Method for the manufacture of a hardened part which does not have LME issues

    公开(公告)号:US11162153B2

    公开(公告)日:2021-11-02

    申请号:US15748395

    申请日:2016-07-11

    Applicant: ARCELORMITTAL

    Abstract: The present invention provides a method for the manufacture of a hardened part. The method includes the provision of a steel sheet pre-coated with a metallic coating including from 2.0 to 24.0% by weight of zinc, from 1.1 to 7.0% by weight of silicon, optionally from 1.1 to 8.0% by weight of magnesium when the amount of silicon is between 1.1 and 4.0%, and optionally additional elements chosen from Pb, Ni, Zr, or Hf, the content by weight of each additional element being less than 0.3% by weight, the balance being aluminum and unavoidable impurities and residuals elements, wherein the ratio Al/Zn is above 2.9. The method further includes the cutting of the coated steel sheet to obtain a blank, the thermal treatment of the blank at a temperature between 840 and 950° C. to obtain a fully austenitic microstructure in the steel, the transfer of the blank into a press tool, the hot-forming of the blank to obtain a part, the cooling of the part in order to obtain a microstructure in steel being martensitic or martensitic-bainitic or made of at least 75% of equiaxed ferrite, from 5 to 20% of martensite and bainite in amount less than or equal to 10%.

    Method for the manufacture of a phosphatable part starting from a steel sheet coated with a metallic coating based on aluminum

    公开(公告)号:US11414737B2

    公开(公告)日:2022-08-16

    申请号:US15748262

    申请日:2016-07-29

    Applicant: ARCELORMITTAL

    Abstract: A method for the manufacture of a hardened part coated with a phosphatable coating is provided. The method includes providing a steel sheet pre-coated with a metallic coating including from 4.0 to 20.0% by weight of zinc, from 1.0 to 3.5% by weight of silicon, optionally from 1.0 to 4.0% by weight of magnesium, and optionally additional elements chosen from Pb, Ni, Zr, or Hf, the content by weight of each additional element being less than 0.3% by weight, the balance being aluminum and unavoidable impurities and residuals elements. The steel sheet is cut to obtain a blank, the blank is thermally treated at a temperature between 840 and 950° C. to obtain a fully austenitic microstructure in the steel, the blank is transferred into a press tool and hot-formed to obtain a part. The part is cooled to obtain a martensitic or martensitic-bainitic microstructure or made of at least 75% of equiaxed ferrite, from 5 to 20% of martensite and bainite in amount less than or equal to 10%.