公开(公告)号:KR101855050B1
公开(公告)日:2018-05-08
申请号:KR1020170169052
申请日:2017-12-11
申请人: 조병학
发明人: 조병학
CPC分类号: Y02W30/92 , C04B18/101 , C04B14/08 , C04B22/12 , C04B22/149 , C04B24/04 , C04B28/02 , C04B2111/00025 , C04B2201/50
摘要: 본발명은시멘트에서생성되는 6가크롬을비롯한중금속등의발암유발물질을제거함과동시에시멘트의강도및 고유물성이유지되는시멘트첨가물및 그제조방법에관한발명이다. 또한, 본발명의시멘트첨가물은열에의해 6가크롬으로산화되지않는시멘트를제공할수 있다.
-
公开(公告)号:KR1020150059658A
公开(公告)日:2015-06-02
申请号:KR1020130142568
申请日:2013-11-22
申请人: (주)에스겔
发明人: 이재준
CPC分类号: C04B14/10 , C04B14/047 , C04B14/18 , C04B16/08 , C04B18/248 , C04B20/026 , C04B22/143 , C04B28/08 , C04B40/0032 , C04B2111/00025
摘要: 본발명은황토분말 40~50중량%, 퍼라이트분말 15~20중량%, 석고플라스터10중량%,고로시멘트5~10중량%, EPS5~10중량%, 제올라이트 5중량%, 및마닐라펄프 5중량%로이루어진황토몰탈조성물및 이의제조방법에관한것이다.
摘要翻译: 本发明涉及一种用于黄土砂浆的组合物,其由40-50重量%的黄土粉末,15-20重量%的珍珠岩粉末,10重量%的石灰膏,5-10重量%的波特兰高炉水泥, EPS的5-10重量%,5重量%的沸石和5重量%的马尼拉纸浆及其制造方法。
-
3.
公开(公告)号:KR101443672B1
公开(公告)日:2014-09-26
申请号:KR1020130101484
申请日:2013-08-27
申请人: (주)대한하이텍건설 , 강창구
CPC分类号: C04B16/02 , B28B1/14 , C04B14/042 , C04B28/04 , C04B2103/0097 , C04B2103/302 , C04B2103/63 , C04B2103/65 , C04B2111/00025 , E04C2/26
摘要: The present invention relates to a building finishing composition which comprises, with respect to 100 parts by weight of cement in which fineness is 3,200-6,500 cm2/g, 10-40 parts by weight of cannabis liquid and cannabis stem mixture; 5-100 parts by weight of stone dust; 5-15 parts by weight of a flame retardant; 0.01-10 parts by weight of a high performance water reducing agent; 0.1-1 parts by weight of one or more condition promoters; and 1-15 parts by weight of one filler. The composition, according to the present invention, improves durability, adds sound absorption, antibacterial, deodorization, insulation, and UV blocking functions, emits far-infrared rays, removes harmful wavelengths, and facilitates the moisture control.
摘要翻译: 本发明涉及一种建筑整理组合物,其包含相对于100重量份细度为3200-6,500cm2 / g的水泥,10-40重量份的大麻液和大麻茎混合物; 石灰粉5-100重量份; 5-15重量份阻燃剂; 0.01-10重量份的高性能减水剂; 0.1-1重量份的一种或多种条件促进剂; 和1-15重量份的一种填料。 根据本发明的组合物提高耐久性,增加吸声,抗菌,除臭,绝缘和UV阻隔功能,发射远红外线,去除有害波长,并且有助于水分控制。
-
公开(公告)号:KR101169941B1
公开(公告)日:2012-08-06
申请号:KR1020090035481
申请日:2009-04-23
申请人: 지만희
IPC分类号: C04B26/02 , C04B14/10 , C04B111/54
CPC分类号: C04B41/009 , C04B28/06 , C04B41/483 , C04B2103/0097 , C04B2103/605 , C04B2111/00025 , C04B2111/00508 , C04B2111/2038 , C04B2111/2076 , C04B2111/27 , C04B2111/545 , C04B14/04 , C04B14/10 , C04B14/305 , C04B14/366 , C04B40/0028 , C04B2103/0093 , C04B2103/14 , C04B41/0045 , C04B41/0072 , C04B2111/805
摘要: 본 발명은 인조 대리석의 제조방법 및 이로부터 제조된 인조 대리석에 관한 것으로, 무늬가 코팅된 투명판에 점토광물 및 폴리아크릴레이트 등을 혼합한 도료를 코팅하여 인조 대리석을 제조하는 방법에 관한 것이다. 본 발명의 제조방법에 의해 제조된 인조 대리석은 습기 및 자외선에 대한 내구성이 강하여 박리현상 및 변색이 일어나지 않고, 원적외선 및 음이온을 방출하여 인체에 유익한 기능성을 보유하는 장점이 있다.
