Polyimide resin composition
    3.
    发明授权
    Polyimide resin composition 失效
    聚酰亚胺树脂组合物

    公开(公告)号:US5580918A

    公开(公告)日:1996-12-03

    申请号:US157129

    申请日:1994-02-16

    CPC分类号: C08L71/00 C08L79/08

    摘要: A polyimide resin composition comprising 50-95 parts by weight of a polyimide resin represented by the following formula (1): ##STR1## wherein X represents a direct bond, a hydrocarbon group, a carbonyl group, a thio group or so, Y.sub.1 -Y.sub.4 individually represent a hydrogen atom, a lower alkyl group or so and R.sub.1 represents an aliphatic group, an aromatic group or so; and 50-5 parts by weight of a polyetheretherketone, said composition having been subjected to heat treatment at 250.degree.-330.degree. C. and, after the heat-treatment, having crystallization enthalpy of 0-6 cal/g.The heat treatment of the polyimide resin composition can be effected at a low temperature in a short time. The polyimide resin composition has excellent dimensional stability and high-temperature physical properties. Moreover, it has excellent moldability and peeling resistance.

    摘要翻译: PCT No.PCT / JP93 / 00515 Sec。 371日期:1994年2月16日 102(e)日期1994年2月16日PCT提交1993年4月21日PCT公布。 出版物WO93 / 21277 日期:1993年10月28日一种包含50-95重量份由下式(1)表示的聚酰亚胺树脂的聚酰亚胺树脂组合物:其中X表示直接键,烃基,羰基, 硫基等,Y1-Y4分别表示氢原子,低级烷基等,R1表示脂肪族基团,芳香族基团等。 和50-5重量份的聚醚醚酮,所述组合物在250-330℃下进行了热处理,并且在热处理之后,结晶焓为0-6cal / g。 聚酰亚胺树脂组合物的热处理可以在短时间内在低温下进行。 聚酰亚胺树脂组合物具有优异的尺寸稳定性和高温物理性能。 此外,其具有优异的成型性和耐剥离性。

    Polyimide based resin composition
    4.
    发明授权
    Polyimide based resin composition 失效
    聚酰亚胺基树脂组合物

    公开(公告)号:US5516837A

    公开(公告)日:1996-05-14

    申请号:US204433

    申请日:1994-03-02

    摘要: A molding resin composition comprising 99.9 to 50% by weight of polyimide represented by the formula: ##STR1## and 0.1 to 50% by weight of polyether ketone resin and/or polyester resin, and more particularly comprising the polyester resin capable of forming an anisotropical molten phase at a temperature of 420.degree. C. or less, and a polyimide-based molding resin composition which comprises the said resins and other additives such as phenolic resin, fluororesin, graphite, carbon fibers, aromatic polyamide fibers, potassium titanate fibers and a crystallization accelerator, and is excellent in thermal resistance, chemical resistance, mechanical strength and processability.

    摘要翻译: 一种模塑树脂组合物,其包含99.9至50重量%的由下式表示的聚酰亚胺:(I)和0.1-50重量%的聚醚酮树脂和/或聚酯树脂,更具体地包括能够 在420℃以下的温度下形成各向异性热熔融相,以及包含所述树脂和酚醛树脂,氟树脂,石墨,碳纤维,芳香族聚酰胺纤维,钛酸钾等其他添加剂的聚酰亚胺系成型树脂组合物 纤维和结晶促进剂,耐热性,耐化学性,机械强度和加工性优异。

    Laminate
    6.
    发明申请
    Laminate 审中-公开
    层压板

    公开(公告)号:US20100183881A1

    公开(公告)日:2010-07-22

    申请号:US12223175

    申请日:2007-01-24

    IPC分类号: B32B27/04

    摘要: In a coextrusion molding method, a laminate having excellent interlaminar adhesion strength with a fluorocopolymer is provided, and also a laminate which can be used more than enough even at high temperatures or in applications where the laminate comes into contact with oil, gasoline or the like by controlling various properties of the adhesive layer is provided.The laminate of the present invention is a laminate of at least two or more layers comprising a structure obtained by bonding and laminating an adhesive (A) defined by the following (i) to (iii) and a fluorocopolymer (B), wherein the adhesive (A) (i) is obtained by allowing a polyolefin (a) having a group reactive with a carbodiimide group to react with a compound (b) having a carbodiimide group, (ii) has a ratio of peak intensity at 2130 to 2140 cm−1 to peak intensity at 1470 cm−1 of 60% or lower in infrared absorption spectroscopy, and (iii) has a density of 0.870 to 0.940 g/cm3. In the formula (1), R1 and R2 each independently represent a hydrogen atom or fluorine atom. In the formula (2), R3 represents a substituent represented by CnH2n+1 (in which n is an integer of 1 or more).

