    摘要: The present invention relates generally to nutritive (e.g., cell culture) medium, medium supplement, media subgroup and buffer formulations. Specifically, the present invention provides powdered nutritive medium, medium supplement and medium subgroup formulations, particularly cell culture medium supplements (including powdered sera such as powdered fetal bovine seum (FBS)), medium subgroup formulations and cell culture media comprising necessary nutritive factors that facilitate the in vitro cultivation of cells. The invention further provides such powdered formulations that produce particular or desired final ionic and/or pH conditions upon reconstitution with a solvent. The invention is also directed to methods of production of these formulations, and also provides kits and methods for cultivation of prokaryotic and eukaryotic cells using these formulations.; The invention also relates to methods of producing sterile formulations, and to methods for producing dry cell powders. The invention also provides cell, media, media supplement, media subgroup and buffer powders produced by the methods of the invention.

    COPPER SULPHIDE LEACHING INFERROUS CHLORIDE MEDIUM WITH BACTERIA

    公开(公告)号:EP3184657A4

    公开(公告)日:2018-03-14

    申请号:EP15833027

    申请日:2015-08-24

    IPC分类号: C22B15/00 C12N1/20 C22B3/18

    摘要: The present invention relates to a method for leaching secondary and primary sulphides of copper in a ferrous chloride medium with iron-oxidising bacteria adapted from the crushing of the mineral from the mine, comprising the steps of: mixing the mineral from the crushing with concentrated sulphuric acid; transporting the material mixed with sulphuric acid by means of a belt; adding a liquid leaching solution at an intermediate point during transport on the belt, said solution consisting of: iron (II) sulphate to reduce the redox potential of the solution-mineral mixture to values less than 550 mV Ag/AgCl; iron (III) sulphate; bacteria and archaea of the mesophile- and thermophile-type belonging to the genera Acidithiobacillus, Leptospirillum and Sulfulobos, previously adapted in an annexed bioreactor plant; and sodium chloride to produce a chlorinated environment in solutions. The method also comprises the subsequent steps of; heaping the material on head pads to rest for a specific amount of time depending on the mineralogical composition of the material or the operating conditions of the plant; during the resting step, injecting air warmed by a liquid/air exchange system, said air being injected through the lower part of the heap by means of fans; and leaching the heaped material by means of a flow of solutions having a low sulphuric acid content, with ferric ion, which contribute to performing the second step of solubilising the copper sulphides.