토르말린, 점토광물, 모나자이트, 음이온, 원적외선, 인조 대리석-
公开(公告)号:KR100987117B1
公开(公告)日:2010-10-11
申请号:KR1020100058065
申请日:2010-06-18
申请人: 주식회사 서영엔지니어링 , 에스피시멘트 주식회사
CPC分类号: C04B28/04 , C04B2103/0025 , C04B2103/0076 , C04B2103/0097 , C04B2111/00017 , C04B2111/00025 , C04B2111/00086 , C04B2111/00241 , C04B2111/0075 , C04B2111/2069 , C04B2111/28 , C04B2111/343 , C04B2111/802 , Y02W30/97 , C04B14/04 , C04B14/06 , C04B18/241 , C04B22/143 , C04B24/06 , C04B24/085 , C04B24/2623 , C04B2103/0088 , C04B2103/58 , C04B22/008
摘要: PURPOSE: An environment-friendly yellow soil mortar composition, and a construction method of a pavement material using thereof are provided to secure the harmlessness to a human body by using yellow soil, sand, and pozzolan. CONSTITUTION: An environment-friendly yellow soil mortar composition contains 35~50 parts of yellow soil powder by weight, 40~50 parts of sand by weight, 10~20 parts of pozzolan powder by weight, 20~35 parts of expansion admixture by weight for preventing the cracking, 10~20 parts of solidifying agent by weight formed with white Portland, 5~10 parts of anhydrous gypsum powder by weight, 1~5 parts of citric acid powder by weight, 1~2 parts of vinyl acetate copolymeric resin by weight, 2~5 parts of nature cellulose fiber by weight, and 1~2 parts of zinc stearate by weight.
摘要翻译: 目的:提供一种环保黄土砂浆组合物,以及使用其的路面材料的施工方法,以通过使用黄土,沙粒和火山灰来确保对人体的无害性。 构成:环保黄土砂浆组合物含有35〜50份重量的黄土粉,重量40〜50份,火山灰粉10〜20份,重量20〜35份膨胀剂 为防止裂纹,10〜20份固化剂用白色波特兰重量形成,重量为5〜10份无水石膏粉,1〜5份柠檬酸粉,1〜2份醋酸乙烯酯共聚树脂 的重量,2〜5份重量的天然纤维素纤维,和1〜2份重量的硬脂酸锌。
-
公开(公告)号:KR100917739B1
公开(公告)日:2009-09-15
申请号:KR1020080056616
申请日:2008-06-17
申请人: 박술목
发明人: 박술목
CPC分类号: C04B41/4584 , C04B41/4803 , C04B41/5001 , C04B41/5024 , C04B2111/00025
摘要: A method for manufacturing a toxic material blocker to be coated on an interior material is provided to remove harmful materials from the air and to show a mosquito control effect. A method for manufacturing a toxic material blocker to be coated on an interior material comprises the following steps of: crushing silicate to a size of Phi10-20mm, dipping the crushed silicate in water, taking it out and heating it to prepare silicate mineral(S1); making charcoal with one or more ingredients selected from the group consisting of coconut trees, bamboo, oak and pine trees using an out-oven baking method(S2); drying fruits of Zanthoxylum piperitum or Zanthoxylum schinifolium and crushing its hulls to prepare a mosquito controller(S3); and agitating the silicate minerals, charcoal and the mosquito controller in water, adding a powdery foaming agent and a viscosity controller, agitating them well and adding an aqueous binder and an inorganic binder(S4).
摘要翻译: 提供一种用于制造要涂覆在内部材料上的有毒材料阻挡剂的方法,以从空气中除去有害物质并显示出蚊子控制效果。 一种用于制造要涂覆在内部材料上的有毒物质阻挡剂的方法包括以下步骤:将硅酸盐破碎至Φ10-20mm的尺寸,将粉碎的硅酸盐浸入水中,取出并加热以制备硅酸盐矿物(S1 ); 使用炉外焙烧方法(S2),使用选自椰子树,竹子,橡木和松树的一种或多种成分制造木炭; 烘干花椒椒(Zanthoxylum piperitum)或花椒(Zanthoxylum schinifolium),粉碎其外壳以制备蚊子控制器(S3); 并搅拌水中的硅酸盐矿物,木炭和蚊子控制剂,加入粉状发泡剂和粘度控制剂,充分搅拌,加入水性粘合剂和无机粘合剂(S4)。
-
7.
