Abstract:
The present invention relates to a method of producing a shaped body, wherein, in step i), a layer of a sinter powder (SP) comprising at least one polyhydric alcohol inter alia is provided and, in step ii), the layer provided in step i) is exposed. The present invention further relates to a method of producing a sinter powder (SP) and to a sinter powder (SP) obtainable by this method. The present invention also relates to use of the sinter powder (SP) in a sintering method, and shaped bodies obtainable by the method of the invention.
Abstract:
The present invention relates to a sinter powder (SP) comprising at least one semicrystalline terephthalate polyester (A), at least one amorphous terephthalate polyester (B) and at least one phosphinic salt (C). The present invention further relates to a method of producing a shaped body by sintering the sinter powder (SP) or by an FFF (fused filament fabrication) method, to a shaped body obtainable by the method of the invention, and to the use of a phosphinic salt in a sinter powder (SP) for broadening the sintering window (WSP) of the sinter powder (SP).
Abstract:
The present invention relates to a polymer composition comprising at least one polyamide and at least one urea compound of the formula I where x is 1, 2 or 3; R1 and R2 are selected from hydrogen, linear C1-C7-alkyl, branched C3-C10-alkyl, unsubstituted or substituted C3-C12-cycloalkyl, unsubstituted or substituted C3-C12-cycloalkyl-C1-C4-alkyl, unsubstituted or substituted aryl and unsubstituted or substituted aryl-C1-C4-alkyl; and Z is selected from C3-C10-alkanediyl, unsubstituted or substituted arylene, unsubstituted or substituted aryl unsubstituted or substituted ene-C1-C4-alkylene-arylene, unsubstituted or substituted heteroarylene, unsubstituted or substituted heteroarylene-C1-C4-alkylene-heteroarylene, unsubstituted or substituted C5-C8-cycloalkylene, C5-C8-cycloalkylene-C1-C4-alkylene-C5-C8-cycloalkylene, unsubstituted or substituted heterocycloalkylene and heterocycloalkylene-C1-C4-alkylene-heterocycloalkylene. This urea compound is used for improving the optical properties of the polyamide polymer composition. The present invention also relates to shaped articles obtained from said composition and to novel urea compounds.
Abstract:
The present invention relates to a polymer composition comprising at least one polyamide and at least one urea compound of the formula I where x is 1, 2 or 3; R1 and R2 are selected from hydrogen, linear C1-C7-alkyl, branched C3-C10-alkyl, unsubstituted or substituted C3-C12-cycloalkyl, unsubstituted or substituted C3-C12-cycloalkyl-C1-C4-alkyl, unsubstituted or substituted aryl and unsubstituted or substituted aryl-C1-C4-alkyl; and Z is selected from C3-C10-alkanediyl, unsubstituted or substituted arylene, unsubstituted or substituted aryl unsubstituted or substituted ene-C1-C4-alkylene-arylene, unsubstituted or substituted heteroarylene, unsubstituted or substituted heteroarylene-C1-C4-alkylene-heteroarylene, unsubstituted or substituted C5-C8-cycloalkylene, C5-C8-cycloalkylene-C1-C4-alkylene-C5-C8-cycloalkylene, unsubstituted or substituted heterocycloalkylene and heterocycloalkylene-C1-C4-alkylene-heterocycloalkylene.This urea compound is used for improving the optical properties of the polyamide polymer composition. The present invention also relates to shaped articles obtained from said composition and to novel urea compounds.
Abstract:
The present invention relates to a thermoplastic moulding composition, comprising at least one thermoplastic polymer A); at least one heat conducting filler B); and at least one halogen-containing flame retardant C). Moreover, the invention relates to the use of the inventive moulding compositions for production of fibers, films or mouldings, to the resultant mouldings and to the use thereof for heat transport.
Abstract:
The present invention relates to a sinter powder (SP) comprising a first polyamide component (PA1) and a second polyamide component (PA2), where the melting point of the second polyamide component (PA2) is higher than the melting point of the first polyamide component (PA1). The present invention further relates to a method of producing a shaped body by sintering the sinter powder (SP) or by an FFF (fused filament fabrication) method, and to a shaped body obtainable by the methods of the invention. The present invention further relates to a method of producing the sinter powder (SP).
Abstract:
The present invention relates to a process for producing a polyamide powder (PP) comprising at least one semicrystalline polyamide (P) and at least one additive (A). The semicrystalline polyamide (P) and the at least one additive (A) are initially compounded with one another in an extruder and subsequently introduced into a solvent (SV) in which the at least one semicrystalline polyamide (P) then crystallizes to obtain the polyamide powder (PP). The present invention further relates to the thus obtainable polyamide powder (PP) and to the use of the polyamide powder (PP) as sintering powder (SP) and also to a process for producing a shaped body by selective laser sintering of a polyamide powder (PP).
Abstract:
The invention relates to a filament comprising a core material (CM) comprising a fibrous filler (FF) and a thermoplastic polymer (TP1), and the core material (CM) is coated with a layer of shell material (SM) comprising a thermoplastic polymer (TP2). Further, the invention relates to a process for the preparation of said filament, as well as to three-dimensional objects and a process for the preparation thereof.
Abstract:
The present invention relates to a method for producing a molded body by the selective laser sintering of a sinter powder (SP). The sinter powder (SP) contains at least one polyamide (P) and 5 to 50 wt %, preferably 10 to 50 wt %, of at least one aluminum silicate. The at least one aluminum silicate has a D50 value in the range of 2.5 to 4.5 μm. The present invention also relates to molded bodies obtainable by means of the method according to the invention.
Abstract:
The present invention relates to a polyamide composition (PC) which comprises at least one polyamide (P) and at least one additive (A). The present invention further relates to the use of the polyamide composition (PC) in a selective laser sintering process, in an injection molding process, for producing molded articles and in an extrusion process.