YELLOW PIGMENT COMPOSITION
    1.
    发明申请

    公开(公告)号:US20220153997A1

    公开(公告)日:2022-05-19

    申请号:US17602019

    申请日:2020-04-07

    Applicant: BASF SE

    Abstract: Described herein is a composition, including bismuth vanadate pigment dispersed in a copolymer of ethylene with at least one comonomer, selected from the group consisting of (meth)acrylic acid, C1-12-alkyl (meth)acrylates and maleic anhydride.

    Pale-colored flame-retardant polyamides
    3.
    发明授权
    Pale-colored flame-retardant polyamides 有权
    浅色阻燃聚酰胺

    公开(公告)号:US09388341B2

    公开(公告)日:2016-07-12

    申请号:US13847511

    申请日:2013-03-20

    Applicant: BASF SE

    CPC classification number: C09K21/14 B01F3/1221 B01F7/164 C08K5/34928 C08L77/00

    Abstract: Thermoplastic molding compositions comprising A) from 10 to 98% by weight of a thermoplastic polyamide, B) from 0.1 to 60% by weight of red phosphorus, C) from 0.5 to 20% by weight of a melamine compound, D) from 1 to 30% by weight of titanium dioxide in the rutile form, E) from 0 to 40% by weight of an impact modifier, and F) from 0 to 60% by weight of further additives, where the sum of the percentages by weight of components A) to F) is 100%.

    Abstract translation: 热塑性成型组合物,其包含A)10至98重量%的热塑性聚酰胺,B)0.1至60重量%的红磷,C)0.5至20重量%的三聚氰胺化合物,D)1至 30重量%的金红石形式的二氧化钛,E)0-40重量%的抗冲改性剂,F)0-60重量%的其它添加剂,其中组分重量百分比的总和 A)至F)为100%。

    PALE-COLORED FLAME-RETARDANT POLYAMIDES
    4.
    发明申请
    PALE-COLORED FLAME-RETARDANT POLYAMIDES 有权
    色彩鲜艳的阻燃聚氨酯

    公开(公告)号:US20130248782A1

    公开(公告)日:2013-09-26

    申请号:US13847511

    申请日:2013-03-20

    Applicant: BASF SE

    CPC classification number: C09K21/14 B01F3/1221 B01F7/164 C08K5/34928 C08L77/00

    Abstract: Thermoplastic molding compositions comprising A) from 10 to 98% by weight of a thermoplastic polyamide, B) from 0.1 to 60% by weight of red phosphorus, C) from 0.5 to 20% by weight of a melamine compound, D) from 1 to 30% by weight of titanium dioxide in the rutile form, E) from 0 to 40% by weight of an impact modifier, and F) from 0 to 60% by weight of further additives, where the sum of the percentages by weight of components A) to F) is 100%.

    Abstract translation: 热塑性成型组合物,其包含A)10至98重量%的热塑性聚酰胺,B)0.1至60重量%的红磷,C)0.5至20重量%的三聚氰胺化合物,D)1至 30重量%的金红石形式的二氧化钛,E)0-40重量%的抗冲改性剂,F)0-60重量%的其他添加剂,其中组分重量百分比的总和 A)至F)为100%。