    摘要翻译: 在共挤出成型方法中,提供了与含氟共聚物具有优异的层间粘合强度的层压体,以及即使在高温下也可以使用的层压体,或者在层压体与油,汽油等接触的应用中 通过控制粘合剂层的各种性质。 本发明的层压体是至少两层以上的层压体,其包含通过粘合和层压由下列(i)至(iii)限定的粘合剂(A)和含氟共聚物(B)而获得的结构,其中粘合剂 (A)(i)是通过使具有与碳二亚胺基反应的基团的聚烯烃(a)与具有碳二亚胺基的化合物(b)反应而获得的,(ii)峰强度的比例为2130〜2140cm -1在红外吸收光谱中在1470cm -1处的峰强度为60%以下,(iii)密度为0.870〜0.940g / cm 3。 在式(1)中,R 1和R 2各自独立地表示氢原子或氟原子。 在式(2)中,R 3表示由C n H 2n + 1表示的取代基(n为1以上的整数)。

    IONOMER RESIN COMPOSITION AND SHAPED ARTICLE OBTAINED FROM THE RESIN COMPOSITION
    7.
    发明申请
    IONOMER RESIN COMPOSITION AND SHAPED ARTICLE OBTAINED FROM THE RESIN COMPOSITION 审中-公开
    由树脂组合物获得的离子树脂组合物和成型品

    公开(公告)号:US20110028658A1

    公开(公告)日:2011-02-03

    申请号:US12935748

    申请日:2009-03-30

    IPC分类号: C08L33/00

    摘要: An ionomer resin composition according to the present invention is obtained by bringing a functional group-containing olefin copolymer (A) having a structural unit derived from a cyclic olefin in the range of 10 percent by mol or more and having a group derived from an acid and/or a derivative thereof as the functional group into contact with a metal compound (B). A shaped article having well-balanced two excellent properties of the optical characteristics and the moisture permeability can be formed by using the ionomer resin composition.

    摘要翻译: 本发明的离聚物树脂组合物是将来自环状烯烃的结构单元的含官能团的烯烃共聚物(A)的摩尔比为10摩尔%以上且具有来自酸的基团 和/或其衍生物作为官能团与金属化合物(B)接触。 通过使用离聚物树脂组合物可以形成具有良好平衡的两个优异的光学特性和透湿性的成形制品。

    AID FOR FILLER-REINFORCED RESINS, FILLER-REINFORCED POLYPROPYLENE RESIN COMPOSITION, AND MOLDED ARTICLE THEREOF
    8.
    发明申请
    AID FOR FILLER-REINFORCED RESINS, FILLER-REINFORCED POLYPROPYLENE RESIN COMPOSITION, AND MOLDED ARTICLE THEREOF 审中-公开
    填料增强树脂,填料增强聚丙烯树脂组合物及其模制品

    公开(公告)号:US20100311892A1

    公开(公告)日:2010-12-09

    申请号:US12734839

    申请日:2008-11-26

    IPC分类号: C08L33/24 C08F8/32

    摘要: An object of the present invention is to provide an aid for filler-reinforced resins, a filler-reinforced resin composition comprising the aid for filler-reinforced resins, and a molded article formed from the filler-reinforced resin composition. The above aid for filler-reinforced resins is capable of improving reinforcing properties and dispersibility of the filler in the filler-reinforced resin composition, and when the filler-reinforced resin composition is formed into a molded article, the aid for filler-reinforced resins enables the molded article to have superior mechanical characteristics, such as an impact resistance and a flexural strength. The present invention provides an aid (C) for filler-reinforced resins which is a modified polyolefin obtained by a reaction between a polyolefin resin (A) having a group reactive with a carbodiimide group and a compound (B) having a carbodiimide group, in which the content of the carbodiimide group to 100 g of the modified polyolefin is 1 to 200 mmol; a filler-reinforced resin composition comprising the aid (C) for filler-reinforced resins, a polypropylene-based resin (F), and a filler (G); and a molded article formed by molding the resin composition.

    摘要翻译: 本发明的一个目的是提供一种填料增强树脂的助剂,一种填料强化树脂组合物和一种由填料增强树脂组合物形成的模塑制品。 上述对填料强化树脂的助剂能够改善填料增强树脂组合物中填料的增强性能和分散性,并且当填料强化树脂组合物形成成型制品时,填料增强树脂的助剂能够 模制品具有优异的机械特性,例如耐冲击性和弯曲强度。 本发明提供一种用于填料增强树脂的助剂(C),其为通过具有与碳二亚胺基反应的基团的聚烯烃树脂(A)和具有碳二亚胺基团的化合物(B)之间的反应而获得的改性聚烯烃, 其中碳二亚胺基团与100g改性聚烯烃的含量为1〜200mmol; 包含用于填料强化树脂的助剂(C),聚丙烯类树脂(F)和填料(G))的填料强化树脂组合物。 以及通过模塑树脂组合物而形成的模制品。