摘要:
According to one embodiment, a supercritical drying method for a semiconductor substrate includes introducing a semiconductor substrate formed with a metal film into a chamber, the surface of the substrate being wet with alcohol, supplying a supercritical fluid of carbon dioxide into the chamber, setting a temperature inside the chamber to a predetermined temperature, to replace the alcohol on the semiconductor substrate with the supercritical fluid, and discharging the supercritical fluid and the alcohol from the chamber while keeping the temperature inside the chamber at the predetermined temperature, to lower a pressure inside the chamber. The predetermined temperature is not lower than 75° C. but lower than a critical temperature of the alcohol.
摘要:
In one embodiment, after rinsing a semiconductor substrate having a fine pattern formed thereon with pure water, the pure water staying on the semiconductor substrate is substituted with a water soluble organic solvent, and then, the semiconductor substrate is introduced into a chamber in a state wet with the water soluble organic solvent. Then, the water soluble organic solvent is turned into a supercritical state by increasing a temperature inside of the chamber. Thereafter, the inside of the chamber is reduced in pressure while keeping the inside of the chamber at a temperature enough not to liquefy the pure water (i.e., rinsing pure water mixed into the water soluble organic solvent), and further, the water soluble organic solvent in the supercritical state is changed into a gaseous state, to be discharged from the chamber, so that the semiconductor substrate is dried.
摘要:
According to one embodiment, a supercritical drying method for a semiconductor substrate includes introducing a semiconductor substrate formed with a metal film into a chamber, the surface of the substrate being wet with alcohol, supplying a supercritical fluid of carbon dioxide into the chamber, setting a temperature inside the chamber to a predetermined temperature, to replace the alcohol on the semiconductor substrate with the supercritical fluid, and discharging the supercritical fluid and the alcohol from the chamber while keeping the temperature inside the chamber at the predetermined temperature, to lower a pressure inside the chamber. The predetermined temperature is not lower than 75° C. but lower than a critical temperature of the alcohol.
摘要:
According to one embodiment, a supercritical drying method comprises cleaning a semiconductor substrate with a chemical solution, rinsing the semiconductor substrate with pure water after the cleaning, changing a liquid covering a surface of the semiconductor substrate from the pure water to alcohol by supplying the alcohol to the surface after the rinsing, guiding the semiconductor substrate having the surface wetted with the alcohol into a chamber, discharging oxygen from the chamber by supplying an inert gas into the chamber, putting the alcohol into a supercritical state by increasing temperature in the chamber to a critical temperature of the alcohol or higher after the discharge of the oxygen, and discharging the alcohol from the chamber by lowering pressure in the chamber and changing the alcohol from the supercritical state to a gaseous state. The chamber contains SUS. An inner wall face of the chamber is subjected to electrolytic polishing.
摘要:
According to one embodiment, a semiconductor substrate having a surface wetted with a chemical solution is introduced into a chamber, and a supercritical fluid is supplied into the chamber. The temperature in the chamber is adjusted to the critical temperature of the chemical solution or higher, so that the chemical solution is put into a supercritical state. The pressure in the chamber is then lowered, and the chemical solution in the critical state is turned into gaseous matter. The gaseous matter is then discharged from the chamber.
摘要:
In one embodiment, after rinsing a semiconductor substrate having a fine pattern formed thereon with pure water, the pure water staying on the semiconductor substrate is substituted with a water soluble organic solvent, and then, the semiconductor substrate is introduced into a chamber in a state wet with the water soluble organic solvent. Then, the water soluble organic solvent is turned into a supercritical state by increasing a temperature inside of the chamber. Thereafter, the inside of the chamber is reduced in pressure while keeping the inside of the chamber at a temperature enough not to liquefy the pure water (i.e., rinsing pure water mixed into the water soluble organic solvent), and further, the water soluble organic solvent in the supercritical state is changed into a gaseous state, to be discharged from the chamber, so that the semiconductor substrate is dried.
摘要:
Certain embodiments provide a supercritical drying device, comprising a sealable first vessel; a fluorine adsorbent provided inside the first vessel; a second vessel being provided inside the first vessel and housing a semiconductor substrate; a heater heating the inside of the first vessel; a pipe connected to the first vessel; and a valve provided on the pipe. Free fluorine generated by heating a fluorine containing solvent is adsorbed to the fluorine adsorbent.
摘要:
According to one embodiment, a substrate having a plurality of adjacent patterns on one surface thereof is cleaned by cleaning liquid. Subsequently, after the cleaning liquid is displaced with pure water, the pure water is displaced with displacement liquid. Under a condition that the displacement liquid among the patterns does not vaporize, the displacement liquid not contributing to prevention of collapse of the patterns is removed. After the displacement liquid is removed, the substrate is held in supercritical fluid and the displacement liquid among the patterns is displaced with the supercritical fluid. After the displacement liquid among the patterns is displaced with the supercritical fluid, the supercritical fluid adhering to the substrate is vaporized.
摘要:
According to one embodiment, a supercritical drying method for a semiconductor substrate, comprises introducing the semiconductor substrate into a chamber in a state, a surface of the semiconductor substrate being wet with alcohol, substituting the alcohol on the semiconductor substrate with a supercritical fluid of carbon dioxide by impregnating the semiconductor substrate to the supercritical fluid in the chamber, and discharging the supercritical fluid and the alcohol from the chamber and reducing a pressure inside the chamber. The method further comprises performing a baking treatment by supplying an oxygen gas or an ozone gas to the chamber after the reduction of the pressure inside the chamber.
摘要:
A substrate processing method and apparatus which can remove an anti-drying liquid, which has entered a three-dimensional pattern with recessed portions formed in a substrate, in a relatively short time. The substrate processing method includes the steps of: carrying a substrate, having a three-dimensional pattern formed in a surface, into a processing container, said pattern being covered with an anti-drying liquid that has entered the recessed portions of the pattern; heating the substrate and supplying a pressurizing gas or a fluid in a high-pressure state into the processing container, thereby forming a high-pressure atmosphere in the processing container before the anti-drying liquid vaporizes to such an extent as to cause pattern collapse and bringing the anti-drying liquid into a high-pressure state while keeping the liquid in the recessed portions of the pattern; and thereafter discharging a fluid in a high-pressure state or a gaseous state from the processing container.