Abstract:
Thermoplastic moulding materials comprising A) from 19.9 to 59.9% by weight of a thermoplastic polyamide, B) from 40 to 80% by weight of an aluminium oxide or magnesium oxide or mixtures thereof, C) from 0.1 to 2% by weight of nigrosine, D) from 0 to 20% by weight of further additives, where the sum of percentages by weight of A) to D) adds up to 100%.
Abstract:
The invention relates to thermoplastic moulding compounds which contain A) 10 to 98 wt.% of a thermoplastic polyamide, B) 0.1 to 60 wt.% of red phosphorus, C) 0.5 to 20 wt.% of a melamine compound, D) 1 to 30 wt.% of rutile-type titanium dioxide, E) 0 to 40 wt.% of an impact modifier, and F) 0 to 60 wt.% of further additives, the sum of the weight percentages of components A) to F) totalling 100%.
Abstract:
Thermoplastic moulding materials comprising A) from 19.9 to 59.9% by weight of a thermoplastic polyamide, B) from 40 to 80% by weight of an aluminium oxide or magnesium oxide or mixtures thereof, C) from 0.1 to 2% by weight of nigrosine, D) from 0 to 20% by weight of further additives, where the sum of percentages by weight of A) to D) adds up to 100%.
Abstract:
Disclosed are thermoplastic molding materials containing A) 10 to 99 percent by weight of at least one thermoplastic polyamide, B) 0.01 to 50 percent by weight of B1) at least one highly branched or hyperbranched polycarbonate having a hydroxyl number ranging between 1 and 600 mg KOH/g of polycarbonate (according to DIN 53240, part 2), or B2) at least one highly branched or hyperbranched polyester of type AxBy, wherein x is at least 1.1 and y is at least 2.1, or the mixtures thereof, C) 0 to 60 percent by weight of other additives, the total percentage by weight of components A) to C) amounting to 100 percent.
Abstract:
The use of thermoplastic molding materials comprising A) 10 to 98.8% by weight of a mixture formed from a1) 40 to 70% by weight of nylon-6,6 or nylon-4,6 or nylon-6 or mixtures thereof, a2) 30 to 60% by weight of a polyamide having a ratio of methylene to amide groups of 7 to 12, B) 1 to 50% by weight of a fibrous or particulate filler, C) 0.1 to 3% by weight of a lubricant, D) 0.05 to 3% by weight of a heat stabilizer, E) 0 to 40% by weight of further additives, where the sum of the percentages by weight A) to E) and a1) and a2) adds to 100%, for production of stress cracking- and corrosion-resistant moldings.
Abstract:
Thermoplastic molding materials comprising: (A) 20 - 85% by weight of at least one polyamide having a number of amino end groups of 50 mmol/kg, (B) 14.9 - 60% by weight of glass fibers, (C) 0.01 - 2% by weight of at least one heat stabilizer, (D) 0 - 1.5% by weight of at least one demolding assistant and (D) 0 - 30% by weight of further additives, where the sum of the percentages by weight of (A) - (E) is 100.
Abstract:
The invention relates to thermoplastic molding materials containing: A) 10 to 98 % by weight of at least one thermoplastic polymer; B) 0.01 to 50 % by weight of; B1) at least one highly branched or hyperbranched polycarbonate with an OH number ranging from 1 to 600 mg KOH/g of polycarbonate (in accordance with DIN 53240, part 2) or; B2) at least one highly branched or hyperbranched polyester of type AxBy with x being at least 1.1 and y being at least 2.1 or mixtures consisting of B1) and B2); C) 1 to 30 % by weight of a flameproofing agent combination consisting, with regard to 100 % by weight of C), of; C1) 20 to 99 % by weight of a halogen-containing flameproofing agent; C2) 1 to 80 % by weight of an antimony oxide, and; D) 0 to 60 % by weight of additional additives, the sum of the weight percentages of constituents A) to D) totaling 100 %.