    摘要: A method of preparing a positive active material for a rechargeable lithium battery including a) mixing a composite metal precursor and a lithium compound; b) firing the mixture to prepare a positive active material; c) mixing the resulting positive active material, a carbon coating material, and a solvent; and d) heat-treating the resulting mixture to provide a positive active material coated with the carbon coating material, wherein the carbon coating material is used in an amount of 1 wt % to 30 wt % based on 100 wt % of the composite metal precursor, lithium compound, and carbon coating material, the firing is performed at 400 to 900° C., and the positive active material provided in d) is represented by the following Chemical Formula 1, is provided. LiaNixCoyMnzM′kO2   [Chemical Formula 1] In Chemical Formula 1, each definition is the same as in the detailed description.

    摘要翻译: 一种制备用于可再充电锂电池的正极活性材料的方法,包括:a)混合复合金属前体和锂化合物; b)烧制混合物以制备正极活性物质; c)将得到的正极活性物质,碳涂层材料和溶剂混合; 和d)对所得混合物进行热处理以提供涂覆有碳涂层材料的正极活性材料,其中所述碳涂层材料的使用量相对于所述复合金属前体的100重量%为1重量%至30重量% ,锂化合物和碳涂层材料,在400-900℃下进行焙烧,并且提供d)中提供的正极活性材料由以下化学式1表示。 LiaNixCoyMnzM'kO2 [化学式1]在化学式1中,每个定义与详细描述相同。