公开(公告)号:KR100886786B1
公开(公告)日:2009-03-04
申请号:KR1020080118375
申请日:2008-11-26
CPC分类号: C04B26/06 , C04B2103/0097 , C04B2103/67 , C04B2111/00025 , C04B2111/00482 , C04B14/04 , C04B14/08 , C04B14/10 , C04B14/366
摘要: A method of manufacturing finishing material for construction for functionality bioceramics liquid is provided to emit far infrared rays and negative ion and to form agreeable residence and living environment according to holding growth of mold or noxious bacteria. A method of manufacturing finishing material for construction for functionality bioceramics liquid comprises steps of: agitating Hydroxy-Apatite, elvan, talc, diatomite and water in a stirred tank; injecting liquid binder 20 ~ 25 weight% including aqueous emulsion in the mixed mixture, agitating it for 20 ~ for 30 minutes at 600 ~ 800rpm and forming the mixture of the liquid; injecting admixture in the mixture of the liquid in which the liquid binder is mixed, agitating it for 20 ~ 30 minutes at 600 ~ 800rpm and forming the finishing material for construction of liquid; removing foreign material and thick particle more than 300 ~ 400 mesh; and wrapping the finishing material for construction of the liquid from which the foreign material is removed up in a container.
摘要翻译: 提供一种制造用于功能性生物陶瓷液体的整理材料的方法,以发射远红外线和负离子,并且根据保持霉菌或有害细菌的生长形成合适的居住和生活环境。 制造功能性生物陶瓷液体结构用整理材料的方法包括以下步骤:在搅拌釜中搅拌羟基磷灰石,埃尔文,滑石,硅藻土和水; 将20〜25重量%的液体粘合剂包含水性乳液混合,在600〜800rpm下搅拌20〜30分钟,形成液体混合物; 在其中混合有液体粘合剂的液体混合物中注入混合物,以600〜800rpm搅拌20〜30分钟,形成用于构造液体的整理材料; 去除异物和厚度超过300〜400目的颗粒; 并且将用于构造除去异物的液体的整理材料包裹在容器中。
-
公开(公告)号:KR100883583B1
公开(公告)日:2009-02-18
申请号:KR1020070111104
申请日:2007-11-01
CPC分类号: C04B28/06 , C04B28/08 , C04B2111/00025 , Y02W30/92 , Y02W30/94 , C04B14/02 , C04B14/06 , C04B14/202 , C04B18/08 , C04B18/141 , C04B18/146 , C04B20/0048 , C04B22/008 , C04B24/08 , C04B2103/0057 , C04B2103/32 , C04B2103/44 , C04B2103/67 , C04B7/32
摘要: An antibiotic mortar using natural ceramic mineral is provided to have excellent durability, antibiotic and deodorization, to increase adhesive force by penetrating into concrete structure and to perform conveniently coating operation. An antibiotic mortar using natural ceramic mineral comprises special cement 30 parts by weight, silica fume 2 parts by weight, fly ash 2.1 parts by weight, blast furnace slag powder 5 parts by weight, natural ceramic system expander 3 parts by weight, vermiculite powder 5 parts by weight, thickening agent 0.1 parts by weight, superplasticizer 0.06 parts by weight, redispersible powder polymer 5 parts by weight, fibrous reinforcement 0.2 parts by weight, silica 27 parts by weight, natural drying aggregate 20 parts by weight, calcium stearate 0.2 parts by weight and antimicrobial agent 0.4 parts by weight.
