EROSION-STABILIZED BIOADHESIVE POLYMERS FUNCTIONALIZED OR BLENDED WITH CATECHOL AND DERIVATIVES THEREOF
    2.
    发明申请
    EROSION-STABILIZED BIOADHESIVE POLYMERS FUNCTIONALIZED OR BLENDED WITH CATECHOL AND DERIVATIVES THEREOF 审中-公开
    功能化或与儿茶酚及其衍生物共混的抗蚀剂稳定的含水聚合物

    公开(公告)号:WO2008002471A3

    公开(公告)日:2008-02-21

    申请号:PCT/US2007014551

    申请日:2007-06-22

    IPC分类号: A61K31/74

    摘要: Polymers with improved bioadhesive properties and methods for improving bioadhesion of polymers have been developed. Such bioadhesive polymers can be stabilized against erosion, particularly in the gastrointestinal tract, by incorporating one or more additives selected from (1) polyanhydrides, such as those having a molecular weight average in excess of 20,000, (2) acidic components, (3) metal compounds, (4) stabilizing polymers, and (5) hydrophobic components. By stabilizing bioadhesive polymers against erosion, residence time at tissue surfaces can be further increased. The stabilized polymers are also useful to maintain the drug release rate-controlling properties for a prolonged period of time.

    摘要翻译: 已经开发出具有改善的生物粘附性质的聚合物和用于改善聚合物的生物粘附性的方法。 通过引入一种或多种选自如下的添加剂来稳定这种生物粘附聚合物以防止侵蚀,特别是在胃肠道中:(1)聚酐,如分子量平均超过20,000的聚酐,(2)酸性组分,(3) 金属化合物,(4)稳定聚合物,和(5)疏水组分。 通过稳定生物粘附聚合物抵抗侵蚀,组织表面处的停留时间可以进一步增加。 稳定化的聚合物也可用于长时间维持药物释放速度控制性能。

    プリント基板用材料、金属積層板、それらの製造方法およびプリント基板の製造方法
    4.
    发明申请
    プリント基板用材料、金属積層板、それらの製造方法およびプリント基板の製造方法 审中-公开
    印刷电路板材料,金属层压板,其制造方法以及制造印刷电路板的方法

    公开(公告)号:WO2016181936A1

    公开(公告)日:2016-11-17

    申请号:PCT/JP2016/063760

    申请日:2016-05-09

    摘要: 電気特性を維持しつつ、高温領域(150~200℃)における反りを改善したプリント基板用材料、金属積層板、それらの製造方法およびプリント基板の製造方法を提供する。 含フッ素樹脂層を有する材料について熱処理する。含フッ素樹脂層は、カルボニル基含有基、ヒドロキシ基、エポキシ基、およびイソシアネート基からなる群から選択される少なくとも1種の官能基を有し、融点が280~320℃で、372℃、49Nの荷重下で測定された溶融流れ速度が2g/10分以上である含フッ素共重合体(a)を含有する組成物からなる。熱処理は、250℃以上、かつ、含フッ素共重合体(a)の融点よりも5℃以上低い温度で、熱処理前後の含フッ素樹脂層の溶融流れ速度の比と、熱処理後の含フッ素樹脂層の溶融流れ速度の値が、それぞれ特定の範囲内となるように行う。

    摘要翻译: 提供:用于印刷电路板的材料,其在保持电性能的同时耐高温翘曲(150-200℃); 金属层压板 其制造方法; 以及印刷电路板的制造方法。 将具有含氟树脂层的材料进行热处理。 含氟树脂层包含含有含有共聚物(a)的组合物,该组合物具有选自含有羰基的基团,羟基,环氧基和异氰酸酯基中的至少一种官能团 的熔点为280-320℃,并且在372℃的负载49N下测量的熔体流动速率为至少2g / 10分钟。 热处理在等于或高于250℃但低于含氟共聚物(a)的熔点至少5℃的温度下进行,使得熔体流动速率 热处理前后的含氟树脂层和热处理后的含氟树脂层的熔体流动速率的值分别落在特定范围内。

    EROSION-STABILIZED BIOADHESIVE POLYMERS FUNCTIONALIZED OR BLENDED WITH CATECHOL AND DERIVATIVES THEREOF
    5.
    发明申请
    EROSION-STABILIZED BIOADHESIVE POLYMERS FUNCTIONALIZED OR BLENDED WITH CATECHOL AND DERIVATIVES THEREOF 审中-公开
    功能化或混合了CATECHOL及其衍生物的抗腐蚀稳定的生物聚合物

