Abstract:
The present invention is to provide a monomer mixture that is cured rapidly even in the presence of oxygen and that forms a cured product having high hardness and excellent adhesion to metals and/or glass. The monomer mixture according to an embodiment of the present invention contains two or more types of cationically polymerizable monomers. As the cationically polymerizable monomers, the monomer mixture contains at least 10 wt. %, based on a total amount of the monomer mixture, of a compound having at least one cationically polymerizable group selected from the group consisting of a vinyl ether group, an epoxy group, and an oxetanyl group, and at least one hydroxy group in a molecule, and at least 5 wt. %, based on the total amount of the monomer mixture, of a compound represented by Formula (b). In the formula, R represents an s-valent straight-chain or branched saturated aliphatic hydrocarbon group or an s-valent group having two or more straight-chain or branched saturated aliphatic hydrocarbon groups bonded to each other through an ether bond, and s represents an integer of 2 or greater.
Abstract:
Provided is a monomer composition that has rapid curability and can be cured rapidly, even in the presence of oxygen and/or water, to form a cured product having excellent adhesion to a wide variety of substrates. The monomer composition according to the present invention contains a vinyl ether compound (A). The vinyl ether compound (A) includes a vinyl ether compound (a) having a cyclic ether skeleton. The monomer composition further contains at least one compound selected from the group consisting of a vinyl ether compound (a′) having a chain hydrocarbon skeleton, a divinyl ether compound (a″-1) having a cyclic hydrocarbon skeleton, an oxetane compound (B), and an epoxy compound (C).
Abstract:
Provided is a monomer composition that has rapid curability and can be rapidly cured, even in the presence of oxygen and/or water, to form a cured product having excellent adhesion to a wide variety of substrates. The monomer composition according to the present invention includes at least one cationically curable monomer. The at least one cationically curable monomer includes at least one of 3-allyloxyoxetane and 3-(2-ethylhexyloxy)oxetane. The at least one of 3-allyloxyoxetane and 3-(2-ethylhexyloxy)oxetane is present in a total content of 5 weight percent or more of the total weight of the monomer composition.
Abstract:
Provided is a sheet-shaped mold possessing a high strength and having a low breakage rate in demolding even in a case where the mold is thin and has a large-area. The sheet-shaped mold is prepared by combining a cured silicone rubber containing a polyorganosiloxane and a fiber for reinforcing the cured silicone rubber. The fiber may comprise a cellulose nanofiber. The sheet-shaped mold may have an uneven pattern on at least one surface (or side) thereof. The fiber may be surface-treated with a hydrophobizing agent. The fiber may forma nonwoven fabric, and the nonwoven fabric may be impregnated with the cured silicone rubber. The cured silicone rubber may comprise a two-component curable silicone rubber having a polydimethylsiloxane unit. The sheet-shaped mold may be a mold for nanoimprint lithography using a photo-curable resin.