Photoactive compound and photosensitive resin composition comprising the same
    11.
    发明授权
    Photoactive compound and photosensitive resin composition comprising the same 有权
    光敏化合物和包含其的感光性树脂组合物

    公开(公告)号:US08252507B2

    公开(公告)日:2012-08-28

    申请号:US12743373

    申请日:2009-04-01

    CPC分类号: C07D405/12 G03F7/031

    摘要: A novel photoactive compound is provided. The photoactive compound has a structure represented by Formula 1: wherein R1, R2, R3, A, X, Y, n and m are as defined in the specification. The photoactive compound efficiently absorbs UV light. Accordingly, the photoactive compound has an improved ability to generate radicals and is efficiently photopolymerized with unsaturated bonds. Further provided is a photosensitive resin composition comprising the photoactive compound. The photosensitive resin composition has good sensitivity because it efficiently absorbs UV light. In addition, the photosensitive resin composition has excellent characteristics in terms of residual film ratio, mechanical strength and resistance to heat, chemicals and development. Therefore, the photosensitive resin composition is advantageously used in curing materials for column spacers, overcoats and passivation films of liquid crystal display devices. In addition, the photosensitive resin composition has excellent thermal processing characteristics.

    摘要翻译: 提供了一种新的光敏化合物。 光活性化合物具有由式1表示的结构:其中R1,R2,R3,A,X,Y,n和m如说明书中所定义。 光敏化合物有效吸收紫外光。 因此,光活性化合物具有改善的产生自由基的能力,并且有效地用不饱和键光聚合。 还提供了包含光敏化合物的感光性树脂组合物。 感光性树脂组合物具有良好的灵敏度,因为它有效地吸收紫外光。 此外,感光性树脂组合物在残留膜比,机械强度和耐热性,化学品和显影方面具有优异的特性。 因此,感光性树脂组合物有利地用于液晶显示装置的柱间隔物,外涂层和钝化膜的固化材料中。 此外,感光性树脂组合物具有优异的热加工特性。

    PHOTOACTIVE COMPOUND AND PHOTOSENSITIVE RESIN COMPOSITION CONTAINING THE SAME
    13.
    发明申请
    PHOTOACTIVE COMPOUND AND PHOTOSENSITIVE RESIN COMPOSITION CONTAINING THE SAME 有权
    光敏化合物和含有它们的光敏树脂组合物

    公开(公告)号:US20110318692A1

    公开(公告)日:2011-12-29

    申请号:US13147342

    申请日:2010-02-12

    摘要: The present invention relates to a photoactive compound of a novel structure represented by Chemical Formula 1 below In Chemical Formula 1, R1 and R2, R3, and A are as defined in the specification, and a photosensitive resin composition comprising the same. The photoactive compound of the present invention comprises a nitro group and a phosphonate structure and thus exhibits excellent sensitivity through efficient absorption for UV light, excellent compatibility between the photoactive compound and the alkali-soluble binder resin, and an improved solubility of the photosensitive resin composition. Furthermore, the photosensitive resin composition of the present invention has excellent residual film thickness and mechanical strength characteristics and heat-resistant, chemical-resistant, and development-resistant properties. Accordingly, the photosensitive resin composition of the present invention is advantageous in hardening the column spacers of liquid crystal displays, an overcoat, and passivation materials and also advantageous in a high-temperature process characteristic.

    摘要翻译: 本发明涉及由化学式1化学式1表示的新结构的光敏化合物,其中R1,R2,R3,A如说明书中所定义,和含有该化合物的感光性树脂组合物。 本发明的光活性化合物包括硝基和膦酸酯结构,因此通过有效吸收UV光,光活性化合物和碱溶性粘合剂树脂之间的相容性优异,并且改善了感光性树脂组合物的溶解性而显示出极好的灵敏度 。 此外,本发明的感光性树脂组合物具有优异的残留膜厚度和机械强度特性以及耐热,耐化学腐蚀和耐开发性能。 因此,本发明的感光性树脂组合物有利于硬化液晶显示器的列间隔物,外涂层和钝化材料,并且在高温工艺特性中也是有利的。

    Polymerized toner and method of producing the same
    14.
    发明授权
    Polymerized toner and method of producing the same 失效
    聚合调色剂及其制备方法

    公开(公告)号:US08394564B2

    公开(公告)日:2013-03-12

    申请号:US12611342

    申请日:2009-11-03

    IPC分类号: G03G9/00

    摘要: A polymerized toner is provided. The polymerized toner has cores containing polyvinylidene fluoride particles. The polyvinylidene fluoride particles have an average particle diameter of 1.1 to 1.5 μm and a melting temperature (Tm) of 140 to 160° C. The polyvinylidene fluoride particles are distributed at a higher concentration near the surface of the cores. This distribution improves the affinity of the cores for silica as an external additive to achieve an increased amount of surface charge and improved transfer efficiency of the polymerized toner. Further provided is a method of producing the polymerized toner.

    摘要翻译: 提供聚合调色剂。 聚合的调色剂具有含有聚偏二氟乙烯颗粒的芯。 聚偏二氟乙烯粒子的平均粒径为1.1〜1.5μm,熔融温度(Tm)为140〜160℃。聚偏二氟乙烯粒子分布在芯的表面附近较高的浓度。 这种分布提高了二氧化硅作为外部添加剂的芯的亲和性,以实现增加的表面电荷量和改善聚合调色剂的转印效率。 还提供了生产聚合调色剂的方法。

    Method for manufacturing a toner having good charging characteristics
    16.
    发明授权
    Method for manufacturing a toner having good charging characteristics 有权
    具有良好充电特性的调色剂的制造方法

    公开(公告)号:US08053157B2

    公开(公告)日:2011-11-08

    申请号:US12226218

    申请日:2007-12-14

    IPC分类号: G03G9/093

    摘要: There is provided a toner having good charging characteristics that is composed of a core region and a thin shell in which a charge control agent is densely distributed so as to improve charging characteristics of the toner, and a method for manufacturing the same. The method for manufacturing a toner having a bi-layered structure includes: producing a toner core using a suspension polymerization method; preparing a suspension of toner particles having a core-shell structure by forming a rigid shell on a surface of the toner core; and recovering the toner particles from the suspension as a post-processing operation.

