Abstract:
Provided is a hot-melt adhesive which satisfies both solidification rate and adhesiveness. A base polymer for a hot-melt adhesive which satisfies the following (1) and (2): (1) a modulus of elasticity in tension at 23° C. is 400 MPa or less; and (2) a semi-crystallization time at 23° C. is 20 minutes or less.
Abstract:
Provided is a spunbonded nonwoven fabric comprising a core-sheath composite fiber having a core part composed of a core component containing a propylene-based resin (A) satisfying the following (a) to (e) and a sheath part composed of a sheath component containing an ethylene-based resin. (a) [mmmm]=20 to 60 mol %, (b) [mm]×[rr]/[mr]2≦2.0, (c) weight average molecular weight (Mw)=10,000 to 200,000, (d) molecular weight distribution (Mw/Mn)
Abstract:
The present invention relates to a nonwoven fabric including a conjugated fiber containing 40% by mass or more and 80% by mass or less of a propylene homopolymer (A) having a melting point (Tm-D) measured by a differential scanning calorimeter (DSC) of higher than 120° C., 4% by mass or more and 40% by mass or less of a polypropylene-based resin (B) having a melting point (Tm-D) measured by a differential scanning calorimeter (DSC) of 120° C. or lower, and 10% by mass or more and 55% by mass or less of a polyethylene-based resin (C), wherein the nonwoven fabric has a texture uniformity of 2.1 or more and 3.0 or less and a bulkiness of 450 μm or more.
Abstract:
The present invention relates to a crimped fiber including one component thereof containing a thermoplastic resin (A) and another component thereof containing a thermoplastic resin (B) and a thermoplastic resin (C), wherein a half-crystallization time at 25° C. of the thermoplastic resin (A) is shorter than a half-crystallization time at 25° C. of the thermoplastic resin (B), and a half-crystallization time at 25° C. of the thermoplastic resin (C) is longer than the half-crystallization time at 25° C. of the thermoplastic resin (B).
Abstract:
Provided is a fibrous nonwoven fabric including a resin composition (C) containing a high-crystalline polyolefin (A) and a low-crystalline polyolefin (B), wherein a half-crystallization time (tc) of the resin composition (C) is 1.2 to 2.0 times a half-crystallization time (ta) of the high-crystalline polyolefin (A).
Abstract:
Provided are a propylene-based polymer which enhances heat creep resistance and a hot-melt adhesive having excellent heat creep resistance. A propylene-based polymer which satisfies the following (1) and (2): (1) 125≦a modulus of elasticity in tension (MPa) at 23° C.≦400; and (2) 100≦an elongation at break (%) at 23° C.≦1,000, and a hot-melt adhesive containing the propylene-based polymer in an amount of 1 to 50% by mass.