摘要翻译: 提供使用天然陶瓷矿物的抗生素砂浆具有优异的耐久性,抗生素和除臭性,通过渗透到混凝土结构中并且执行方便的涂布操作来增加粘合力。 使用天然陶瓷矿物的抗生素砂浆包括30重量份特种水泥,硅粉2重量份,粉煤灰2.1重量份,高炉渣粉5重量份,天然陶瓷体系膨胀机3重量份,蛭石粉5 重量份,增稠剂0.1重量份,超增塑剂0.06重量份,可再分散粉末聚合物5重量份,纤维增强剂0.2重量份,二氧化硅27重量份,天然干燥骨料20重量份,硬脂酸钙0.2份 和抗菌剂0.4重量份。
-
公开(公告)号:KR100873051B1
公开(公告)日:2008-12-09
申请号:KR1020080041838
申请日:2008-05-06
申请人: 주식회사 삼우씨엠건축사사무소
发明人: 손명기
CPC分类号: C04B28/02 , C04B2111/00017 , C04B2111/00025 , C04B2111/00267 , C04B2111/00482 , C04B2111/27 , C04B2111/28 , C04B2111/80 , Y02W30/94 , C04B7/32 , C04B14/06 , C04B14/10 , C04B14/106 , C04B14/28 , C04B14/322 , C04B18/146 , C04B20/0008 , C04B20/0048 , C04B20/008 , C04B22/00 , C04B22/064 , C04B22/143 , C04B24/26 , C04B2103/10 , C04B2103/20 , C04B2103/408 , C04B2103/50 , C04B2103/54
摘要: An inorganic polymer resin mortar finishing material composition is provided to be environment-friendly, to have a high function and to show an excellent tensile strength, compressive strength, expansion and contraction intensity and abrasion resistance. An inorganic polymer resin mortar finishing material composition includes a rubber latex aqueous emulsion for a cement admixture and an inorganic material color powder at a weight ratio of 1:4~1:4.5. The inorganic material color powder comprises: an inorganic filler of 5~10 weight% selected from a group consisting of white cement of 35~50 weight%, nature or artificial silica sand of 40~48 weight%, micro-silica, lime, emery, calcium carbonate, clay, spherical silica(micro shell shape) and a mixture thereof; a viscosity stabilizer of 0.2~1 weight% selected from a group consisting of alumina cement of 0.1~10 weight%, anhydrous gypsum of 0.1~8 weight%, metakaolin of 2~10 weight%, nature fiber, microdot soil and a mixture thereof; a dispersing agent of 0.2~0.7 weight%; an antifoaming agent of 0.2~0.5 weight%; a curing accelerator of 0.1~0.2 weight%; a retarder of 0.1~0.2 weight% and the inorganic pigment of 0.5~5 weight%.
摘要翻译: 提供无机聚合物树脂砂浆整理材料组合物是环境友好的,具有高功能性并且显示出优异的拉伸强度,抗压强度,膨胀和收缩强度和耐磨性。 无机聚合物树脂砂浆整理材料组合物包括用于水泥混合物的橡胶胶乳水性乳液和重量比为1:4〜1:4.5的无机材料着色粉末。 无机材料着色粉末包括:5〜10重量%的无机填料,选自35〜50重量%的白色水泥,40〜48重量%的天然或人造硅砂,微硅石,石灰,金刚砂 ,碳酸钙,粘土,球形二氧化硅(微壳形)及其混合物; 选自0.1〜10重量%的氧化铝水泥,0.1〜8重量%的无水石膏,2〜10重量%的偏高岭土,自然纤维,微孔土及其混合物的0.2〜1重量%的粘度稳定剂 ; 0.2〜0.7重量%的分散剂; 0.2〜0.5重量%的消泡剂; 固化促进剂为0.1〜0.2重量% 0.1〜0.2重量%的缓凝剂,0.5〜5重量%的无机颜料。
-
公开(公告)号:KR100831846B1
公开(公告)日:2008-05-22
申请号:KR1020070048761
申请日:2007-05-18
CPC分类号: C04B28/001 , C04B2103/0097 , C04B2111/00017 , C04B2111/00025 , C04B14/041 , C04B14/047 , C04B14/06 , C04B14/20 , C04B22/124 , C04B24/128
摘要: A mortar composition based on zeolite is provided to obtain a building finishing material capable of preventing emission of various harmful substances and adsorbing harmful substances present in an indoor environment, thereby realizing an excellent air refreshing effect. A mortar composition as a building finishing material for imparting an air refreshing effect to an indoor environment comprises: a mixture containing 52.998-60 wt% of zeolite, 8-12 wt% of bentonite, 8-12 wt% of illite, 4-6 wt% of feldspar, 13-17 wt% of quartz and 0.001-0.002 wt% of chlorophyll, and water, wherein the mixing ratio of the mixture and water is 75-80:20-25. In a variant, the mortar composition comprises a chloride solution instead of water. Further, a size of particles of the zeolite is 100 to 300 nm.
摘要翻译: 提供了一种基于沸石的砂浆组合物以获得能够防止各种有害物质的排放和吸附室内环境中存在的有害物质的建筑物整理材料,从而实现优异的空气清新效果。 作为用于向室内环境赋予空气清新效果的建筑物整理材料的砂浆组合物包括:含有52.998-60重量%的沸石,8-12重量%的膨润土,8-12重量%的伊利石,4-6 重量%的长石,13-17重量%的石英和0.001-0.002重量%的叶绿素和水,其中混合物和水的混合比为75-80:20-25。 在一个变型中,砂浆组合物包含氯化物溶液而不是水。 此外,沸石的颗粒尺寸为100〜300nm。
-
-
-
-
-
-
-
-
-