    摘要翻译: 提供了具有良好的充电特性的调色剂,其由芯区域和薄壳体组成,其中电荷控制剂密集分布以改善调色剂的充电特性及其制造方法。 具有双层结构的调色剂的制造方法包括:使用悬浮聚合法制造调色剂芯; 通过在调色剂芯的表面上形成刚性壳来制备具有核 - 壳结构的调色剂颗粒的悬浮液; 并且作为后处理操作从悬浮液中回收调色剂颗粒。

    Method for Manufacturing a Toner Having Good Charging Characteristics
    17.
    发明申请
    Method for Manufacturing a Toner Having Good Charging Characteristics 有权
    制造具有良好充电特性的调色剂的方法

    公开(公告)号:US20090246673A1

    公开(公告)日:2009-10-01

    申请号:US12226218

    申请日:2007-12-14

    IPC分类号: G03G9/08

    摘要: There is provided a toner having good charging characteristics that is composed of a core region and a thin shell in which a charge control agent is densely distributed so as to improve charging characteristics of the toner, and a method for manufacturing the same. The method for manufacturing a toner having a bi-layered structure includes: producing a toner core using a suspension polymerization method; preparing a suspension of toner particles having a core-shell structure by forming a rigid shell on a surface of the toner core; and recovering the toner particles from the suspension as a post-processing operation.

    摘要翻译: 提供了具有良好的充电特性的调色剂,其由芯区域和薄壳体组成,其中电荷控制剂密集分布以改善调色剂的充电特性及其制造方法。 具有双层结构的调色剂的制造方法包括:使用悬浮聚合法制造调色剂芯; 通过在调色剂芯的表面上形成刚性壳来制备具有核 - 壳结构的调色剂颗粒的悬浮液; 并且作为后处理操作从悬浮液中回收调色剂颗粒。

    Method of producing polymerized toner
    19.
    发明授权
    Method of producing polymerized toner 有权
    生产聚合调色剂的方法

    公开(公告)号:US08216761B2

    公开(公告)日:2012-07-10

    申请号:US12671416

    申请日:2008-10-08

    IPC分类号: G03G5/00

    摘要: Disclosed is a method for producing a polymerized toner. In the method, a mixture of colloidal silica as an aqueous dispersant and a polyvinylpyrrolidone is used during suspension polymerization. The amount of polyvinylpyrrolidone/colloidal silica aggregates having a diameter smaller than 100 nm is also limited to 1% by weight or less, based on the total weight of all aggregates. A polymerized toner produced by the method has a volume average particle diameter (dv) of 5 to 10 μm and a volume average particle diameter/number average particle diameter ratio (dv/dp) of 1.5 or less. The polymerized toner is consumed in a small amount during printing. According to the method, the formation of emulsion particles having a size smaller than 0.5 μm is inhibited.

    摘要翻译: 公开了一种聚合调色剂的制造方法。 在该方法中,在悬浮聚合中使用作为水性分散剂的胶体二氧化硅与聚乙烯吡咯烷酮的混合物。 直径小于100nm的聚乙烯吡咯烷酮/胶体二氧化硅聚集体的量也以所有聚集体的总重量计为1重量%以下。 通过该方法制造的聚合调色剂的体积平均粒径(dv)为5〜10μm,体积平均粒径/数均粒径比(dv / dp)为1.5以下。 聚合调色剂在印刷过程中少量消耗。 根据该方法,抑制了尺寸小于0.5μm的乳液颗粒的形成。

    METHOD OF PRODUCING POLYMERIZED TONER
    20.
    发明申请
    METHOD OF PRODUCING POLYMERIZED TONER 有权
    生产聚合物的方法

    公开(公告)号:US20100190103A1

    公开(公告)日:2010-07-29

    申请号:US12671416

    申请日:2008-10-08

    IPC分类号: G03G9/00

    摘要: Disclosed is a method for producing a polymerized toner. In the method, a mixture of colloidal silica as an aqueous dispersant and a polyvinylpyrrolidone is used during suspension polymerization. The amount of polyvinylpyrrolidone/colloidal silica aggregates having a diameter smaller than 100 nm is also limited to 1% by weight or less, based on the total weight of all aggregates. A polymerized toner produced by the method has a volume average particle diameter (dv) of 5 to 10 μm and a volume average particle diameter/number average particle diameter ratio (dv/dp) of 1.5 or less. The polymerized toner is consumed in a small amount during printing. According to the method, the formation of emulsion particles having a size smaller than 0.5 μm is inhibited.

    摘要翻译: 公开了一种聚合调色剂的制造方法。 在该方法中,在悬浮聚合中使用作为水性分散剂的胶体二氧化硅与聚乙烯吡咯烷酮的混合物。 直径小于100nm的聚乙烯吡咯烷酮/胶体二氧化硅聚集体的量也以所有聚集体的总重量计为1重量%以下。 通过该方法制造的聚合调色剂的体积平均粒径(dv)为5〜10μm,体积平均粒径/数均粒径比(dv / dp)为1.5以下。 聚合调色剂在印刷过程中少量消耗。 根据该方法,抑制了尺寸小于0.5μm的乳液颗粒的形成。