公开(公告)号:US20220259439A1
公开(公告)日:2022-08-18
申请号:US17625090
申请日:2020-06-09
Applicant: FIRST POINT A.S.
Inventor: Gabriela Chlandová , Petr Spaniel
IPC: C09D1/04 , C09D7/61 , C09D7/63 , C09D7/65 , C08K3/34 , C08K3/04 , C08K7/14 , C08K7/28 , C08K5/19 , C08L25/14 , B05D7/14 , B05D7/00
Abstract: The invention relates to a coating composition, especially to a coating composition intended for thermal insulation of hot metals, which contains an aqueous solution of silicate and which consists of the first layer containing 35 to 71 volume percent of hollow glass spheres, 26 to 62 volume percent of an aqueous solution of potassium silicate, 1 to 3 volume percent of an adhesive additive, and 0.1 volume percent of a water glass stabilizer, and of at least one second layer containing 71 to 84.6 volume percent of hollow glass spheres, 9 to 22.6 volume percent of an aqueous solution of potassium silicate, 0.2 to 0.3 volume percent of an adhesive additive, 0.1 volume percent of a water glass stabilizer, 2 to 3 volume percent of cut glass fibres, and 1.7 to 3 volume percent of a styrene-acrylate dispersion. Method of application of the coating composition, especially method of application of the coating composition which consists of at least one layer containing an aqueous solution of silicate according to which, as the first step, the first layer containing 35 to 71 volume percent of hollow glass spheres, 26 to 62 volume percent of an aqueous solution of potassium silicate, 1 to 3 volume percent of an adhesive additive, and 0.1 volume percent of a water glass stabilizer is applied and then the second layer containing 71 to 84.6 volume percent of hollow glass spheres, 9 to 22.6 volume percent of an aqueous solution of potassium silicate, 0.2 to 0.3 volume percent of an adhesive additive, 0.1 volume percent of a water glass stabilizer, 2 to 3 volume percent of cut glass fibres, and 1.7 to 3 volume percent of a styrene-acrylate dispersion is applied onto the first layer.
-
公开(公告)号:US12138823B2
公开(公告)日:2024-11-12
申请号:US17627661
申请日:2020-06-09
Applicant: FIRST POINT A.S.
Inventor: Gabriela Chlandová , Petr Španiel
Abstract: A wood chip material, especially a fireproof water resistant wood chip material, especially a fireproof water resistant wood chip material to make oriented strand boards which consists of a mixture containing 30 to 43 weight percent of wood chips, 53 to 61.9 weight percent of an aqueous solution of silicate, 2 to 5 weight percent of aluminium hydroxide, 1 to 3 weight percent of water, 0.1 to 1 weight percent of a stabilizer of the aqueous solution of silicate, and a hardener of the aqueous solution of sodium silicate in the concentration of 0.5 to 5 weight percent to the pure aqueous solution of sodium silicate providing always that the density of the aqueous solution of sodium silicate ranges from 1370 to 1400 kg/m3 and the SiO2 to NA2O molar ratio in the aqueous solution of sodium silicate ranges from 3.2 to 3.4. A method of production of a wood chip material, especially method of production of a fireproof water resistant wood chip material, especially method of production of a fireproof water resistant wood chip material to make oriented strand boards according to which, as the first step, the aluminium hydroxide is mixed with water, then wood chips are added into the mixture and everything is stirred thoroughly in such a manner that a wood chip mixture is formed, then the stabilizer of the aqueous solution of sodium silicate is added in the aqueous solution of silicate and after that the hardener of the aqueous solution of sodium silicate is admixed in this solution. Then the solution is stirred for 1 to 10 minutes until a binding solution is formed. Then the wood chip mixture is poured, at continuous stirring, in the binding solution and everything is stirred thoroughly again. Then the resulting mixture is poured in the place of application.
-
公开(公告)号:US12071580B2
公开(公告)日:2024-08-27
申请号:US17627667
申请日:2020-06-26
Applicant: FIRST POINT A.S.
