Apparatus and methods for industrial-scale production of metal matrix nanocomposites (MMNCs) are provided. The apparatus and methods can be used for the batch production of an MMNC in a volume of molten metal housed within the cavity of a production chamber. Within the volume of molten metal, a flow is created which continuously carries agglomerates of nanoparticles, which have been introduced into the molten metal, through a cavitation zone formed in a cavitation cell housed within the production chamber.
摘要:
A coupling has an opening and a protrusion extending downward from the opening. The protrusion has threads that are preferably positioned outside of the opening. A rotor shaft that connects to the coupling has an internal bore with threads that receives and retains the protrusion, such as by a threaded connection between the two, so the protrusion applies driving force to the shaft.
摘要:
The present invention relates to an apparatus and method for purifying materials using a fractional solidification. Devices and methods shown provide control over a temperature gradient and cooling rate during fractional solidification, which results in a material of higher purity. The apparatus and methods of the present invention can be used to make silicon material for use in solar applications such as solar cells.
摘要:
Apparatus and methods for industrial-scale production of metal matrix nanocomposites (MMNCs) are provided. The apparatus and methods can be used for the batch production of an MMNC in a volume of molten metal housed within the cavity of a production chamber. Within the volume of molten metal, a flow is created which continuously carries agglomerates of nanoparticles, which have been introduced into the molten metal, through a cavitation zone formed in a cavitation cell housed within the production chamber.
摘要:
A method for treating spheroidal graphite iron includes the step: pouring molten spheroidal graphite iron into a pouring electrical furnace (1); covering the molten spheroidal graphite iron (5) with alkali slag (6) which is melted at high temperature and rich in alkali earth metal ion, rare earth metal ion, or mixture of them; connecting the molten spheroidal graphite iron (5) with the negative pole of the direct current source by one pole (7); connecting the alkali slag (6) with the positive pole of the direct current source by another pole (4), treating the molten spheroidal graphite iron (5) with the alkali slag (6) which is used as electrolyte. The method can prevent the spheroidized fading velocity of the spheroidal graphite iron. The pouring electrical furnace can be used for treating the molten spheroidal graphite iron.
摘要:
An apparatus for condensing metal vapors has at least one inlet conduit that is cooled to cause a portion of the metal vapor to condense to liquid. The apparatus also has a holding tank that is connected to the inlet conduit that collects condensed liquid metal. The apparatus also has at least one outlet conduit connected to the holding tank that is cooled to cause a portion of the remaining metal vapor to condense to solid metal. The apparatus also has at least one heater that heats the at least one outlet conduit to cause the solid metal to melt to liquid metal and subsequently flow in to the holding tank. The apparatus also has at least one sealing mechanism located at a distal end of the at least one outlet conduit for preventing metal vapor and carrier gas from exiting the outlet conduit during heating of the outlet conduit.
摘要:
A method for treating spheroidal graphite iron includes the step: pouring molten spheroidal graphite iron into a pouring electrical furnace (1); covering the molten spheroidal graphite iron (5) with alkali slag (6) which is melted at high temperature and rich in alkali earth metal ion, rare earth metal ion, or mixture of them; connecting the molten spheroidal graphite iron (5) with the negative pole of the direct current source by one pole (7); connecting the alkali slag (6) with the positive pole of the direct current source by another pole (4), treating the molten spheroidal graphite iron (5) with the alkali slag (6) which is used as electrolyte. The method can prevent the spheroidized fading velocity of the spheroidal graphite iron. The pouring electrical furnace can be used for treating the molten spheroidal graphite iron.
摘要:
A steel plate is provided which has excellent hydrogen induced cracking resistance. The steel plate is suitable for use in a line pipe. The steel plate satisfies a predetermined composition. In a composition of an inclusion contained in the steel and having a width of 1 μm or more, the ratio (RES/CaS) of the mass of an REM sulfide (RES) to that of a Ca sulfide (CaS) is equal to or more than 0.05, a Zr content of the inclusion is in a range of 5 to 60%, and a Nb content of the inclusion is 5% or less.
摘要:
Nanomaterials are incorporated within a material, such as within a metal-based material. As may be implemented in accordance with various embodiments, nanomaterials are introduced to a metal-based material in a liquid state, and the metal-based material and nanomaterials are cooled from the liquid state to a viscous state. The metal-based material is stirred in the viscous state to disperse the nanomaterials therein, and the metal-based material is used in the viscous state to maintain dispersion of the nanomaterials as the metal-based material cools.
摘要:
Apparatus and methods for industrial-scale production of metal matrix nanocomposites (MMNCs) are provided. The apparatus and methods can be used for the batch production of an MMNC in a volume of molten metal housed within the cavity of a production chamber. Within the volume of molten metal, a flow is created which continuously carries agglomerates of nanoparticles, which have been introduced into the molten metal, through a cavitation zone formed in a cavitation cell housed within the production chamber.