A method for producing a flat steel product with high reflectivity, in which at least one surface has an arithmetic mean roughness Ra of less than 0.03 μm includes providing a flat steel product, at least one surface of which has an arithmetic mean roughness Ra of less than 2.5 μm. The flat steel product is cold rolled in a plurality of rolling passes. Also a flat steel product with high reflectivity in the finished re-rolled state on at least one of its surface has a low arithmetic mean roughness, a high gloss, and a high directed reflection. A solar concentrator is produced from such a flat steel product.
摘要:
A method for producing a flat steel product with high reflectivity, in which at least one surface has an arithmetic mean roughness Ra of less than 0.03 μm includes providing a flat steel product, at least one surface of which has an arithmetic mean roughness Ra of less than 2.5 μm. The flat steel product is cold rolled in a plurality of rolling passes. Also a flat steel product with high reflectivity in the finished re-rolled state on at least one of its surface has a low arithmetic mean roughness, a high gloss, and a high directed reflection. A solar concentrator is produced from such a flat steel product.
摘要:
The invention relates to the use of a Q&P steel for production of a formed component (2) for high-wear applications, wherein the Q&P steel has a hardness of at least 230 HB, especially at least 300 HB, preferably at least 370 HB, and a bending angle α of at least 60°, especially at least 75°, preferably at least 85°, determined to VDA238-100, and/or a bending ratio of r/t