摘要:
The invention relates to a process for producing a water-absorbing material by coating water-absorbing polymer particles with a film-forming polyurethane and silica, heat treating the coated particles and coating the heat-treated particles with pyrogenic hydrophilic silica. The invention further relates to the water-absorbing material obtainable according to the process of the invention. The water-absorbing material has improved wicking ability (FHA) and core shell saline flow conductivity (CS-SFC).
摘要:
The invention relates to a process for producing a water-absorbing material by coating water-absorbing polymer particles with a film-forming polyurethane and silica, heat treating the coated particles and coating the heat-treated particles with pyrogenic hydrophilic silica. The invention further relates to the water-absorbing material obtainable according to the process of the invention. The water-absorbing material has improved wicking ability (FHA) and core shell saline flow conductivity (CS-SFC).
摘要:
The invention relates to a process for producing a water-absorbing material by coating water-absorbing polymer particles with a film-forming polyurethane and pyrogenic silica and heat treating the coated particles. The invention further relates to the water-absorbing material obtainable according to the process of the invention. The water-absorbing material has improved wicking ability (FHA) and fixed swell rate (FSR).
摘要:
The use of water-absorbing polymer particles for dewatering feces, the water-absorbing polymer particles being obtainable by polymerizing a foamed monomer solution or suspension, drying the polymeric foam and grinding the dried foam.
摘要:
A process for producing water-absorbing polymer particles with improved free swell rate by polymerizing a monomer solution or suspension comprising an ethylenically unsaturated monomer bearing acid groups, an ethylenically unsaturated monomer, a crosslinker and an initiator.
摘要:
The use of water-absorbing polymer particles for dewatering feces, the water-absorbing polymer particles being obtainable by polymerizing a foamed monomer solution or suspension, drying the polymeric foam and grinding the dried foam.
摘要:
Spherical particles having a mean diameter in the range from 1 to 20 μm, comprising (a) from 85 to 99% by weight of a crosslinked random copolymer having a glass transition temperature Tg in the range from −75 to −40° C. (b) and from 1 to 15% by weight of at least one organic substance selected from waxes, protective colloids and plasticizers.
摘要:
Spherical particles having a mean diameter in the range from 1 to 20 μm, comprising (a) from 85 to 99% by weight of a crosslinked random copolymer having a glass transition temperature Tg in the range from −75 to −40° C. (b) and from 1 to 15% by weight of at least one organic substance selected from waxes, protective colloids and plasticizers.