    公开(公告)号:WO2008002471A2

    公开(公告)日:2008-01-03

    申请号:PCT/US2007/014551

    申请日:2007-06-22

    IPC分类号: A61F2/02

    摘要: Polymers with improved bioadhesive properties and methods for improving bioadhesion of polymers have been developed. Such bioadhesive polymers can be stabilized against erosion, particularly in the gastrointestinal tract, by incorporating one or more additives selected from (1) polyanhydrides, such as those having a molecular weight average in excess of 20,000, (2) acidic components, (3) metal compounds, (4) stabilizing polymers, and (5) hydrophobic components. By stabilizing bioadhesive polymers against erosion, residence time at tissue surfaces can be further increased. The stabilized polymers are also useful to maintain the drug release rate-controlling properties for a prolonged period of time.

    摘要翻译: 已经开发了具有改进的生物粘附性质的聚合物和改善聚合物生物粘附的方法。 通过掺入一种或多种选自(1)聚酐,例如分子量平均超过20,000的那些,(2)酸性组分,(3)和(3)的组分,可以稳定这种生物粘合聚合物,特别是在胃肠道中, 金属化合物,(4)稳定聚合物,和(5)疏水组分。 通过稳定生物粘附聚合物以抵抗侵蚀,组织表面的停留时间可以进一步提高。 稳定的聚合物也可用于在长时间内维持药物释放速率控制性质。

    A LIGHT-CURABLE RESIN COMPOSITION
    8.
    发明申请
    A LIGHT-CURABLE RESIN COMPOSITION 审中-公开
    光固化树脂组合物

    公开(公告)号:WO2015159442A1

    公开(公告)日:2015-10-22

    申请号:PCT/JP2014/061501

    申请日:2014-04-17

    摘要: The present application relates to a resin composition and in particular to a light-curable resin composition. It is known to achieve a thixotropic behavior of an adhesive composition by adding an inorganic additive like fumed silica. Adding inorganic additives results in significant particle problems as fumed silica is a solid particle and affects the optical performance of the adhesive composition. In accordance with the invention a particle free resin composition with a thixotropic behavior is provided. The inventive composition comprises a) 30 to 90 wt% of a urethane acrylate oligomer with a molecular weight greater than 15000, b) 2 to 40 wt% of a (meth)acrylate monomer having a benzene ring, and c) 0,2 to 10 wt% of a photo initiator.

    摘要翻译: 本申请涉及树脂组合物,特别涉及光固化树脂组合物。 已知通过加入无机添加剂如热解法二氧化硅来实现粘合剂组合物的触变性能。 添加无机添加剂导致显着的颗粒问题,因为气相二氧化硅是固体颗粒并影响粘合剂组合物的光学性能。 根据本发明,提供了具有触变性能的无颗粒树脂组合物。 本发明的组合物包含a)30-90重量%的分子量大于15000的氨基甲酸酯丙烯酸酯低聚物,b)2-40重量%的具有苯环的(甲基)丙烯酸酯单体,和c)0.2至 10重量%的光引发剂。

    加飾物品および加飾用積層体
    10.
    发明申请
    加飾物品および加飾用積層体 审中-公开
    装饰品和装饰层压板

    公开(公告)号:WO2016111286A1

    公开(公告)日:2016-07-14

    申请号:PCT/JP2016/050110

    申请日:2016-01-05

    摘要:  本発明の実施形態の一つは、高温環境下における経時的な意匠性の低下を抑制可能な加飾物品およびこれに用いられる加飾用積層体を提供することを主目的とする。 本発明の実施形態の一つは、樹脂を含有する被着体と、上記被着体上に配置された接着層と、上記接着層上に配置された加飾層とを有する加飾物品であって、上記接着層が、カルボキシル基を有するアクリル樹脂と、エポキシ基を有する架橋剤とを混合して得られ、上記カルボキシル基および上記エポキシ基が反応したエステル基を有するものを含むことにより、上記課題を解決する。

    摘要翻译: 本发明的其中一个实施例的主要目的是提供一种可以在高温环境中随时间抑制设计特性的降低的装饰品,并提供一种用于装饰的装饰层压板 装饰品。 本发明的一个实施方案是具有包含树脂的被粘物,设置在被粘物上的粘合剂层和设置在粘合剂层上的装饰层的装饰品,其中粘合剂层通过将具有 羧基和具有环氧基的交联剂,并且包括具有由羧基和环氧基之间的反应获得的酯基的部分,从而达到上述目的。