Abstract:
The present invention relates to a process for producing a shaped body by selective laser sintering of a sinter powder (SP). The sinter powder (SP) comprises at least one semicrystalline polyamide, at least one nylon-6I/6T and at least one polyaryl ether. The present invention further relates to a shaped body obtainable by the process of the invention and to the use of a polyaryl ether in a sinter powder (SP) for broadening the sintering window (WSP) of the sinter powder (SP).
Abstract:
The present invention relates to a process for producing a shaped body, wherein, in step i), a layer of a sinter powder (SP) comprising at least one mineral flame retardant inter alia is provided and, in step ii), the layer provided in step i) is exposed. The present invention further relates to a process for producing a sinter powder (SP) and to a sinter powder (SP) obtainable by this process. The present invention also relates to the use of the sinter powder (SP) in a sintering process and to shaped bodies obtainable by the process of the invention.
Abstract:
Thermoplastic molding compositions comprising A) from 10 to 99.7% by weight of a polyamide, B) from 1 to 30% by weight of an impact modifier, C) from 0.1 to 10% by weight of a copolymer of C1) from 50 to 95% by weight of styrene or substituted styrenes of the general formula I or a mixture of these in which R is an alkyl radical having from 1 to 8 carbon atoms or a hydrogen atom and R1 is an alkyl radical having from 1 to 8 carbon atoms and n has the value 0, 1, 2, or 3, and C2) from 5 to 50% by weight of structural units derived from one or more dicarboxylic anhydrides, D) from 0.001 to 20% by weight of iron powder, E) from 0.05 to 3% by weight of a copper-containing stabilizer, F) from 100 ppm to 5% by weight of a phosphorus-containing, inorganic acid or salts thereof or ester derivatives thereof or a mixture thereof, G) from 0 to 2% by weight of a polyethyleneimine homo- or copolymer, H) from 0 to 60% by weight of further additives, where the total of the percentages by weight of A) to H) is 100%.
Abstract:
Thermoplastic molding compositions comprising A) from 10 to 99.7% by weight of a polyamide, B) from 1 to 30% by weight of an impact modifier, C) from 0.1 to 10% by weight of a copolymer of C1) from 50 to 95% by weight of styrene or substituted styrenes of the general formula I or a mixture of these in which R is an alkyl radical having from 1 to 8 carbon atoms or a hydrogen atom and R1 is an alkyl radical having from 1 to 8 carbon atoms and n has the value 0, 1, 2, or 3, and C2) from 5 to 50% by weight of structural units derived from one or more dicarboxylic anhydrides, D) from 0.001 to 20% by weight of iron powder, E) from 0.05 to 3% by weight of a copper-containing stabilizer, F) from 100 ppm to 5% by weight of a phosphorus-containing, inorganic acid or salts thereof or ester derivatives thereof or a mixture thereof, G) from 0 to 2% by weight of a polyethyleneimine homo- or copolymer, H) from 0 to 60% by weight of further additives, where the total of the percentages by weight of A) to H) is 100%.
Abstract:
Thermoplastic molding compositions comprising A) from 10 to 99.7% by weight of a polyamide, B) from 1 to 30% by weight of an impact modifier, C) from 0.1 to 10% by weight of a copolymer of C1) from 50 to 95% by weight of styrene or substituted styrenes of the general formula I or a mixture of these in which R is an alkyl radical having from 1 to 8 carbon atoms or a hydrogen atom and R1 is an alkyl radical having from 1 to 8 carbon atoms and n has the value 0, 1, 2, or 3, and C2) from 5 to 50% by weight of structural units derived from one or more dicarboxylic anhydrides, D) from 0.001 to 20% by weight of iron powder, E) from 0.05 to 3% by weight of a copper-containing stabilizer, F) from 100 ppm to 5% by weight of a phosphorus-containing, inorganic acid or salts thereof or ester derivatives thereof or a mixture thereof, G) from 0 to 2% by weight of a polyethyleneimine homo- or copolymer, H) from 0 to 60% by weight of further additives, where the total of the percentages by weight of A) to H) is 100%.
Abstract:
The present invention relates to the use of at least one urea compound of the formula I where x is 1, 2 or 3; R1 and R2 are selected from hydrogen, linear C1-C7-alkyl, branched C3-C10-alkyl, unsubstituted or substituted C3-C12-cycloalkyl, unsubstituted or substituted C3-C12-cycloalkyl-C1-C4-alkyl, unsubstituted or substituted aryl and unsubstituted or substituted aryl-C1-C4-alkyl; and Z is selected from C3-C10-alkanediyl, unsubstituted or substituted arylene, unsubstituted or substituted arylene-C1-C4-alkylene-arylene, unsubstituted or substituted heteroarylene, unsubstituted or substituted heteroarylene-C1-C4-alkylene-heteroarylene, unsubstituted or substituted C5-C8-cycloalkylene, unsubstituted or substituted C5-C8-cycloalkylene-C1-C4-alkylene-C5-C8-cycloalkylene, unsubstituted or substituted heterocycloalkylene and unsubstituted or substituted heterocycloalkylene-C1-C4-alkylene-heterocycloalkylene for improving at least one solid state property of a polyamide resin. The solid state property is preferably selected from mechanical properties and gloss.