Abstract:
Wässrige Klebstoffdispersion enthaltend 25 bis 70 Gew- % Acrylatblockcopolymere und/oder Styrolblockcopolymere, die ein Molekulargewicht von über 15000 g/mol und mindestens zwei unterschiedlichen Glasübergangstemperaturen aufweisen, wobei eine Glasübergangstemperatur (Tg) oberhalb von 50 °C beträgt, die andere Glasübergangstemperatur unterhalb von +10°C, sowie zusätzlich weitere Additive, wobei die Dispersion weniger als 0,5 Gew-% organische Lösemittel enthält.
Abstract:
The invention relates to a metal surface, which is coated with a polymer layer containing at least one polymer that is not soluble in water and at least one water-soluble polymer, whereby the layer thickness of the polymer layer is equal to 2 mu m or less. The invention also relates to a method for reducing the susceptibility of a metal surface to fingerprints, according to which a metal surface is coated with a less than 2 mu m thick layer of a polymer mixture containing at least one water-soluble polymer and at least one polymer that is not soluble in water or is coated with a compound of general formula (I) Y-R -X comprising at least two acid groups.
Abstract:
The invention provides adhesives comprising at least one polymer component which contains at least 65 weight percent propylene, at least one nucleator and at least one functionalized wax. The inventive adhesives have increased heat resistance and decreased set- time, making them particularly well suited for assembly and packaging applications.
Abstract:
Die Erfindung betrifft die Verwendung eines Schmelzklebstoffs mit hoher Härte zur Verklebung von Metall-, Papier- und/oder Kunststofffolien. Die Erfindung betrifft weiterhin ein Verfahren zum Verkleben einer Metall-, Papier- und/oder Kunststofffolie auf einem Substrat.
Abstract:
The present invention relates to a process for manufacturing an adhesive by extrusion, wherein the adhesive comprises at least one degraded polypropylene (co)polymer and at least one additional additive.
Abstract:
Verfahren zum Durchführen einer Phasenumwandlung, insbesondere eines Schmelzprozesses, durch Erwärmen eines Trägermediums, das einen phasenveränderlichen Stoff enthält oder darstellt, in einem Reaktor, wobei man das Trägermedium in Kontakt mit einem durch elektromagnetische Induktion erwärmbaren festen Heizmedium bringt, das sich innerhalb des Reaktors befindet und das von dem Trägermedium umgeben ist, und das Heizmedium durch elektromagnetische Induktion mit Hilfe eines Induktors erwärmt, wobei der phasenveränderliche Stoff eine Phasenumwandlung eingeht und wobei man das Trägermedium nach der Phasenumwandlung von dem Heizmedium abtrennt. Vorzugsweise erfolgt dies in einem Durchflussreaktor. Der Induktor erzeugt vorzugsweise ein Wechselfeld mit einer Frequenz im Bereich von 1 bis 100 kHz.
Abstract:
The invention provides adhesives comprising at least one polymer component which contains at least 65 weight percent propylene, at least one nucleator and at least one functionalized wax. The inventive adhesives have increased heat resistance and decreased set- time, making them particularly well suited for assembly and packaging applications.
Abstract:
The invention relates to a method for performing a phase conversion, in particular a melting process, by means of heating a carrier medium that comprises or constitutes a phase-variable material, in a reactor, wherein the carrier medium is brought into contact with a solid heating medium, which can be heated by means of electromagnetic induction and which is located within the reactor and surrounded by the carrier medium, and the heating medium is heated by means of electromagnetic induction using an inductor, wherein the phase-variable material enters a phase conversion and wherein the carrier medium is separated from the heating medium after the phase conversion. Said method preferably takes place in a flow reactor. The inductor preferably generates an alternating field having a frequency in the range of 1 to 100 kHz.
Abstract:
Schmelzklebstoff enthaltend 5 bis 40 Gew.-% mindestens eines Copolymeren auf Basis von Ethylen und mindestens einem C 3 bis C 20 -α-Olefinen, das durch Metallocene-katalysierte Polymerisation erhältlich ist, 10 bis 65 Gew.-% mindestens eines klebrigmachenden Harzes, 0 bis 35 Gew.-% eines Weichmachers, 0,01 bis 30 Gew.-% Additive und Zusatzstoffe ausgewählt aus Stabilisatoren, Haftvermittler, Füllstoffe oder Pigmente, Wachsen und/oder anderen Polymeren, wobei die Summe 100 % betragen soll, dadurch gekennzeichnet, dass das Copolymer A ein Blockcopolymer ist, das im Bereich von 0°C bis 25°C eine weitgehend gleichbleibendes elastisches Verhalten zeigt gemessen als Verhältnis des Speichermoduls E' gemäß (E' 0C - E' 25C ) / E' 25C
Abstract:
Die Erfindung betrifft einen Schmelzklebstoff auf der Basis mindestens eines Ethylen und/oder Propylen/C 4 bis C 20 α--Olefin Copolymeren, das durch Metallocenekatalysierte Polymerisation erhältlich ist, mindestens eines klebrig machenden Harzes, sowie mindestens 0,1 bis 15 Gew.-% eines Co- oder Terpolymeren auf Basis von von C 2 bis C 5 -Olefinen mit (Meth)acrylsäureestern von niedermolekularen Alkanolen, wobei das Copolymer COOH-Gruppen oder Anhydridgruppen enthält sowie ggf. Wachs und Additive und seine Verwendung zur Verklebung von veredelten Substratoberflächen.