SYSTEMS FOR CENTRIFUGALLY CASTING HIGHLY REACTIVE TITANIUM METALS
    13.
    发明申请
    SYSTEMS FOR CENTRIFUGALLY CASTING HIGHLY REACTIVE TITANIUM METALS 审中-公开
    用于离心铸造高反应性钛金属的系统

    公开(公告)号:US20090133850A1

    公开(公告)日:2009-05-28

    申请号:US11945388

    申请日:2007-11-27

    IPC分类号: B22D13/00

    CPC分类号: B22D13/00

    摘要: Systems for centrifugally casting a highly reactive titanium metal including a cold wall induction crucible for containing a titanium metal charge, the induction crucible having a plurality of induction coils and a removable bottom plate, a power source to heat the titanium metal charge in the induction crucible to obtain a molten metal, a preheated secondary crucible for catching the molten metal as it falls from the induction crucible after the removable bottom plate has been withdrawn and the power source turned off, and a centrifugal casting machine for holding and accelerating the secondary crucible to centrifugally force the molten metal into a casting mold and produce a cast component.

    摘要翻译: 用于离心铸造高反应性钛金属的系统,包括用于容纳钛金属电荷的冷壁感应坩埚,所述感应坩埚具有多个感应线圈和可移除的底板,用于加热所述诱导坩埚中的钛金属电荷的电源 以获得熔融金属,预热的二次坩埚,用于在可移除的底板已经被取出并且电源关闭之后从熔化金属落下时捕获熔融金属;以及用于将二次坩埚保持和加速的离心铸造机 将熔融金属离心力压入铸模中并生产铸件。

    Turbine component protected with environmental coating
    15.
    发明授权
    Turbine component protected with environmental coating 有权
    涡轮机组件采用环保涂层保护

    公开(公告)号:US07364801B1

    公开(公告)日:2008-04-29

    申请号:US11567382

    申请日:2006-12-06

    摘要: An environmental coating suitable for use on turbine components, such as turbine disks and turbine seal elements, formed of alloys susceptible to oxidation and hot corrosion. The environmental coating is predominantly a solid solution phase of nickel, iron, and/or cobalt. The coating contains about 18 weight percent to about 60 weight percent chromium, which ensures the formation of a protective chromia (Cr2O3) scale while also exhibiting high ductility. The coating may further contain up to about 8 weight percent aluminum, as well as other optional additives. The environmental coating is preferably sufficiently thin and ductile to enable compressive stresses to be induced in the underlying substrate through shot peening without cracking the coating.

    摘要翻译: 一种适用于涡轮机部件的环境涂层,例如涡轮盘和涡轮密封件,由易受氧化和热腐蚀的合金形成。 环境涂层主要是镍,铁和/或钴的固溶相。 该涂层含有约18重量%至约60重量%的铬,这确保形成保护性氧化铬(Cr 2 O 3 O 3),同时还具有高延展性。 该涂层还可含有至多约8重量%的铝以及其它任选的添加剂。 环境涂层优选是足够薄且延性的,以使压缩应力能够通过喷丸硬化在下面的基材中被引发而不会使涂层破裂。