公开(公告)号:US11866807B2
公开(公告)日:2024-01-09
申请号:US17290564
申请日:2020-04-24
Applicant: UACJ Corporation , UACJ EXTRUSION CORPORATION
Inventor: Taichi Suzuki , Kiyotake Sawa , Shuhei Shakudo
Abstract: An aluminum alloy pipe includes a pipe body portion made of an Al—Mg series alloy that includes Mg at a concentration equal to or higher than 0.7 mass % and lower than 2.5 mass % and Ti at a concentration higher than 0 mass % and equal to or lower than 0.15 mass %, with the balance being Al and unavoidable impurities, and a Zn-containing layer being outside the pipe body portion and including Zn being diffused in the Al—Mg series alloy at a concentration equal to or higher than 0.1 mass %.
-
公开(公告)号:US20180347017A1
公开(公告)日:2018-12-06
申请号:US15777798
申请日:2016-11-18
Applicant: UACJ CORPORATION
Inventor: Taichi Suzuki , Hidenori Hatta , Shuhei Shakudo
Abstract: An aluminum alloy material as one aspect of the present disclosure has a chemical composition including: Zn: more than 6.5% (mass %, same applies hereafter) and 8.5% or less; Mg: 0.5% or more and 1.5% or less; Cu: 0.10% or less; Fe: 0.30% or less; Si: 0.30% or less; Mn: less than 0.05%; Cr: less than 0.05%; Zr: 0.05% or more and 0.10% or less; and Ti: 0.001% or more and 0.05% or less, a balance including Al and inevitable impurities. In the aluminum alloy material, a mass ratio of Zn to Mg (Zn/Mg) is 5 or more and 16 or less, and a metallographic structure includes an equigranular recrystallized structure.
-
3.
公开(公告)号:US20240247355A1
公开(公告)日:2024-07-25
申请号:US18583027
申请日:2024-02-21
Applicant: UACJ CORPORATION
Inventor: Shuhei Shakudo , Ken Atsuta
IPC: C22F1/053 , B23K9/23 , B23K31/00 , B23K103/10 , C22C21/10
CPC classification number: C22F1/053 , B23K9/23 , B23K31/00 , C22C21/10 , B23K2103/10
Abstract: A production method of producing a welded structural member with excellent stress corrosion cracking resistance that includes a first artificial aging treatment step of maintaining a 7000-series aluminum alloy material at a temperature of 90 to 110° C. for 1 to 5 hours, a second artificial aging treatment step of maintaining the 7000-series aluminum alloy material subjected to the first artificial aging treatment step at a temperature of 145 to 160° C. for 4 to 12 hours; a welding step of welding the 7000-series aluminum alloy material subjected to the second artificial aging treatment step with another aluminum alloy material to form a welded structure; and a heat treatment step of heat-treating the welded structure at a temperature of 165 to 195° C. for 10 to 60 minutes. The material includes Zn, Mg, Zr, Ti, Cu, Mn, Cr, and Al, and is formed of a metallographic structure that is of a fibrous structure.
-
-