DIMENSIONALLY STABLE FAST ETCHING GLASSES
    102.
    发明申请
    DIMENSIONALLY STABLE FAST ETCHING GLASSES 审中-公开
    尺寸稳定的快速蚀刻玻璃

    公开(公告)号:US20160168014A1

    公开(公告)日:2016-06-16

    申请号:US15048492

    申请日:2016-02-19

    CPC classification number: C03C3/093 C03C3/087 C03C3/091

    Abstract: Substantially alkali free glasses are disclosed with can be used to produce substrates for flat panel display devices, e.g., active-matrix liquid crystal displays (AMLCDs). The glasses have high annealing temperatures and etch rates. Methods for producing substantially alkali free glasses using a downdraw process (e.g., a fusion process) are also disclosed.

    Abstract translation: 公开了基本上不含碱的玻璃,其可以用于制造用于平板显示装置的基板,例如有源矩阵液晶显示器(AMLCD)。 玻璃具有很高的退火温度和蚀刻速率。 还公开了使用下拉工艺(例如,熔融工艺)生产基本上无碱玻璃的方法。

    METHODS AND APPARATUS FOR STRENGTH AND/OR STRAIN LOSS MITIGATION IN COATED GLASS
    103.
    发明申请
    METHODS AND APPARATUS FOR STRENGTH AND/OR STRAIN LOSS MITIGATION IN COATED GLASS 审中-公开
    用于强度和/或应变涂层玻璃中的损失的方法和装置

    公开(公告)号:US20160060161A1

    公开(公告)日:2016-03-03

    申请号:US14838482

    申请日:2015-08-28

    Abstract: Methods and apparatus provide for: a glass substrate having a first strain to failure characteristic, a first elastic modulus characteristic, and a flexural strength; and a coating applied over the glass substrate to produce a composite structure in order to increase a hardness thereof, where the coating has a second strain to failure characteristic and a second elastic modulus characteristic, where the first strain to failure characteristic is higher than the second strain to failure characteristic, and one of: (i) the first elastic modulus characteristic is above a minimum predetermined threshold such that any reduction of the flexural strength of the glass substrate resulting from application of the coating is mitigated; and (ii) the first elastic modulus characteristic is below a maximum predetermined threshold such that any reduction of the strain to failure of the glass substrate resulting from application of the coating is mitigated.

    Abstract translation: 方法和装置提供:具有第一应变失效特性,第一弹性模量特性和弯曲强度的玻璃基底; 以及施加在玻璃基板上的涂层以产生复合结构以增加其硬度,其中涂层具有第二应变破坏特性和第二弹性模量特性,其中第一应变破坏特性高于第二应变破坏特性 应变破坏特性,以及(i)第一弹性模量特性高于最小预定阈值,从而减轻了施加涂层导致的玻璃基板的弯曲强度的任何降低; 和(ii)第一弹性模量特性低于最大预定阈值,从而减轻由于施加涂层导致的玻璃基板的破坏应变的任何减少。

    OPAQUE COLORED GLASS-CERAMICS COMPRISING NEPHELINE CRYSTAL PHASES
    104.
    发明申请
    OPAQUE COLORED GLASS-CERAMICS COMPRISING NEPHELINE CRYSTAL PHASES 有权
    OPAQUE彩色玻璃陶瓷,包括NEPHELINE CRYSTAL PHASES

    公开(公告)号:US20150284288A1

    公开(公告)日:2015-10-08

    申请号:US14672854

    申请日:2015-03-30

    Abstract: Disclosed herein are opaque glass-ceramics comprising at least one nepheline crystal phase and comprising from about 30 mol % to about 65 mol % SiO2, from about 15 mol % to about 40 mol % Al2O3, from about 10 mol % to about 20 mol % (Na2O+K2O), and from about 1 mol % to about 10 mol % (ZnO+MgO). Also disclosed herein are opaque-glass ceramics comprising at least one nepheline crystal phase and at least one spinel-structure phase doped with at least one colorant chosen from transition metals and rare earth elements. Further disclosed herein are methods for making these opaque glass-ceramics. e opaque glass-ceramics.

    Abstract translation: 本文公开了包含至少一个霞石结晶相的不透明玻璃陶瓷,其包含约30mol%至约65mol%的SiO 2,约15mol%至约40mol%的Al 2 O 3,约10mol%至约20mol% (Na 2 O + K 2 O)和约1mol%至约10mol%(ZnO + MgO)。 本文还公开了包含至少一个霞石结晶相和掺杂有选自过渡金属和稀土元素的至少一种着色剂的至少一个尖晶石结构相的不透明玻璃陶瓷。 本文进一步公开了制造这些不透明玻璃陶瓷的方法。 不透明玻璃陶瓷。

    ALKALI-FREE PHOSPHOBOROSILICATE GLASS
    110.
    发明申请
    ALKALI-FREE PHOSPHOBOROSILICATE GLASS 有权
    无碱无机硅玻璃

    公开(公告)号:US20140335331A1

    公开(公告)日:2014-11-13

    申请号:US14267086

    申请日:2014-05-01

    Abstract: Alkali-free phosphoboroaluminosilicate glasses are provided. The glasses include the network formers SiO2, B2O3, and at least one of Al2O3 and P2O5. The glass may, in some embodiments, have a Young's modulus of less than about 78 GPa and/or a coefficient of thermal expansion, averaged over a temperature range from about 20° C. to about 300° C., of less than about 38×10−7/° C. The glass may be used as a cover glass for electronic devices or as an outer clad layer for a glass laminate.

    Abstract translation: 提供了无碱磷钼硼硅玻璃。 玻璃包括网络形成体SiO 2,B 2 O 3以及Al 2 O 3和P 2 O 5中的至少一种。 在一些实施方案中,玻璃在约20℃至约300℃的温度范围内具有小于约78GPa的杨氏模量和/或热膨胀系数小于约38 ×10-7 /℃。该玻璃可以用作电子器件的玻璃罩或玻璃层压板的外包层。