摘要:
A foamed sheet including: a polylactic acid; and a filler, wherein the foamed sheet has a compressive stress of 0.2 Mpa or less when the cushioning coefficient of the foamed sheet is 10 or less; and wherein the foamed sheet has a puncture strength of 2 N or more when the sheet thickness of the foamed sheet is 2 mm.
摘要:
Provided is a toner including at least: a non-crystalline polyester resin; and a crystalline polyester resin, wherein when a cross-section of the toner is observed, the crystalline polyester resin has a maximum length of 100 nm or greater but less than 500 nm, and a ratio Dv/Dn of a volume average diameter Dv of the crystalline polyester resin to a number average diameter Dn of the crystalline polyester resin is less than 1.20.
摘要:
To provide a polymer production apparatus, which contains: a first supply unit configured to supply raw materials including a monomer; a second supply unit configured to supply a compressive fluid; a contact unit configured to bring the monomer into contact with the compressive fluid; and a reaction unit configured to allow the monomer, which has been brought into contact with the compressive fluid, to react in the presence of the compressive fluid, wherein the reaction unit contains one, or two or more extrusion devices, and one, or two or more stirring devices.
摘要:
Provided is a polymer product that has a melting point difference (Tm1−Tm0) of 3° C. or more between a polymer melting point Tm0 before it is heated and a polymer melting point Tm1 after it is heated under a nitrogen atmosphere for 60 minutes at a temperature that is higher than the highest polymer melting point by from 10° C. to 50° C.
摘要:
Toner contains a binder resin and a colorant, wherein the binder resin contains a resin having a polyhydroxy carboxylic acid skeleton, wherein the toner has a half effusion temperature of from 80° C. to 120° C. as measured by a temperature rising method using a flow tester.
摘要:
A method of manufacturing an aliphatic polyester resin composition is provided. The method includes kneading an aliphatic polyester resin and a filler at a temperature lower than a melting point of the aliphatic polyester resin in the presence of a compressible fluid.
摘要:
To provide a polymer product, which contains aliphatic polycarbonate, wherein an oxide unit content in the aliphatic polycarbonate is 20 mol % or less, and wherein a monomer content in the aliphatic polycarbonate is 500 ppm or less, where the monomer is a monomer that is a base of the aliphatic polycarbonate.
摘要:
A toner prepared by a method comprising granulating while polymerizing a ring-opening polymerizable monomer with a catalyst under the presence of a surfactant and a colorant in a compressible fluid.
摘要:
A toner including a colorant and a first binder resin is provided. The first binder resin has first and second glass transition points at a temperature Tg1 of −20 to 20° C. and a temperature Tg2 of 35 to 65° C., respectively, measured by a differential scanning calorimeter at a heating rate of 5° C./min. A ratio h1/h2 of a baseline displacement h1 observed in the first glass transition point to a baseline displacement h2 observed in the second glass transition point is less than 1.0. The first binder resin has a structure in which a first phase is dispersed in a second phase. The first and second phases consist of portions having larger and smaller phase difference values, respectively, than an intermediate value between maximum and minimum phase difference values in a binarized phase image obtained by an atomic force microscope with a tapping mode method.
摘要:
An aliphatic polyester resin composition contains an aliphatic polyester resin and a cross-linking agent, wherein the proportion of the gel proportion of the aliphatic polyester resin composition is less than 5 percent, wherein the weight average molecular weight of the aliphatic polyester resin composition after the aliphatic polyester resin composition is melted at 200° C. for 10 minutes increases by 50,000 or greater compared to the weight average molecular weight of the aliphatic polyester resin composition before the aliphatic polyester resin composition is melted at 200° C. for 10 minutes.