ester aqueous solution or the like having a concentration of not less than 10 ppm in terms of phosphorus atom. The present invention further provides a polyester having excellent transparency and tint and molded products of the polyester such as a blow molded article, a film, a sheet and a fiber. The polyester is obtained by polycondensing an aromatic dicarboxylic acid or an ester-forming derivative thereof and an aliphatic diol or an ester-forming derivative thereof in the presence of a catalyst for polyester production which comprises a polycondensation catalyst component comprising a solid titanium compound and a co-catalyst component comprising a magnesium compound. This polyester has a titanium content of 1 to 100 ppm, a magnesium content of 1 to 200 ppm and a weight ratio (Mg/Ti) of magnesium to titanium of not less than 0.01.
摘要:
The present invention provides a catalyst for polyester production capable of producing a polyester with high catalytic activity, a process for producing a polyester using the catalyst and a polyester produced thereby. The catalyst comprises a solid titanium compound obtained by dehydro-drying a hydrolyzate obtained by hydrolysis of a titanium halide and which has a molar ratio (OH/Ti) of a hydroxyl group (OH) to titanium (Ti) exceeding 0.09 and less than 4. In the process, the polyester is obtained by polycondensing an aromatic dicarboxylic acid, or an ester-forming derivative thereof, and an aliphatic diol, or ester-forming derivative thereof, in the presence of the catalyst. The resulting polyester has excellent transparency and tint, a titanium content of 1 to 100 ppm, a magnesium content of 1 to 200 ppm and a magnesium to titanium weight ratio of not less than 0.01.
摘要:
The present invention provides a catalyst for polyester production capable of producing a polyester with high catalytic activity, a process for producing a polyester using the catalyst and a polyester produced thereby. The catalyst comprises a solid titanium compound obtained by dehydro-drying a hydrolyzate obtained by hydrolysis of a titanium halide and which has a molar ratio (OH/Ti) of a hydroxyl group (OH) to titanium (Ti) exceeding 0.09 and less than 4. In the process, the polyester is obtained by polycondensing an aromatic dicarboxylic acid, or an ester-forming derivative thereof, and an aliphatic diol, or ester-forming derivative thereof, in the presence of the catalyst. The resulting polyester has excellent transparency and tint, a titanium content of 1 to 100 ppm, a magnesium content of 1 to 200 ppm and a magnesium to titanium weight ratio of not less than 0.01.
摘要:
Disclosed are polyester pellets made of a polyester which comprises dicarboxylic acid constituent units derived from dicarboxylic acids containing terephthalic acid and isophthalic acid and diol constituent units derived from diols containing ethylene glycol and 1,3-bis(2-hydroxyethoxy)benzene, and which has the properties: constituent units derived from terephthalic acid are 15 to 99.5% by mol and constituent units derived from isophthalic acid are 0.5 to 85% by mol, both based on the total amount of dicarboxylic acid isophthalic acid constituent units (i); constituent units derived from ethylene glycol are 25 to 99.5% by mol and constituent units derived from 1,3-bis(2-hydroxyethoxy)benzene are 0.5 to 75% by mol, both based on the total amount of the diol constituent units (ii); the intrinsic viscosity is in the range of 0.5 to 1.5 dl/g; and the melting point (Tm (°C.)), as measured by a differential scanning calorimeter, satisfies the formula [1/527−0.0017·ln(1−(mI+mB)/200)]−1−273
摘要:
A process for preparing polyester pellets which involves blending polyethylene terephthalate and polyethylene isophthalate copolymer before solid state polymerization, the polyethylene isophthalate copolymer being composed of dicarboxylic acid constituent units derived from dicarboxylic acids containing terephthalic acid and isophthalic acid and diol constituent units derived from diols containing ethylene glycol and 1,3-bis(2-hydroxyethoxy)benzene, palletizing the blend and crystallizing the pellets.
摘要:
A process for producing aliphatic polyester wherein a crystallized aliphatic polyester prepolymer formed from an aliphatic dihydric alcohol and an aliphatic dicarboxylic acid and having a weight-average molecular weight of 2,000 to 100,000 is caused to undergo solid-phase polymerization in the presence of a volatile catalyst to make an aliphatic polyester having a weight-average molecular weight of 50,000 to 1,000,000. This process is more efficient than any prior process calling for a complicated step for catalyst removal, since it enables the removal of the catalyst from the reaction system during and/or after solid-phase polymerization. The polyester is comparable in stability to any aliphatic polyester having any catalyst removed therefrom.
摘要:
The invention relates to a process for producing an aliphatic polyester excellent in stability which includes subjecting an aliphatic polyester containing at least 50% of an aliphatic hydroxycarboxylic acid unit, obtainable by solid-phase polymerization under a flowing gas in the presence of a volatile catalyst so as to have a desired weight average molecular weight within the range of 50,000 to 1,000,000, to a heat treatment at a temperature equal to or higher than the reaction temperature of the solid-phase polymerization under a flowing gas with maintaining the aliphatic polyester in a solid state. According to the process of the invention, an aliphatic polyester excellent in stability at molding and storage stability is obtained.
摘要:
The invention provides a process for producing high-molecular aliphatic polyesters capable of being substitutes for general-purpose resins that are required to have high toughness, in a simplified manner and at a high volume efficiency. Specifically, in the process, used as the starting material is an easily-available, low-molecular aliphatic polyester prepolymer to be prepared through polycondensation of inexpensive materials of an aliphatic hydroxycarboxylic acid such as lactic acid, glycolic acid or the like, an aliphatic polyalcohol such as butanediol or the like, and an aliphatic polycarboxylic acid such as succinic acid or the like, and the starting prepolymer is crystallized and thereafter polycondensed in a solid phase in the presence of a catalyst to give the intended, tough and high-molecular aliphatic polyester.