Inventor: Gabriela Chlandová , Petr {hacek over (S)}paniel
IPC: C09K21/02 , C04B14/42 , C04B28/26 , C04B111/00 , C04B111/28
CPC classification number: C09K21/02 , C04B14/42 , C04B28/26 , C04B2111/00017 , C04B2111/28
Abstract: A fire-proof material, in particular a fire-proof thermal insulation material containing water glass, which is composed of a compound which contains 34 to 49.9 wt % of inorganic non-flammable fibres, 50 to 65 wt % of an aqueous silicate solution, and 0.1 to 1 wt % of water glass stabiliser, while it further contains a water glass hardener and the aqueous silicate solution has a density in the range of 1370 to 1400 kg/m3 and a molar ratio of SiO2 to Na2O in the range of 3.2 to 3.4.
-
公开(公告)号:US20220315489A1
公开(公告)日:2022-10-06
申请号:US17624835
申请日:2020-05-26
Applicant: FIRST POINT A.S.
Inventor: Gabriela Chlandová , Petr Spaniel
Abstract: An insulating material, in particular a permeable fire-proof insulating material comprising water glass and polystyrene, consisting of a hardening mixture which contains 1 to 32.4 wt % of expanded polystyrene, 57.5 to 96.0 wt % of aqueous sodium silicate solution, 2 to 6 wt % of aluminium hydroxide, 0.8 to 2.6 wt % water glass hardener and 0.1 to 0.5 wt % of water glass stabilizer, while the surface of the expanded polystyrene is provided with carbon black, the carbon black making up 0.1 to 1 wt % of total weight. A method for the production of insulating material, in particular a method for the production of permeable fire-proof insulating material comprising water glass and polystyrene, according to which firstly the polystyrene beads are mixed with an aqueous solution of carbon black so as to coat their entire surface, then is added to the aqueous sodium silicate solution aluminium hydroxide and the whole is mixed so as to form an insulating mixture, and then a water glass stabilizer is added to the aqueous sodium silicate solution, and then to this solution is mixed water glass hardener, with this solution being further stirred for 1 to 10 minutes to form a binder solution, and the insulating mixture is added to the binder solution with constant stirring, and the whole is mixed, and the resulting mixture is then poured into the application site.
-
公开(公告)号:US20220267613A1
公开(公告)日:2022-08-25
申请号:US17624841
申请日:2020-05-26
Applicant: FIRST POINT A.S.
Inventor: Gabriela Chlandová , Petr Spaniel
Abstract: A surface protection compound, in particular a compound for the non-flammable water-resistant non-hazardous biocidal surface protection of wood, or paper, or textile, or plastic, which contains an aqueous silicate solution which contains 93 to 98 wt % of an aqueous solution of potassium silicate, 1 to 6 wt % of aluminium hydroxide and, 0.5 to 1.5 wt % of stabiliser of the aqueous solution of potassium silicate.
-
公开(公告)号:US20220242791A1
公开(公告)日:2022-08-04
申请号:US17627669
申请日:2020-06-26
Applicant: FIRST POINT A.S.
Inventor: Gabriela Chlandová , Petr Spaniel
Abstract: An insulating material, in particular a permeable fire-proof insulating material comprising water glass and which is composed of a air harden-able compound which contains 2 to 40 wt % of plastic balls, 55 to 95.0 wt % of aqueous sodium silicate solution, 2 to 6 wt % of aluminium hydroxide, and 0.1 to 0.5 wt % water glass stabiliser. A method for the production of insulating material, in particular a method for the production of permeable fire-proof insulating material comprising water glass and plastic balls, according to which firstly the plastic balls are mixed with an aqueous solution of carbon black so as to coat their entire surface, then is added to the aqueous sodium silicate solution aluminium hydroxide and the whole is mixed so as to form an insulating mixture, and then a water glass stabiliser is added to the aqueous sodium silicate solution, and then to this solution is mixed water glass hardener, with this solution being further stirred for 1 to 10 minutes to form a binder solution, and the insulating mixture is added to the binder solution with constant stirring, and the whole is mixed, and the resulting mixture is then poured into the application site.
-
-
-
-
-