摘要:
A method for producing a thick film includes disposing a precursor solution onto a substrate to form a precursor film. The precursor solution contains precursor components to a rare-earth/alkaline-earth-metal/transition-metal oxide including a salt of a rare earth element, a salt of an alkaline earth metal, and a salt of a transition metal in one or more solvents, wherein at least one of the salts is a fluoride-containing salt, and wherein the ratio of the transition metal to the alkaline earth metal is greater than 1.5. The precursor solution is treated to form a rare earth-alkaline earth-metal transition metal oxide superconductor film having a thickness greater than 0.8 μm. precursor solution.
摘要:
A superconducting wire includes first and second superconducting layers disposed on one or more substrates in stacked relationship, the first superconducting layer comprising a high temperature superconducting oxide of a first composition and the second superconducting layer comprising a high temperature superconducting layer of a second composition, wherein the first and second compositions are different. The first superconductor layer optionally includes a high temperature superconductor composition selected to provide enhanced critical current (Ic(c)) in the presence of magnetic fields perpendicular to surface of the superconducting layer (H//c). The second superconductor layer optionally includes a high temperature superconductor composition selected to provide enhanced critical current (Ic) in the presence of magnetic fields parallel to surface of the superconducting layer (H//ab).
摘要:
A method for producing a thick film includes disposing a precursor solution onto a substrate to form a precursor film. The precursor solution contains precursor components to a rare-earth/alkaline-earth-metal/transition-metal oxide including a salt of a rare earth element, a salt of an alkaline earth metal, and a salt of a transition metal in one or more solvents, wherein at least one of the salts is a fluoride-containing salt, and wherein the ratio of the transition metal to the alkaline earth metal is greater than 1.5. The precursor solution is treated to form a rare earth-alkaline earth-metal transition metal oxide superconductor film having a thickness greater than 0.8 μm. precursor solution.
摘要:
A superconducting wire includes first and second superconducting layers disposed on one or more substrates in stacked relationship, the first superconducting layer comprising a high temperature superconducting oxide of a first composition and the second superconducting layer comprising a high temperature superconducting layer of a second composition, wherein the first and second compositions are different. The first superconductor layer optionally includes a high temperature superconductor composition selected to provide enhanced critical current (Ic(c)) in the presence of magnetic fields perpendicular to surface of the superconducting layer (H//c). The second superconductor layer optionally includes a high temperature superconductor composition selected to provide enhanced critical current (Ic) in the presence of magnetic fields parallel to surface of the superconducting layer (H//ab).
摘要:
A method for producing a thin film includes disposing a precursor solution onto a substrate to form a precursor film. The precursor solution contains precursor components to a rare-earth/alkaline-earth-metal/transition-metal oxide including a salt of a rare earth element, a salt of an alkaline earth metal, and a salt of a transition metal in one or more solvents, wherein at least one of the salts is a fluoride-containing salt. The precursor solution also contains an additive component comprising one or more metal compounds capable of forming a second phase nanoparticle, either alone or in combination with one or more of the precursor components of the precursor solution or a dopant component comprising one or more metal compounds capable of substituting for an element of the rare-earth/alkaline-earth-metal/transition-metal oxide, and treating the precursor film to form an intermediate metal oxyfluoride including the rare earth, the alkaline earth metal, the transition metal and the additive metal or dopant metal of the precursor solution.
摘要:
A method for producing a thick film includes disposing a precursor solution onto a substrate to form a precursor film. The precursor solution contains precursor components to a rare-earth/alkaline-earth-metal/transition-metal oxide including a salt of a rare earth element, a salt of an alkaline earth metal, and a salt of a transition metal in one or more solvents, wherein at least one of the salts is a fluoride-containing salt, and wherein the ratio of the transition metal to the alkaline earth metal is greater than 1.5. The precursor solution is treated to form a rare earth-alkaline earth-metal transition metal oxide superconductor film having a thickness greater than 0.8 μm. precursor solution.
摘要:
A method for producing a thick film includes disposing a precursor solution onto a substrate to form a precursor film. The precursor solution contains precursor components to a rare-earth/alkaline-earth-metal/transition-metal oxide including a salt of a rare earth element, a salt of an alkaline earth metal, and a salt of a transition metal in one or more solvents, wherein at least one of the salts is a fluoride-containing salt, and wherein the ratio of the transition metal to the alkaline earth metal is greater than 1.5. The precursor solution is treated to form a rare earth-alkaline earth-metal transition metal oxide superconductor film having a thickness greater than 0.8 μm. precursor solution.
摘要:
Under one aspect, a method of making a superconductor wire includes providing an oxide superconductor layer overlaying a substrate; forming a substantially continuous barrier layer over the oxide superconductor layer, the barrier layer including metal; depositing a layer of metal particles over the barrier layer, said depositing including applying a liquid including metal particles over the barrier layer; and sintering the layer of metal particles to form a substantially continuous metal layer over the barrier layer. In one or more embodiments, the oxide superconductor layer is oxygen-deficient, and the method may include oxidizing the oxygen-deficient oxide superconductor layer. At least a portion of the sintering and the oxidizing may occur simultaneously, for example by performing them at an oxygen partial pressure and a temperature sufficient to both sinter the metal particles and to oxidize the oxygen-deficient oxide superconductor layer.
摘要:
Under one aspect, a method of making a superconductor wire includes providing an oxide superconductor layer overlaying a substrate; forming a substantially continuous barrier layer over the oxide superconductor layer, the barrier layer including metal; depositing a layer of metal particles over the barrier layer, said depositing including applying a liquid including metal particles over the barrier layer; and sintering the layer of metal particles to form a substantially continuous metal layer over the barrier layer. In one or more embodiments, the oxide superconductor layer is oxygen-deficient, and the method may include oxidizing the oxygen-deficient oxide superconductor layer. At least a portion of the sintering and the oxidizing may occur simultaneously, for example by performing them at an oxygen partial pressure and a temperature sufficient to both sinter the metal particles and to oxidize the oxygen-deficient oxide superconductor layer.