摘要:
Disclosed is a thermoplastic composition including at least one semi-aromatic polyamide having a glass transition equal to or greater than 100° C. and a melting point of equal to or greater than 280° C.; a thermally conducting filler having a thermal conductivity of at least 5 W/mK, for instance CaF2 powder; and at least one hyperbranched polyesteramide having terminal hydroxy groups; and molded articles made therefrom.
摘要:
Disclosed is a thermoplastic composition including at least one semi-aromatic polyamide having a glass transition equal to or greater than 100° C. and a melting point of equal to or greater than 280° C., at least one hyperbranched aromatic polyamide having terminal alkylcarboxamide groups, and, optionally a thermally conductive filler; and molded articles made therefrom.
摘要:
Disclosed is a thermoplastic composition including at least one semi-aromatic polyamide having a glass transition equal to or greater than 100° C. and a melting point of equal to or greater than 280° C.; a thermally conducting filler having a thermal conductivity of at least 5 W/mK, for instance CaF2 powder; and at least one hyperbranched polyesteramide having terminal hydroxy groups; and molded articles made therefrom.
摘要:
Polyamide compositions containing semi-crystalline polyamide, amorphous polyamide, non-halogenated flame retardant, zinc borate and fillers that have a high stiffness and hardness, a low warpage, and external appearance, such as gloss and reduced corrosion effects on melt processing equipment.
摘要:
Disclosed is polyamide resin composition including a polyamide resin, at least one reinforcing agent, and at least one flame retardant, wherein, (a) the polyamide resin includes at least one aliphatic polyamide and an aromatic polyamide blend including at least one semi-crystalline semi-aromatic polyamide and at least one amorphous semi-aromatic polyamide; (b) based on the total weight of the polyamide resin, about 35 to about 70 wt % of the at least one aliphatic polyamide and about 30 to about 65 wt % of the aromatic polyamide blend are present in the polyamide resin; and (c) based on the total weight of the aromatic polyamide blend, about 15 to about 80 wt % of the at least one semi-crystalline semi-aromatic polyamide and about 20 to about 85 wt % of the at least one amorphous semi-aromatic polyamide are present in the aromatic polyamide blend.