COATINGS FOR BUILDING PANELS
    4.
    发明公开

    公开(公告)号:US20240141177A1

    公开(公告)日:2024-05-02

    申请号:US18383640

    申请日:2023-10-25

    CPC classification number: C09D5/18 C09D1/00 C09D1/04 C09D7/63 E04B9/001

    Abstract: Described herein is a building panel comprising a first major exposed surface opposite a second major exposed surface, the building panel comprising: a body having a first major surface opposite a second major surface and a plurality of perforations extending from the first major surface toward the second major surface; a flame-retardant coating atop the first major surface of the body and extending into the plurality of perforations, the coating comprising a silicate compound and an amphoteric surfactant; and wherein the building panel has an airflow resistance of less than about 12,000 rayls as measured between the first major exposed surface and the second major exposed surface.

    Inorganic coating composition which can be cured at low temperature and a preparation method thereof

    公开(公告)号:US20190016899A1

    公开(公告)日:2019-01-17

    申请号:US15929043

    申请日:2018-09-17

    Applicant: Xiaodong LIU

    Inventor: Xiaodong LIU

    Abstract: The present invention relates to coating composition. And in particular, to an inorganic coating composition which can be cured at low temperature and a preparation method thereof. In order to solve the problems that the organic coating is harmful for the environment, the inorganic coating has bad flexibility, and the traditional ceramic coatings need heat and is inconvenient for curing in prior art, the present invention provide an inorganic coating composition which can be cured at low temperature and a preparation method thereof. The inorganic coating composition comprises the ingredient as below: 70-80 wt % of inorganic solution; 5-10 wt % of functional additives, which are potassium titanate, alumina, or a compound thereof; 10-20 wt % of inorganic pigment; 0.5-2.0 wt % of other functional additives. The said inorganic solution comprises the following ingredients: 30-40 wt % of organic alkoxy-silane, 15-20 wt % of organic solvent, and 25-30 wt % of silica sol. The inorganic coating composition is able to be cured at low temperature, the film formed by it has excellent flexibility, and the film will not release harmful organic gases, and is beneficial to the environmental.