Battery
    3.
    发明授权
    Battery 失效
    电池

    公开(公告)号:US07510803B2

    公开(公告)日:2009-03-31

    申请号:US10486635

    申请日:2002-08-23

    IPC分类号: H01M4/52 H01M4/58 H01M10/40

    摘要: A battery with a high battery voltage at charging and improved energy density is provided. A cathode (12) and an anode (14) are laminated with a separator (15) sandwiched therebetween which is impregnated with an electrolyte. The cathode (12) has a cathode active material including a lithium composite oxide which contains lithium, at least either cobalt or nickel, and oxygen. The battery voltage at charging is 4.25 V or more. The total amount of lithium carbonate and lithium sulphate in the cathode (12) to the cathode active material is 1.0 wt % or less, a concentration of protic impurities in the electrolyte, which is converted to a mass ratio of protons to the electrolyte, is 20 ppm or less, or moisture content in the electrolyte is 20 ppm mass ratio or less to the electrolyte. This inhibits metal eluting from the lithium composite oxide even at high voltages.

    摘要翻译: 提供了在充电时具有高电池电压并且提高能量密度的电池。 阴极(12)和阳极(14)与夹在其间的隔膜(15)层叠,浸渍有电解质。 阴极(12)具有包含锂复合氧化物的正极活性物质,所述锂复合氧化物含有至少钴或镍的锂和氧。 充电时的电池电压为4.25V以上。 阴极(12)与阴极活性物质的碳酸锂和硫酸锂的总量为1.0重量%以下,电解质中的质子杂质的浓度转换为质子与电解质的质量比为 20ppm以下,或电解质中的水分含量与电解质的质量比为20ppm以下。 即使在高电压下也能抑制锂复合氧化物洗脱的金属。

    Solid electrolyte battery with porous members between exposed current collectors and method for manufacturing same
    4.
    发明授权
    Solid electrolyte battery with porous members between exposed current collectors and method for manufacturing same 失效
    固体电解质电池与暴露的集电器之间的多孔构件及其制造方法

    公开(公告)号:US06890687B2

    公开(公告)日:2005-05-10

    申请号:US10137070

    申请日:2002-05-02

    摘要: A solid electrolyte battery includes a battery element in which a cathode having a cathode composite mixture layer formed by applying a cathode composite mixture on a cathode current collector so as to provide a part to which the cathode composite mixture is not applied at an end part in the longitudinal direction of the cathode current collector and an anode having an anode composite mixture layer formed by applying an anode composite mixture on an anode current collector so as to provide a part to which the anode composite mixture is not applied at an end part in the longitudinal direction of the anode current collector are laminated so as to provide a solid electrolyte layer between the cathode and the anode. Porous members made of ceramics or non-woven fabrics are arranged between the longitudinal end parts of the cathode composite mixture layer and the longitudinal end parts of the anode composite mixture layer to extend to the parts of the cathode current collector to which the cathode composite mixture is not applied. Thus, a short-circuit in the end parts of the cathode composite mixture layer is prevented and yield upon manufacturing the solid electrolyte battery is improved.

    摘要翻译: 固体电解质电池包括电池元件,其中具有阴极复合混合物层的阴极,阴极复合混合物层通过在阴极集电器上施加阴极复合材料混合物而形成,以便提供阴极复合材料混合物未在其末端部分施加的部分 阴极集电体的纵向方向和具有通过在阳极集电器上施加阳极复合材料混合物而形成的阳极复合材料混合物层的阳极,以便提供阳极复合材料混合物未在其中的端部处施加的部分 层叠阳极集电体的纵向,以在阴极和阳极之间提供固体电解质层。 由陶瓷或无纺布制成的多孔构件设置在阴极复合材料层的纵向端部与阳极复合材料层的纵向端部之间延伸到阴极复合混合物的阴极集电体部分 不适用。 因此,可以防止阴极复合混合层的端部短路,提高制造固体电解质电池时的产率。