Single-source precursor for semiconductor nanocrystals
    14.
    发明授权
    Single-source precursor for semiconductor nanocrystals 有权
    半导体纳米晶体的单源前体

    公开(公告)号:US08287951B2

    公开(公告)日:2012-10-16

    申请号:US12088590

    申请日:2006-06-27

    IPC分类号: B05D7/00

    摘要: A process for preparing a single source solid precursor matrix for semiconductor nanocrystals having the steps of: mixing 0.1-1 Molar of an aqueous/non-aqueous (organic) solution containing the first component of the host matrix with 0.001-0.01 Molar of an aqueous/non-aqueous solution containing the first dopant ions, which needs in situ modification of valency state, dissolving 10-20 milligram of an inorganic salt for the in situ reduction of the first dopant ion in the solution, addition of 0.001-0.01 Molar of an aqueous/non-aqueous solution of an inorganic salt containing the dopant ions which do not need modifications of their valency state, addition of 0.1-1 Molar of an aqueous/non-aqueous solution of an inorganic salt containing the second component of the host material, addition of 5-10% by weight of an aqueous solution containing a pH modifying complexing agent, to obtain a mixture, and heating the mixture to obtain a solid layered micro-structural precursor compound.

    摘要翻译: 制备用于半导体纳米晶体的单源固体前体基质的方法,其具有以下步骤:将含有主体基质的第一组分的0.1-1摩尔水/非水(有机)溶液与0.001-0.01摩尔的水性 /含有第一掺杂剂离子的非水溶液,其需要原位改性的价态,将10-20毫克的无机盐溶解在溶液中原位还原第一掺杂剂离子,加入0.001-0.01摩尔 含有不需要改变其价态的掺杂剂离子的无机盐的水/非水溶液,加入0.1-1摩尔含有主体第二组分的无机盐的水/非水溶液 添加5-10重量%的含有pH改性络合剂的水溶液,得到混合物,加热混合物,得到固体层状微结构前体化合物。

    Single-Source Precursor for Semiconductor Nanocrystals
    15.
    发明申请
    Single-Source Precursor for Semiconductor Nanocrystals 有权
    半导体纳米晶体的单源前体

    公开(公告)号:US20090218550A1

    公开(公告)日:2009-09-03

    申请号:US12088590

    申请日:2006-06-27

    IPC分类号: H01B1/22 C01G9/08 C09K3/00

    摘要: A process for preparing a single source solid precursor matrix for semiconductor nanocrystals having the steps of: mixing 0.1-1 Molar of an aqueous/non-aqueous (organic) solution containing the first component of the host matrix with 0.001-0.01 Molar of an aqueous/non-aqueous solution containing the first dopant ions, which needs in situ modification of valency state, dissolving 10-20 milligram of an inorganic salt for the in situ reduction of the first dopant ion in the solution, addition of 0.001-0.01 Molar of an aqueous/non-aqueous solution of an inorganic salt containing the dopant ions which do not need modifications of their valency state, addition of 0.1-1 Molar of an aqueous/non-aqueous solution of an inorganic salt containing the second component of the host material, addition of 5-10% by weight of an aqueous solution containing a pH modifying complexing agent, to obtain a mixture, and heating the mixture to obtain a solid layered micro-structural precursor compound.

    摘要翻译: 制备用于半导体纳米晶体的单源固体前体基质的方法,其具有以下步骤:将含有主体基质的第一组分的0.1-1摩尔水/非水(有机)溶液与0.001-0.01摩尔的水性 /含有第一掺杂剂离子的非水溶液,其需要原位改性的价态,将10-20毫克的无机盐溶解在溶液中原位还原第一掺杂剂离子,加入0.001-0.01摩尔 含有不需要改变其价态的掺杂剂离子的无机盐的水/非水溶液,加入0.1-1摩尔含有主体第二组分的无机盐的水/非水溶液 添加5-10重量%的含有pH改性络合剂的水溶液,得到混合物,加热混合物,得到固体层状微结构前体化合物。