Process for making thermoset polyphenylene oxide/epoxy laminates
    2.
    发明公开
    Process for making thermoset polyphenylene oxide/epoxy laminates 失效
    维他命Zur Herstellung von Laminaten aushitzehärtbaremPolyphenyloxid / -epoxid。

    公开(公告)号:EP0537005A1

    公开(公告)日:1993-04-14

    申请号:EP92309181.3

    申请日:1992-10-08

    IPC分类号: C08J5/24

    摘要: Broadly, the present invention comprises a solventless process wherein blends of thermoset polyphenylene oxide and epoxy can be processed into fiber reinforced laminates, and especially laminates prepared by the Wiggins Teape process. One aspect of the present inventive process comprises blending the polyphenylene powder with a liquid epoxy material, optionally with flame retardants and catalysts, preferably in a high shear mixer at elevated temperature, e.g. in the range of about 100°-130°C. The resultant up-staged or partially-cured blend is sufficiently solidified to be granulated into a powder for Wiggins Teape processing or, optionally, conventional press processing into a fiber reinforced laminates. Resin systems thus-prepared exhibit both improved solderability resistance and improved resistance to organic solvents when compared to thermoplastic systems.

    摘要翻译: 广泛地说,本发明包括无溶剂方法,其中热固性聚苯醚和环氧树脂的共混物可以加工成纤维增强层压材料,特别是通过Wiggins Teape方法制备的层压材料。 本发明方法的一个方面包括将聚苯醚粉末与液体环氧材料混合,任选地含有阻燃剂和催化剂,优选在高剪切混合器中,例如高温下。 在约100-130℃的范围内。所得到的上级或部分固化的共混物充分固化,以造粒成用于Wiggins Teape加工的粉末,或任选地,常规的冲压加工成纤维增强层压材料。 如此制备的树脂体系与热塑性体系相比表现出改进的耐焊接性和改善的耐有机溶剂性。

    Polyetherimide/epoxy chopped fiber reinforced laminates and the preparation thereof
    3.
    发明公开
    Polyetherimide/epoxy chopped fiber reinforced laminates and the preparation thereof 失效
    聚醚醚酮/环氧树脂和Verfahren zu ihrer Herstellung。

    公开(公告)号:EP0499697A2

    公开(公告)日:1992-08-26

    申请号:EP91120127.5

    申请日:1991-11-26

    IPC分类号: C08J5/24 C08J9/30

    摘要: The present invention is directed to a method for making a chopped fiber-reinforced composite. The method comprises dispersing a polyamide acid/epoxy blend and greater than 50 wt-% chopped fiber in an aerated surfactant foam. The foam is deposited on a foraminous layer and collapsed to form a web. The web is consolidated at a temperature of greater than about 280°C and a pressure of greater than about 500 psi. The resulting composite typically has a flexural modulus of greater than 2,000 ksi and flexural strength values of greater than about 30,000 psi and typically between about 30,000 and 50,000 psi. The composite should find use in applications requiring effective high mechanical stiffness and strength, and flame resistance.

    摘要翻译: 本发明涉及一种短切纤维增强复合材料的制造方法。 该方法包括将聚酰胺酸/环氧共混物和大于50重量%的短切纤维分散在充气表面活性剂泡沫中。 将泡沫沉积在多孔层上并折叠以形成网。 纤维网在大于约280℃的温度和大于约500psi的压力下固结。 所得到的复合材料通常具有大于2,000ksi的弯曲模量和大于约30,000psi,典型地在约30,000和50,000psi之间的弯曲强度值。 该复合材料应用于需要有效的高机械刚度和强度以及阻燃性的应用中。

    Poly (cyclohexanedimethanol terephthalate) molding compositions
    8.
    发明公开
    Poly (cyclohexanedimethanol terephthalate) molding compositions 失效
    Formmassen aus聚环己烷二甲醇对苯二甲酸酯。

    公开(公告)号:EP0273149A2

    公开(公告)日:1988-07-06

    申请号:EP87116435.6

    申请日:1987-11-06

    摘要: Molding compositions comprising poly(cyclohexane­dimethanol terephthalate), a reinforcing agent, optionally, a crystallization promoting agent, optionally a flame retardant agent and tribranched epoxy and/or triallyl isocyanurates as melt stabilizers, are disclosed. These compositions are characterized by substantially higher melt stability and improved thermal aging properties.

    摘要翻译: 公开了包含聚(环己烷二甲醇对苯二甲酸酯),增强剂,任选的结晶促进剂,任选的阻燃剂和三角环氧树脂和/或三烯丙基异氰脲酸酯作为熔体稳定剂的成型组合物。 这些组合物的特征在于具有显着更高的熔体稳定性和改善的热老化性能。