摘要:
In order to provide a method of producing a cathode ray tube in a manner which well matches with a usual technique of producing a cathode ray tube by forming a spiral high-resistor on an inner face of a glass tube, in an electron gun of which a main focusing lens is configured by the spiral high-resistor, the step of fritting seal rings to both ends of the glass tube in which a hole is opened in the center portion; the step of applying a high-resistor paste to the glass tube, drying the paste, and then forming a spiral structure in the high-resistor film; the step of firing at 420 to 550 deg. C.; and the step of combining other electron gun parts to form the electron gun are included, and the spiral high-resistor is formed by a high-resistor paste in which ruthenium oxide is added to a glass material having a softening point that is lower than the annealing point of the glass tube.
摘要:
The present invention relates to a plasma display device apt to increase luminance of a phosphor layer and prevent degradation of a discharge characteristic, and to a phosphor used for the device. This plasma display device has a green phosphor having a crystal structure of Zn2SiO4:Mn, and a monovalent oxide is substituted for part of the green phosphor. The monovalent oxide is one or more of lithium oxide (Li2O), sodium oxide (Na2O), potassium oxide (K2O), cesium oxide (Cs2O), rubidium oxide (Rb2O), copper oxide (Cu2O), and silver oxide (Ag2O). This structure allows reduction of oxygen defects occurring in the green phosphor, suppression of the luminance decrease of the green phosphor, and improvement of a discharge characteristic.
摘要翻译:本发明涉及一种能够增加荧光体层的亮度并防止放电特性劣化的等离子体显示装置以及用于该装置的荧光体。 该等离子体显示装置具有具有Zn 2+ SiO 4·Mn的晶体结构的绿色荧光体,并且一价氧化物被一部分绿色荧光体所代替。 一价氧化物是氧化锂(Li 2 O 2),氧化钠(Na 2 O 2),氧化钾(K 2 O 3) O),氧化铯(Cs 2 O),氧化铷(Rb 2 O),氧化铜(Cu 2 O 2)和银 氧化物(Ag 2 O)。 这种结构可以减少在绿色荧光体中发生的氧缺陷,抑制绿色荧光体的亮度降低和放电特性的改善。
摘要:
The present invention provides an ethylene-hexafluoropropylene copolymer which is suitable as a hose or seal for engine oil of an automobile and has sufficient amine resistance, while maintaining heat resistance, oil resistance and chemical resistance close to that of conventional fluorine rubber. The ethylene-hexafluoropropylene copolymer comprises 35 to 60% by mole of ethylene structural unit, 25 to 50% by mole of hexafluoropropylene structural unit and 0 to 15% by mole of structural unit derived from a monomer copolymerizable therewith and has a fluorine content of at least 60% by weight and number average molecular weight of 3,000 to 500,000.
摘要:
An ultraviolet-crosslinkable polymer composition comprising a polymer containing iodine and/or bromine in an amount of from 0.001 to 10% by weight, a photoinitiator as a crosslinking agent and a polyfunctional unsaturated compound as a crosslinking aid. By using iodine and/or bromine as a crosslinking point, it is possible to carry out crosslinking of various polymers including fluorine-containing polymers which have been very difficult to crosslink with ultraviolet rays, and molding or processing can be made easily at working site at low temperature.
摘要:
Disclosed is a plasma display device that provides high luminance and minimal degradation in luminance under panel operations. A blue phosphor in a phosphor layer has a crystal structure of MeMgSi2O6:Eu or Me3MgSi2O8:Eu (where, Me contains at least one of Ca, Sr, and Ba) produced with a precursor that is obtained by any one of methods: an aqueous solution synthesis method, a spray synthesis method, a hydrothermal synthesis method, and a hydrolysis method. The phosphor has an average particle diameter ranging from 0.1 to 3.0 μm.
摘要翻译:公开了一种在面板操作下提供高亮度和最小亮度劣化的等离子体显示装置。 荧光体层中的蓝色荧光体具有MeMgSi 2 O 6:Eu或Me 3 M 2 Si 2 N 2的晶体结构 Eu(其中,Me含有Ca,Sr和Ba中的至少一种),其通过以下任一方法获得的前体制备:水溶液合成法,喷雾合成法 方法,水热合成法和水解法。 荧光体的平均粒径为0.1〜3.0μm。
摘要:
The present invention has as its objective to provide a display panel with silver electrodes without yellowing, and a method of producing such a display panel. After patterning and applying silver paste to form display electrodes on a substrate, glass paste is applied to form the dielectric layer, covering the electrodes, and both layers are simultaneously baked. Glass frit contained in the silver paste is chosen to have a lower softening point than die glass contained in the glass paste, and the baking process is divided into a first step, in which the baking temperature is equal to or higher than the softening point of the glass frit but lower than the softening point of the glass, and a second step, in which the baking temperature is higher than the softening point of the glass. This process allows a display panel to be produced with fewer bakings and reduced yellowing.
摘要:
The present invention relates to a process for preparing an elastomeric ethylene-hexafluoropropylene copolymer with excellent vulcanization properties, which comprises emulsion polymerizing ethylene, hexafluoropropylene and when in demand, a monomer copolymerizable therewith in a aqueous medium at a low temperature of −20° C. to 40° C. using a radical polymerization initiator.
摘要:
The present invention has as its objective to provide a display panel with silver electrodes without yellowing, and a method of production such a display panel. After patterning and applying silver paste to form display electrodes on the substrate, glass paste is applied to form the dielectric layer, covering the electrodes, and both layers are simultaneously baked. Glass flit contained in the silver paste is chosen to have a lower softening point than the glass contained in the glass paste, and the baking process is divided into a first step, in which the baking temperature is equal to or higher than the softening point of the glass flit but lower than the softening point of the glass, and a second step, in which the baking temperature is higher than the softening point of the glass. This process allows a display panel to be produced with fewer bakings and reduced yellowing.
摘要:
The object of the present invention is to provide a thermoplastic polymer composition which is flexible and capable of melt-molding and has excellent heat resistance, chemical resistance and oil resistance. Another object of the present invention is to provide a molded article, a laminated article, a hose for industrial use, a tube for industrial use, a fuel hose and a fuel tube comprising the thermoplastic polymer composition. Further object of the present invention is to provide a process for preparing a thermoplastic polymer composition. The thermoplastic polymer composition comprises a fluororesin (A) comprising a fluorine-containing ethylenic polymer (a) and a crosslinked fluororubber (B) in which at least a part of at least one kind of fluororubber (b) is crosslinked, and a weight ratio of the fluororesin (A) to the crosslinked fluororubber (B) is 85/15 to 40/60, a fuel permeation coefficient of a molded article obtained from the composition is not more than 40 g·mm/m2·day and a tensile modulus of elasticity of the molded article is not more than 400 MPa.
摘要:
An object of the present invention is to provide a thermoplastic polymer composition which is flexible and capable of melt-molding and has excellent heat resistance and chemical resistance. Further object of the present invention is to provide a molded article, a sealing material, peripheral parts of fuel system, a fuel hose and a fuel container comprising the thermoplastic polymer composition. The present invention relates to a thermoplastic polymer composition comprising a fluororesin (A) containing a fluorine-containing ethylenic polymer (a), a crosslinked fluororubber (B) in which at least a part of at least one kind of fluororubber (b) is crosslinked, and a fluorine-containing thermoplastic elastomer (C).